Temperature dependence of initial deformation and cracks of indium tin oxide film by quasi-continuous-wave laser irradiations

Liping Peng, Yuan’an Zhao, Xiaofeng Liu, Zhaoliang Cao, Dawei Li, Yafei Lian, Hao Ma, Ruijin Hong, Chunxian Tao, Dawei Zhang, Jianda Shao

Optical Materials Express· Volume 10· Issue 10

Abstract

In this study, we investigated the temperature dependence of the initial deformation and cracks of indium tin oxide (ITO) thin films deposited on a fused silica substrate using a 1064-nm quasi-continuous-wave laser. We observed that the laser-induced morphology threshold of the film shows a dramatic thickness effect. The laser-induced morphology threshold of a 100-nm ITO film is four times that of a 300-nm ITO film. Initial laser-induced surface morphologies of the initial deformation and cracks will occur as long as temperature rises to about 520 K and 1250 K, respectively, irrespective of the thickness of a film. Experimental results indicate that a thin ITO film is more likely to tolerate laser irradiation because of lower absorptivity than a thicker ITO film. Studying the temperature effect helps clarify more about the laser annealing process, which is a promising process in improving the performance of the ITO films.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Surface Roughness and Optical Measurements · Laser Material Processing Techniques · Thin-Film Transistor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Hu · Photonics Res. · 2020 · 8 · 27910.1364/PRJ.381262 ↗
2. Ellmer · Nat. Photonics · 2012 · 6 · 80910.1038/nphoton.2012.282 ↗
3. Li · Photonics Res. · 2019 · 7 · 47310.1364/PRJ.7.000473 ↗
4. Pawlewicz · Appl. Phys. Lett. · 1979 · 34 · 19610.1063/1.90727 ↗
5. Wu · Photonics Res. · 2018 · 6 · 109410.1364/PRJ.6.001094 ↗
6. Ling · Liq. Cryst. · 2016 · 43 · 206210.1080/02678292.2016.1196506 ↗
7. Zhou · Appl. Phys. B · 2018 · 124 · 3510.1007/s00340-018-6905-1 ↗
8. Marshall · Proc. SPIE · 2012 · 8475 · 84750U10.1117/12.929918 ↗
9. Yoo · Phys. Status Solidi A · 2019 · 216 · 190045910.1002/pssa.201900459 ↗
10. Bhopal · Vacuum · 2016 · 133 · 10810.1016/j.vacuum.2016.09.001 ↗
11. Kim · J. Appl. Phys. · 1999 · 86 · 645110.1063/1.371708 ↗
12. Yoo · Opt. Express · 2017 · 25 · 2553310.1364/OE.25.025533 ↗
13. Hu · Vacuum · 2004 · 75 · 18310.1016/j.vacuum.2004.01.081 ↗
14. Chen · Opt. Lasers Eng. · 2012 · 50 · 49110.1016/j.optlaseng.2011.10.002 ↗
15. Gui · Sci. Rep. · 2019 · 9 · 1127910.1038/s41598-019-47631-5 ↗
16. Wang · Opt. Mater. Express · 2017 · 7 · 272710.1364/OME.7.002727 ↗
17. Yoo · Opt. Express · 2016 · 24 · 1761610.1364/OE.24.017616 ↗
18. Jae-Hyuck · Opt. Mater. Express · 2017 · 7 · 81710.1364/OME.7.000817 ↗
19. Alam · Science · 2016 · 352 · 79510.1126/science.aae0330 ↗
20. de Ceglia · Phys. Rev. B · 2013 · 87 · 15514010.1103/PhysRevB.87.155140 ↗
21. Luk · Appl. Phys. Lett. · 2015 · 106 · 15110310.1063/1.4917457 ↗
22. Lee · Photonics Res. · 2020 · 8 · 104910.1364/PRJ.385249 ↗
23. Eshaghi · Optik · 2014 · 125 · 147810.1016/j.ijleo.2013.09.011 ↗
24. Kumar · Appl. Surf. Sci. · 2011 · 257 · 307510.1016/j.apsusc.2010.10.119 ↗
25. Wu · Proc. SPIE · 1996 · 2714 · 29410.1117/12.240357 ↗
26. Chow · Appl. Opt. · 2000 · 39 · 65010.1364/AO.39.000650 ↗
27. Wang · Opt. Express · 2011 · 19 · 2428610.1364/OE.19.024286 ↗
28. Ya-Hsin · Opt. Express · 2017 · 25 · 3313410.1364/OE.25.033134 ↗
29. Peng · Opt. Mater. Express · 2019 · 9 · 91110.1364/OME.9.000911 ↗
30. Xiao · Appl. Phys. A: Mater. Sci. Process. · 2012 · 107 · 33310.1007/s00339-012-6820-y ↗
31. El-Nahass · Mater. Sci. Eng., B · 2012 · 177 · 14510.1016/j.mseb.2011.10.018 ↗
32. Elsner · Thin Solid Films · 1990 · 185 · 18910.1016/0040-6090(90)90018-9 ↗
33. Gu · Adv. Polym. Technol. · 2001 · 20 · 1410.1002/1098-2329(200121)20:1<14::AID-ADV1001>3.0.CO;2-S ↗