article·1970-03-16

Electrical resistivity of dilute binary chromium alloys with nickel and manganese

Sigurds Arajs

Publisher page

Abstract

Electrical resistivity, ϱ, of binary chromium alloys containing 0.4, 0.8, 1.7, 2.6, 4.4 at% nickel and 2.1, 4.0 at% manganese has been measured as a function of temperature, T, between 4 and 320 °K. Shallow anomalies in the ϱ vs. T curves appear at the Néel temperature in the chromium–nickel samples. No anomalies are observed in the electrical resistivity of chromium–manganese alloys since manganese increases the Néel temperature of chromium. The results of this study are compared with all the known previous investigations. Der spezifische elektrische Widerstand ϱ von binären Chromlegierungen mit 0,4; 0,8; 1,7; 2,6; 4,4 At% Nickel und 2,1; 4,0 At% Mangan wurde in Abhängigkeit von der Temperatur T zwischen 4 und 320 °K gemessen. Flache Anomalien treten in der (ϱ über T)-Kurve bei der Néel-Temperatur in den Chrom–Nickel-Proben auf. Im Verlauf des spezifischen elektrischen Widerstands von Chrom–Mangan-Legierungen wurden keine Anomalien beobachtet, weil Mangan die Néel-Temperatur von Chrom erhöht. Die Ergebnisse der Arbeit werden mit allen bekannten früheren Untersuchungen verglichen.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fusion materials and technologies · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References