The Nature of Stage IIA Recovery in Cold-Worked Aluminium
Source abstract
Abstract
The structure of differential isochronal recovery curves between 60 and 100 K (stage IIA) in aluminium cold-drawn by 5 to 16% at 4.2 K is investigated by the measurement of residual electrical resistivity. The recovery curves consist of two different sub-peaks at about 75 and about 90 K. The ratio of P75/P90 decreases with increasing the amount of extention, where P75 is the height of the first peak and P90 is that of the second one. The ratio decreases by a prior deformation and a low-temperature anneal. An interpretation of these recoveries is made in terms of pipe diffusion of vacancies along dislocations. Die Struktur der isochronen differentiellen Erholungskurven zwischen 60 und 100 K (Erholungsstufe IIA) von um 5 bis 16% bei 4,2 K deformiertem Aluminium wird durch Messung des elektrischen Restwiderstandes untersucht. Die Erholungskurven bestehen aus zwei verschiedenen Submaxima bei etwa 75 und 90 K. Das Verhältnis P75/P90 nimmt mit zunehmendem Dehnungsgrad zu, wobei P75 die Höhe des ersten Maximums und P90 die des zweiten ist. Das Verhältnis nimmt durch eine vorhergehende Deformation und eine Niedertemperaturtemperung ab. Eine Interpretation dieser Erholung wird mit Pipe-Diffusion von Leerstellen entlang von Versetzungen gemacht.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.