The creep behaviour of high purity polycrystalline magnesium at 0.32 to 0.51Tm

D. O. Northwood, I. O. Smith

Publisher page

Abstract

High purity (99.99%) polycrystalline magnesium is creep tested in air at temperatures of 25, 100, and 200°C (0.32 to 0.51Tm, where Tm is the melting temperature) and the stress-dip test during steady-state creep is used to determine the effective (σe) and internal (σi) stresses. The stress exponent of steady-state creep n (in equation \documentclass{article}\pagestyle{empty}\begin{document}$ \mathop \varepsilon \limits^ \cdot \rm S \, = \,A\sigma ^n $\end{document}) shows a transition from n = 2.5 to 3.3 at low values of σ to n = 5.3 to 10.3 for high values of σ. This transition in behaviour occurs at higher values of σ for lower creep temperatures. Such a transition in stress exponent indicates a change in rate controlling mechanism(s). The magnitude of the internal or back stress in comparison with the applied stress σ increases as the creep temperature decreases: when expressed as σi ∼ σx, x is 0.98 at 20°C, 0.81 at 100°C, and 0.76 or 0.81 at 200°C. These results for σi with σi/σ ratios increasing as the creep temperature decreases, are in agreement with the generally accepted theory that creep at these temperatures is controlled by glide recovery in that the degree of recovery will be smaller at the lower temperatures thus leading to a larger internal or back stress.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Tribology and Wear Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.