Abstract

Conductivity profiles and impurity concentration of silicon implanted with 30 keV phosphorus ions (implantation dose 6 Cm−2) were studied. The defect annealing has been found to terminate practically during the first minutes at Tann = 600 to 900°C. Diffusion redistribution of implanted atoms becomes appreciable after 6 h at 600°C, after 2 h at 800°C, and after 2 to 5 min at 900°C. The annealing process at 900°C is accompanied by a considerable change of the defect concentration and therefore of the coefficient D of the radiation-induced diffusion. A calculation of D(x, t) basing on the variation of the phosphorus concentration profile shows that initially the diffusion coefficient in the region of maximum defect concentration is 2 to 2.5 orders of magnitude higher than the coefficient for ordinary diffusion. [Russian Text Ignored].
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Integrated Circuits and Semiconductor Failure Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References

Reference metadata was not supplied for this record.