Analysis of DLTS Curves of Aggregated Deep Level Impurities
Source abstract
Abstract
Rate equations of the occupancy of aggregated impurities including two interaction parameters are solved. The DLTS curves, in particular their widths, heights, and shifts for various interaction strengths are calculated. Further, the filling factor as a function of the filling pulse duration is calculated for various interactions. Finally, the DLTS on n-CdTe Schottky junctions are measured; the dominant peak is interpreted as a deep level aggregate and its parameters are determined.