Stoichiometric annealing and electrical properties of Hg0.8Cd0.2Te grown by solid state recrystallization
Source abstract
Abstract
A stoichiometric annealing treatment is proposed for removing the tellurium precipitates from Hg0.8Cd0.2Te crystals grown by solid state recrystallisation. The fact that the chemical potential of tellurium decreases with increasing x in Hg saturated Hg1−xCdxTe is high-lighted and utilized in evolving the treatment. An Hg–Hg0.7Cd0.3Te source is used for annealing the bulk grown Hg0.8Cd0.2Te wafers. The annealing was carried out isothermally first at 420 °C and subsequently at 260 °C. Because of the retrograde solubility of Te in MCT the Te microprecipitates are partly dissolved back into the matrix at 420 °C and the remaining excess of Te is driven out into the ambient under the chemical potential gradient provided by the source. The proposed treatment almost completely eliminates the wafer-to-wafer and batch-to-batch variation in electrical properties of the low-temperature annealed Hg0.8Cd0.2Te crystals.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Semiconductor Detectors and Materials · Chalcogenide Semiconductor Thin Films · Thermography and Photoacoustic Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.