article·1978-02-16

Annealing spectrum of cold-worked dilute AlLi alloys

R. Kamel, A. R. Ali, Z. Farid

Publisher page

Abstract

Two annealing bands are found in the recovery of cold-worked pure Al and three dilute AlLi alloys (0.25, 2.5, and 4.5 at% Li) in the temperature range 25 to 200 °C. A third one occurring at higher temperatures is detected only in Al–2.5 at% Li and Al–4.5 at% Li. The first annealing band is characterized by the annealing out of relatively free dislocations. The Li solute atoms, acting as impurity-pinning points, retarded the dislocation mobility and, consequently, the recovery process. The second annealing stage, attributed to recrystallization, is found to be activated by an energy in the range 1.2 to 1.4 eV which is found to increase with increasing solute concentration. The binding energy between the Li solute atoms and dislocations is about 0.16 eV. At higher temperatures, a third stage of annealing characterized by a high activation energy (1.46 eV), is assumed to originate from the tendency of solute lithium atoms to form clusters in the matrix.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.