article·1975-12-16

Melt Growth of Crystalline Silicon Tubes by a Capillary Action Shaping Technique

T.F. Ciszek

Publisher page

Abstract

Silicon tubes 6 mm in diameter and over 1 m long were grown by a capillary action shaping technique using a 7 mm diameter graphite capillary die with a 1.3 mm thick wall. Diameter and wall thickness could be varied from 6.6 to 5.7 mm and 1.2 to 0.4 mm respectively by relative system temperature changes of up to 6.7 °C or growth rate variations in the range 11 to 21 mm/min. The tubes were doped with boron to a 2 Ωcm resistivity. Planar defects and some large angle grain boundaries were present, with the largest grains extending over one quarter of the tube circumference. Siliziumrohre mit 6 mm Durchmesser und mit einer Länge von mehr als 1 m wurden mit einer Kristallziehtechnik gezogen, die auf der Kapillarwirkung von Graphitkapillaren mit 7 mm Durchmesser und 1,3 mm Wanddicke beruht. Durch relative Temperaturänderung des Systems bis zu 6,7 °C und durch Variation der Wachstumsrate im Bereich von 11 bis 21 mm/min konnten der Durchmesser der Si-Rohre von 6,6 bis 5,7 mm und die Wanddicke von 1,2 bis 0,4 mm variiert werden. Die Rohre wurden mit Bor dotiert bis zu einem Widerstand von 2 Ωcm. Sie enthalten ebene Gitterdefekte und Großwinkelkorngrenzen, wobei sich die größten Körner über ein Viertel des Rohrumfanges erstrecken.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Modular Robots and Swarm Intelligence

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.