High Temperature Implantation of Silicon by B+ and BF2+ Ions

G. A. Kachurin, Igor Tyshchenko, Л. И. Федина, E. Wieser, Ch. Weise

Publisher page

Abstract

(100) n-type silicon is implanted by B+ and BF ions at temperatures in the range of 600 to 1100 °C. The depth distribution of the impurities boron and fluorine and of the charge carrier concentration is determined by SIMS and Van der Pauw measurements after stepwise sheet removal. The development of lattice defects is studied by TEM. The observed depth of the boron profiles up to about 1 μm is explained by an enhanced diffusion due to excess vacancies. The differences in the development of defects for B+ and BF implantation and its influence on the electrical activation and the diffusion behaviour of boron is discussed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Integrated Circuits and Semiconductor Failure Analysis · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.