Materials depth distribution and degradation of a FIrpic based solution-processed blue OLED
Source abstract
Abstract
Abstract To improve the lifetime of solution processed OLEDs it is important to identify at which position within the multi-material stack the materials degrade. To this end, we have analyzed the materials depth distribution of a solution processed phosphorescent OLED consisting of the blend PVK, OXD-7 and FIrpic prior and after electrical device degradation via TOF-SIMS. We have found that FIrpic not only agglomerates strongly at the PEDOT:PSS hole injecting electrode, but also degrades only at this interface. What is more, PSS fragments can be found across the entire stack. We finally identify two methods that lead to an improved OLED lifetime.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Organic Light-Emitting Diodes Research · Thin-Film Transistor Technologies · Organic Electronics and Photovoltaics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. Device physics – enlightening solutions10.1038/437327a ↗
2. Chemical degradation in organic light-emitting devices: mechanisms and implications for the design of new materials10.1002/adma.201205022 ↗
3. Degradation mechanisms in small-molecule and polymer organic light-emitting diodes10.1002/adma.200902624 ↗
4. Chemical degradation mechanisms of highly efficient blue phosphorescent emitters used for organic light emitting diodes10.1016/j.orgel.2012.10.003 ↗
5. Highly efficient solution processed blue organic electrophosphorescence with 14lm/W luminous efficacy10.1063/1.2212060 ↗
6. New crosslinkable hole conductors for blue-phosphorescent organic light-emitting diodes10.1002/anie.200605055 ↗
7. Solution-processed highly efficient blue phosphorescent polymer light-emitting diodes enabled by a new electron transport material10.1002/adma.201001585 ↗
8. Cyclometalated Ir(III) complexes for high-efficiency solution-processable blue PhOLEDs10.1021/cm4010773 ↗
9. Crosslinkable TAPC-based hole-transport materials for solution-processed organic light-emitting diodes with reduced efficiency roll-off10.1002/adfm.201201197 ↗
10. Degradation mechanism in simplified phosphorescent organic light-emitting devices utilizing one material for hole transport and emitter host10.1063/1.4817918 ↗
11. Stability of the interface between indium-tin-oxide and poly(3,4-ethylenedioxythiophene)/poly(styrenesulfonate) in polymer light-emitting diodes10.1063/1.1315344 ↗
12. Highly phosphorescent organic mixed films: the effect of aggregation on triplet–triplet annihilation10.1063/1.3123815 ↗
13. Degradation of HTL layers during device operation in PhOLEDs10.1016/j.solidstatesciences.2009.07.017 ↗
14. Operational degradation of organic light-emitting diodes: mechanism and identification of chemical products10.1063/1.2430922 ↗
15. Analysis of chemical degradation mechanism within sky blue phosphorescent organic light emitting diodes by laser-desorption/ionization time-of-flight mass spectrometry10.1016/j.orgel.2010.11.004 ↗
16. Fluorine cleavage of the light blue heteroleptic triplet emitter FIrpic10.1016/j.jfluchem.2009.04.009 ↗
17. Efficiency roll-off in organic light-emitting diodes10.1002/adma.201301603 ↗
18. Nucleophilic substitution of fluorine atoms in 2,6-difluoro-3-(pyridin-2-yl)benzonitrile leading to soluble blue-emitting cyclometalated Ir(III) complexes10.1021/jo200357e ↗