Highly photoluminescent polymer films deposited on glass and flexible substrates based on partially oxidized silicon nanocrystals
Source abstract
Abstract
In this work, optical properties of Silicon (Si) Oxide powders with Si nanocrystals (Si-nCs) embedded in a polymeric matrix (polymethyl methacrylate-PMMA) on BK7 glass and flexible substrates (acetate) are reported. The Si oxide powders were exfoliated from porous silicon layers (PSLs) with porosities of 57–98.3% obtained at 65 mA. The PSLs were obtained by electrochemical etching using, Si p-type (110), ρ=0.25-0.6 Ω-cm. For this, current densities of 65 mA and 35 mA were used with hydrofluoric acid and ethanol solution (Hf:EtOH) in (3:1), (1:3), (1:2), and (1:1) proportions respectively. To passivate and preserve the Photoluminescence (PL), the Si-oxide powders collected from exfoliation of PSLs were immersed at the polymeric matrix and deposited on acetate and BK7 glass substrates by spin-coating method. The PSLs were characterized by Photoluminescence (PL), Scanning Electron Microscopy (SEM) and X-ray spectroscopy (EDS). Subsequently, Si-oxide powders as a polymeric film exhibited strong PL emission either on acetate or on BK7 glass substrates, for which samples were characterized by PL and Raman measurements. The presence of oxidized Si-nCs were detected by Raman measurements, with average sizes between 1 to 1.5 nm, creating radiative defects (Si=O) that could be responsible of PL. The PSLs PL emission maximum position remained almost at the same wavelength even after when it is deposited on the polymer. In this manner, oxidized Si-nCs serve as effective passivating agents for PL. • SiOPF films were obtained from exfoliated PSLs and transferred onto BK7 and acetate substrates. • SiOPF exhibit PL emission in the 550–700 nm range, and their PL intensity depends on oxygen content and the initial PSLs porosity. • Raman analysis confirms oxidized Si–nCs with crystal sizes of 1–1.5 nm. • A blue shift in PL emission is observed in the SiOPF/BK7 and SiOPF/acetate samples as the oxygen concentration increases.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Silicon Nanostructures and Photoluminescence · Silicon Effects in Agriculture · Thin-Film Transistor Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Light-emitting porous silicon10.1016/0254-0584(95)01493-4 ↗
2. Silicon quantum wire array fabrication by electrochemical and chemical dissolution of wafers10.1063/1.103561 ↗
3. The origin of visible luminescencefrom ‘porous silicon’: a new interpretation10.1016/0038-1098(92)90815-Q ↗
4. Role of interfacial oxide-related defects in the red-light emission in porous silicon10.1103/PhysRevB.49.2238 ↗
5. Emission mechanisms of Si nanocrystals and defects in SiO materials10.1155/2014/409482 ↗
6. Electronic states and luminescence in porous silicon quantum dots: the role of oxygen10.1103/PhysRevLett.82.197 ↗
7. A review on solar cells from Si-single crystals to porous materials and Quantum dots10.1016/j.jare.2013.10.001 ↗
8. Growth of silicon quantum dots by oxidation of the silicon nanocrystals embedded within silicon carbide matrix10.1063/1.4897378 ↗
9. Temperature dependent photoluminescence from porous silicon nanostructures: Quantum confinement and oxide related transitions10.1063/1.3657771 ↗
10. A silicon nanocrystals/polymer nanocomposite as down-conversion layer in organic and hybrid solar cells10.1039/C5NR02703A ↗
11. Study of the photon down-conversion effect produced by thin silicon-rich oxide films on silicon solar cells10.1002/er.3622 ↗
12. Down-conversion effect created by SiOx films obtained by HFCVD and applied over Pn-Junctions10.1007/s12633-018-0029-4 ↗
13. Highly stabilized gradient alloy quantum dots and silica hybrid nanospheres by core double shells for photoluminescence devices10.1021/acs.jpclett.9b03578 ↗
14. Interfacial optimization of quantum dot and silica hybrid nanocomposite for simultaneous enhancement of fluorescence retention and stability10.1063/5.0026314 ↗
15. Effect of HF concentration on physical and electronic properties of electrochemically formed nanoporous silicon
16. Effects of thermal oxidation on the photoluminescence properties of porous silicon10.1016/j.jlumin.2009.11.018 ↗
17. Surface chemistry, reactivity, and pore structure of porous silicon oxidized by various methods10.1021/la301642w ↗
18. Photoluminescence from defect centers in high-purity silica glasses observed under 7.9-eV excitation
19. Blue photo- and electroluminescence of silicon dioxide layers ion-implanted with group IV elements10.1007/PL00006966 ↗
20. Raman shifts in Si nanocrystals10.1063/1.117371 ↗
21. Raman spectroscopy of porous silicon substrates10.1016/j.ijleo.2018.08.084 ↗
22. Improved one-phonon confinement model for an accurate size determination of silicon nanocrystals10.1063/1.370988 ↗
23. Raman investigation of ring configurations in vitreous silica10.1038/292140a0 ↗
24. Kinetics of solid phase crystallization of amorphous silicon analyzed by Raman spectroscopy10.1063/1.4818949 ↗
25. Crystallization processes of amorphous Si by thermal annealing and pulsed laser processing10.1088/1757-899X/23/1/012035 ↗