Low-temperature NIR-VUV optical constants of (001) LaAlO3 crystal
Source abstract
Abstract
The optical constants and dielectric function of (001) LaAlO3 crystal were investigated at low temperatures down to 10 K in the NIR-VUV spectral range (photon energies 0.8-8.8 eV). Reflection variable angle spectroscopic ellipsometry and transmission spectroscopy were applied. Interband transitions were examined using the Tauc plots and the critical-point analysis. At room temperature, the indirect bandgap of 5.6 ± 0.01 eV and the lowest-energy direct transition at 7.2 ± 0.03 eV were detected. On cooling to 10 K, a blueshift of ∼0.2 eV and ∼0.1 eV was observed for the indirect and direct transitions, respectively. In the transparency spectral range, the index of refraction was found to be nearly temperature-independent and vary with photon energy from 2.0 (1 eV) to 2.5 (5.5 eV). It was suggested that the excellent thermal stability of the index of refraction may be related to the revealed thermally stable interband transitions. The results are of importance for modeling and design of modern optical devices.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Electronic and Structural Properties of Oxides · Luminescence Properties of Advanced Materials · Photorefractive and Nonlinear Optics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Institute of Physics of the Czech Academy of Sciences
Czech Technical University in Prague
University of Oulu
Funding
European Structural and Investment Funds and the Ministry of Education, Youth and Sports of the Czech Republic through Programme "Research, Development and Education" · The Grant Agency of the Czech Technical University in Prague
References (32)
Show source-provided references
1. Pompeo · Measurement · 2017 · 98 · 41410.1016/j.measurement.2015.07.058 ↗
2. Klein · IEEE Trans. Appl. Supercond. · 1999 · 9 · 357310.1109/77.783802 ↗
3. Lv · J. Alloys Compd. · 2013 · 580 · 61410.1016/j.jallcom.2013.07.161 ↗
4. Zhang · J. Nanosci. Nanotechnol. · 2014 · 14 · 382710.1166/jnn.2014.7997 ↗
5. Xing · Opt. Lett. · 2009 · 34 · 167510.1364/OL.34.001675 ↗
6. Guo · Appl. Opt. · 2010 · 49 · 567810.1364/AO.49.005678 ↗
7. Ortmann · ACS Nano · 2018 · 12 · 768210.1021/acsnano.8b01293 ↗
8. Ortmann · Opt. Mater. Express · 2019 · 9 · 298210.1364/OME.9.002982 ↗
9. Simon · Appl. Phys. Lett. · 1988 · 53 · 267710.1063/1.100543 ↗
10. Koren · Supercond. Sci. Technol. · 2002 · 15 · 311133510.1088/0953-2048/15/9/311 ↗
11. Michael · Phys. C (Amsterdam, Neth.) · 1994 · 235240 · 71710.1016/0921-4534(94)91582-2 ↗
12. Subramanyam · J. Appl. Phys. · 1992 · 72 · 239610.1063/1.351583 ↗
13. Lim · J. Appl. Phys. · 2002 · 91 · 450010.1063/1.1456246 ↗
14. Nelson · J. Vac. Sci. Technol., A · 2012 · 30 · 06140410.1116/1.4754811 ↗
15. Chernova · Opt. Mater. Express · 2017 · 7 · 384410.1364/OME.7.003844 ↗
16. Willett-Gies · Thin Solid Films · 2014 · 571 · 62010.1016/j.tsf.2013.11.140 ↗
17. Chemical mechanical polishing method and practice
18. Chemical-mechanical polishing (CMP): a controlled tribocorrosion process
19. Fox · 2001
20. Gibbons · IEEE Trans. Appl. Supercond. · 1997 · 7 · 217710.1109/77.621025 ↗
21. Tompkins · 2005
22. Fujiwara · Phys. Rev. B · 2000 · 61 · 1083210.1103/PhysRevB.61.10832 ↗
23. Jellison Jr · J. Appl. Phys. · 2010 · 107 · 01351410.1063/1.3272909 ↗
24. Aoki · J. Electrochem. Soc. · 1996 · 143 · L19110.1149/1.1837082 ↗
25. Luo · J. Appl. Phys. · 2008 · 104 · 05350310.1063/1.2973671 ↗
26. Tauc · Phys. Status Solidi B · 1966 · 15 · 62710.1002/pssb.19660150224 ↗
27. Davis · Philos. Mag. · 1970 · 22 · 090310.1080/14786437008221061 ↗
28. Mott · 1979
29. Viezbicke · Phys. Status Solidi B · 2015 · 252 · 170010.1002/pssb.201552007 ↗
30. Lautenschlager · Phys. Rev. B · 1987 · 36 · 482110.1103/PhysRevB.36.4821 ↗
31. Logothetidis · Phys. Rev. · 1986 · 34 · 245810.1103/PhysRevB.34.2458 ↗
32. Tyunina · APL Mater. · 2020 · 8 · 07110710.1063/5.0007209 ↗