In this Erratum, the authors revisit the “Results and discussion” and “Conclusion” parts of their previous article [Phys. Status Solidi A 206, 2000 (2009)] after correction of one data point for the incorporation efficiency η of phosphorus plotted in Fig. 2 of the article. Figure 2 in the article by Frangieh et al. [Phys. Status Solidi A 206, 2000 (2009)] has to be replaced by the following corrected figure: Plot of the phosphorus incorporation efficiency, η, as a function of the [C*]/[H2] ratio. Within the Section 3, the second and third paragraphs should read as follows: The phosphorus concentration, [P], reached in this study is in the range of 4 × 1017–2 × 1019 P/cm3. The incorporation efficiency of phosphorus (P) is defined by: In Section 4, the second sentence has to be corrected as follows: Phosphorus is successfully incorporated (up to 2 × 1019 P/cm3) with an incorporation efficiency up to ∼0.026%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Diamond and Carbon-based Materials Research · Advanced Materials Characterization Techniques · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.