The influence of defects formed by Ca excess and thermal post-treatments on the persistent luminescence of CaTiO_3:Pr
Source abstract
Abstract
Red emitting CaTiO3:Pr phosphors with a nominal composition of Ca0.998+xPr0.002TiO3+δ (0.02≤x≤0.04) were prepared by solid state reactions with different thermal post treatments and characterized by X-ray diffraction, transmission electron microscopy and photoluminescence. The Ca excess exhibited complete solubility up to 4% in the samples treated at 1400 °C but segregation in the form of Ruddlesden-Popper phases (Ca3Ti2O7 - Ca4Ti3O10) was observed in samples prepared at 1500 °C. The increase in temperature for stoichiometric samples showed a monotonic increase of decay time due to the reduction of non-radiative recombination defects. It was found that the Ca excess favored the formation of oxygen vacancies which are known to act as trap. In the samples treated at 1400 °C, 3% of Ca excess showed to be the best concentration to increase the decay time of persistent luminescence. For the samples treated at 1500 °C, the segregation of Ruddlesden-Popper phases left a constant amount of Ca soluble in all the CaTiO3 samples. This constant concentration of Ca caused the same density of defects and, consequently, the same decay time in all samples.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Radiation Detection and Scintillator Technologies · Ferroelectric and Piezoelectric Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Matsuzawa · J. Electrochem. Soc. · 1996 · 143 · 267010.1149/1.1837067 ↗
2. Lin · Mater. Lett. · 2001 · 51 · 1410.1016/S0167-577X(01)00257-9 ↗
3. Smet · J. Electrochem. Soc. · 2009 · 156 · H24310.1149/1.3073551 ↗
4. Wang · Mater. Chem. Phys. · 2003 · 80 · 110.1016/S0254-0584(02)00097-4 ↗
5. Lecointre · J. Phys. Chem. C · 2011 · 115 · 421710.1021/jp108038v ↗
6. Jia · J. Appl. Phys. · 2000 · 88 · 340210.1063/1.1286419 ↗
7. Wang · J. Lumin. · 2003 · 102–103 · 3410.1016/S0022-2313(02)00541-0 ↗
8. Yu · Mater. Lett. · 2004 · 58 · 366110.1016/j.matlet.2004.05.085 ↗
9. Van den Eeckhout · J. Lumin. · 2009 · 129 · 114010.1016/j.jlumin.2009.05.007 ↗
10. Pan · J. Solid State Chem. · 2003 · 174 · 6910.1016/S0022-4596(03)00175-0 ↗
11. Chedha · SID Int. Symp. Digest Tech. Papers · 1994 · 51 · 51
12. Jia · J. Lumin. · 2006 · 119–120 · 1310.1016/j.jlumin.2005.12.067 ↗
13. Jacobsen · J. Soc. Inf. Disp. · 1996 · 4 · 33110.1889/1.4731187 ↗
14. Zhang · J. Alloy. Comp. · 2010 · 498 · 15210.1016/j.jallcom.2010.03.138 ↗
15. Yin · J. Alloy. Comp. · 2007 · 441 · 32710.1016/j.jallcom.2006.09.120 ↗
16. Zhang · J. Lumin. · 2007 · 122–123 · 95810.1016/j.jlumin.2006.01.337 ↗
17. Zhang · J. Phys. Chem. C · 2007 · 111 · 1804410.1021/jp076128l ↗
18. Zhou · J. Mater. Sci. Mater. Electron. · 2002 · 13 · 69710.1023/A:1021552602704 ↗
19. Zhu · Physica B · 2011 · 406 · 269710.1016/j.physb.2011.04.010 ↗
20. Ceh · J. Mater. Sci. · 1994 · 29 · 629510.1007/BF00354574 ↗
21. Elcombe · Acta Crystallogr. B · 1991 · 47 · 30510.1107/S0108768190013416 ↗
22. Balachandran · Mater. Sci. Eng. · 1982 · 54 · 22110.1016/0025-5416(82)90116-1 ↗
23. Ruddlesden · Acta Crystallogr. · 1958 · 11 · 5410.1107/S0365110X58000128 ↗
24. Beznosikov · Crystallogr. Rep. · 2000 · 45 · 79210.1134/1.1312923 ↗
25. Kwestroo · J. Am. Ceram. Soc. · 1959 · 42 · 29210.1111/j.1151-2916.1959.tb12957.x ↗
26. Okamoto · J. Appl. Phys. · 2002 · 91 · 549210.1063/1.1458050 ↗