Abstract

The paper investigates microalloying effects of Fe in NiAl crystals. High-purity NiAl–0.2 at% Fe single crystals were prepared by a modified Bridgman method. The impurity content was less than 20 wt ppm metallic impurities, 50 wt ppm oxygen and 5 wt ppm nitrogen. The alloy composition was analyzed by different wet chemical methods, which give evidence to stoichiometry deviations smaller than 0.2 at%. The residual resistivity ratio of the as-grown crystals was near R295 K/R4.2 K ≈︂ 4. The secondary ion mass spectrometry investigations revealed segregation effects of Fe. These could be reduced by increasing the growth rate. For soft orientated 〈123〉 Fe microalloyed NiAl samples room-temperature compressive deformations to failure of more than 40% have been achieved, which exceed the level of ≈︂20% for binary NiAl crystals. There was a significant reduction of the critical resolved shear stress at room temperature from 104 MPa for as-grown binary crystals to 54 MPa for Fe microalloyed crystals. This value is comparable with 45 to 55 MPa of annealed binary high-purity NiAl crystals. A dopant/point defect interaction mechanism is supposed to be responsible for the improvement of the mechanical properties due to microalloying.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Energetic Materials and Combustion · Ion-surface interactions and analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.