Study of thermal properties, electrical conductivity, and the crystallization process of the glassy alloy SeGe20
Source abstract
Abstract
The samples are prepared by introducing 5% of selenium in pure germanium. The samples are subjected to hea ttreatment at temperatures of 80, 90, and 100 °C. These temperatures are selected by differential thermal analysis (DTA). After annealing of the samples at these temperatures the electrical conductivity σ20 at 20 °C, the activation energy Eg of the conductivity process, and the density d are determined and taken as a measure of the crystallization rate of the annealed samples. The crystallization process depends on the selected annealing temperature and also on the time of annealing. The estimated value of activation energy of the crystallization process is equal to 9.55 × 104 J/mol. It is found also that the process of crystallization of the annealed glassy alloy SeGe20 is one-dimensional. The thermal properties (thermal conductivity λ, thermal diffusivity a, and specific heat capacity cp) of the heat treated SeGe20 at temperature 100 °C are measured. It is found that the main mechanism of heat transfer is due to phonons. The calculated values of the role of electrons and bipolars are very small.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Phase-change materials and chalcogenides · Material Dynamics and Properties · Chemical Thermodynamics and Molecular Structure
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.