article·1987-07-16

Plastic Behaviour of Polycrystalline Al−0.72 wt% Si

T. H. Youssef, F. A. Saadalah, I. K. Bishay

Publisher page

Abstract

Isochronal annealing of as received aluminium wires of commercial purity is carried out from room temperature up to 600 °C. The results show the existence of two annealing stages, one from room temperature up to 300 °C and the other from 300 °C upwards. The first annealing stage with an activation energy of 0.2 eV is interpreted by vacancy-silicon binding energy and clustering of Si atoms on grain boundaries. The second annealing stage is proved to be a multi-energy stage with an activation energy ranging between 0.36 and 0.80 eV, this is in agreement with that for the Si diffusion in the aluminium matrix during the recrystallization process. The wires are then subjected to combined tensile-torsion deformation. The results show (i) negative tensile strain (−ΔL/L) i.e. contraction for samples annealed over the temperature range of the first annealing stage. This behaviour is inferred to hardening due to internal stresses formed on clustering of Si atoms at grain boundaries, as well as the formation of Lüders bands at the grain boundaries during twisting, (ii) normal positive tensile strain (+ΔL/L) for samples annealed over the temperature range of the second annealing stage. This behaviour is attributed to the decrease in the internal stresses; because annealing at these relatively high temperatures (above 300 °C) leads to the diffusion of Si atoms collected at grain boundaries — at the first annealing stage — in the matrix.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.