Influence of cathode oxidation via the hole extraction layer in polymer:fullerene solar cells
Source abstract
Abstract
In this paper, we elucidate the role of poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate) (PEDOT:PSS) in the degradation of polymer:PCBM ((6,6)-phenyl C61-butyric acid methyl ester) solar cells. The study is done on unencapsulated cells exposed to ambient conditions in dark. The cell degradation results from reduced carrier extraction, and an investigation of the various interfaces within the cell allows us to correlate this to oxidation of the low work function metal cathode. We further show that this oxidation is caused by water vapor diffusion from the edges through the hygroscopic PEDOT:PSS layer. We demonstrate that only the hygroscopic nature of PEDOT:PSS, and not its acidity, has a detrimental impact. The oxidation of the cathode progresses in synchrony with the water ingress into the PEDOT:PSS layer from the edges of the device towards the central part, and results in a progressive constriction of the active area. When the PEDOT:PSS layer is replaced by an evaporated layer of MoO3, the device lifetime is improved considerably even with highly reactive metal cathodes. Finally, we provide a quantitative relationship between device lifetime and the level of humidity in the ambient, thus establishing a suitable accelerated shelf-life test for organic solar cells and their encapsulation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Organic Electronics and Photovoltaics · Conducting polymers and applications · Semiconductor materials and interfaces
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Organic-based photovoltaics: toward low-cost power generation10.1557/mrs2005.2 ↗
2. Polymer–fullerene bulk-heterojunction solar cells10.1002/adma.200903697 ↗
3. Organic tandem solar cells with complementary absorbing layers and a high open-circuit voltage10.1063/1.3464169 ↗
4. Highly efficient organic solar cells with sprayed hole-transport and active layers10.1002/adfm.201001562 ↗
5. Fabrication and processing of polymer solar cells: a review of printing and coating techniques10.1016/j.solmat.2008.10.004 ↗
6. Stability/degradation of polymer solar cells10.1016/j.solmat.2008.01.005 ↗
7. Material challenges for flexible organic devices10.1016/S1369-7021(06)71446-8 ↗
8. 2008
9. Light-induced degradation of the active layer of polymer-based solar cells10.1016/j.polymdegradstab.2009.11.021 ↗
10. The mechanism of photo- and thermooxidation of poly(3-hexylthiophene) (p3ht) reconsidered10.1016/j.polymdegradstab.2009.03.005 ↗
11. Oxygen doping of p3ht:pcbm blends: influence on trap states charge carrier mobility and solar cell performance10.1016/j.orgel.2010.07.016 ↗
12. Influence of oxygen on semi-transparent organic solar cells with gas permeable electrodes10.1016/j.orgel.2009.08.001 ↗
13. Dynamics and reversibility of oxygen doping and de-doping for conjugated polymer10.1063/1.2917419 ↗
14. Photoinduced degradation of polymer and polymer–fullerene active layers: experiment and theory10.1002/adfm.201001079 ↗
15. Degradation mechanisms in small-molecule and polymer organic light-emitting diodes10.1002/adma.200902624 ↗
16. Water vapor and oxygen degradation mechanisms in organic light emitting diodes10.1002/1616-3028(200104)11:2<116::AID-ADFM116>3.0.CO;2-B ↗
17. Impact of contact evolution on the shelf life of organic solar cells10.1039/b910213b ↗
18. Water-induced degradation of polymer solar cells studied by h2o-o18 labeling10.1021/am800039w ↗
19. Air-stable polymer electronic devices10.1002/adma.200602653 ↗
20. Air-stable inverted flexible polymer solar cells using zinc oxide nanoparticles as an electron selective layer10.1063/1.2945281 ↗
21. Air stable polymer photovoltaics based on a process free from vacuum steps and fullerenes10.1016/j.solmat.2008.01.013 ↗
22. Highly durable inverted-type organic solar cell using amorphous titanium oxide as electron collection electrode inserted between ITO and organic layer10.1016/j.solmat.2008.06.012 ↗
23. Degradation of organic solar cells due to air exposure10.1016/j.solmat.2006.06.041 ↗
24. Lifetimes of organic photovoltaics: photochemistry, atmosphere effects and barrier layers in ITO-MEHPPV:PCBM-aluminium10.1016/j.solmat.2004.09.002 ↗
25. Effect of buffer layers on stability pf polymer-based organic solar cells10.1143/JJAP.49.01AC02 ↗
26. 2004
27. Effect of interchain interactions on the absorption and emission of poly(3-hexylthiophene)10.1103/PhysRevB.67.064203 ↗
28. Two-dimensional electronic excitations in self-assembled conjugated polymer nanocrystals10.1126/science.287.5454.839 ↗
29. Stability of the interface between indium-tin-oxide and poly(3,4-ethylenedioxythiophene)/poly(styrenesulfonate) in polymer light-emitting diodes10.1063/1.1315344 ↗
30. Modification of PEDOT:PSS as hole injection layer in polymer LEDs10.1002/pssa.200404338 ↗
31. Clevios website: .
32. Lifetime of organic light emitting diodes on polymer anodes10.1063/1.2975369 ↗
33. A roll-to-roll process to flexible polymer solar cells: model studies, manufacture and operational stability studies10.1039/b823001c ↗
34. Degradation patterns in water and oxygen of an inverted polymer solar cell10.1021/ja106299g ↗
35. Nature of non-emissive black spots in polymer light-emitting diodes by in-situ micro-Raman spectroscopy10.1002/1521-4095(20020205)14:3<206::AID-ADMA206>3.0.CO;2-J ↗
36. Ultralow power microfuses for write-once read-many organic memory elements10.1002/adma.200800960 ↗
37. Formation of bubbles on electrical contacts to polymer light-emitting diode devices10.1016/j.tsf.2004.10.039 ↗
38. Long-term operational lifetime and degradation analysis of P3HT:PCBM photovoltaic cells solar energy materials and solar cells
39. Sol–gel processed CuOx thin film as an anode interlayer for inverted polymer solar cells10.1016/j.orgel.2010.08.009 ↗
40. Efficient polymer photovoltaic cells using solution-processed MoO3 as anode buffer layer10.1016/j.solmat.2010.01.004 ↗
41. Performance and stability improvement of P3HT:PCBM-based solar cells by thermally evaporated chromium oxide (CrOx) interfacial layer10.1021/am100541d ↗
42. Longterm stability of efficient inverted P3HT:PCBM solar cells10.1016/j.solmat.2008.12.022 ↗