Magnetic Relaxation in Dilute Iron–Nickel Alloys Following Low-Temperature Electron Irradiation
Source abstract
Abstract
Magnetic after-effect measurements are made in the temperature range 30 to 300 K on a series of dilute FeNi alloys with varying Ni concentrations (100 at ppm ≦ CNi ≦ 1.0 at%) following 3 MeV electron-irradiation at 44 K. The resulting relaxation spectra are very similar to those obtained on identical samples after low-temperature neutron-irradiation; each relaxation peak in the electron-irradiated sample has its analogue in the neutron-irradiated specimen. The results are discussed in terms of impurity-trapping of interstitials at substitutionally dissolved Ni atoms.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Magnetic Properties and Applications · Microstructure and Mechanical Properties of Steels · Magnetic properties of thin films
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References
Reference metadata was not supplied for this record.