Intermetallic formation by solute segregation during dissimilar welding of Inconel 718 and SS316L stainless steel poses a severe challenge of solidification cracking in the welded structure. The minimisation of these intermetallic phases and, eventually, the solidification cracks through variation in welding speed is undertaken in the current study. With a reduction in welding speed, an improvement in the weld dilution level is observed along with a change in microstructural morphology from columnar to equiaxed dendrites. A reduction in solute segregation is evident with higher weld dilution level and equiaxed structure as compared with the columnar dendrites. The enrichment of Nb, Mo, and Ti is witnessed near micro-crack sites produced with a higher welding speed. X-ray diffraction (XRD) analysis confirmed the presence of various intermetallic phases and found to decrease with a reduction in the welding speed. With a reduction in welding speed, the tensile strength improved marginally, whereas a remarkable improvement in tensile ductility (∼ 90%) was found.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Mechanical Engineering, IIT Guwahati, Assam, India

School of Mechanical Engineering, Xi’an Jiaotong University, Xi’an, People’s Republic of China

National Key Laboratory for Precision Hot Processing of Metals, Harbin Institute of Technology, Harbin, People's Republic of China

References (15)

Show source-provided references
1. 10.1007/978-981-32-9072-3_2010.1007/978-981-32-9072-3_20 ↗
2. 10.1179/13621710422501709910.1179/136217104225017099 ↗
3. Brooks J.W. · Superalloys · 1988 · 88 · 33
4. 10.1007/s10853-009-3691-510.1007/s10853-009-3691-5 ↗
5. 10.1179/imr.1975.20.1.8310.1179/imr.1975.20.1.83 ↗
6. S. Kou, Welding Metallurgy, 2nd ed., A John Wiley & Sons, Inc., Hoboken, NJ, 2003, pp.431–446.
7. 10.1179/stw.1999.4.1.110.1179/stw.1999.4.1.1 ↗
8. 10.1080/09500839.2019.159799110.1080/09500839.2019.1597991 ↗
9. Knorovsky G.A. · Inconel 718: A solidification diagram · 1989 · 20 · 2149
10. 10.1016/j.matdes.2014.05.01910.1016/j.matdes.2014.05.019 ↗
11. 10.1016/j.jallcom.2017.12.29510.1016/j.jallcom.2017.12.295 ↗
12. 10.1080/09500839.2014.99574010.1080/09500839.2014.995740 ↗
13. 10.1016/S0167-577X(01)00653-X10.1016/S0167-577X(01)00653-X ↗
14. 10.1016/j.jmatprotec.2013.09.00610.1016/j.jmatprotec.2013.09.006 ↗
15. 10.1179/13621710222500680410.1179/136217102225006804 ↗