KOH-based shallow etching for exposing subsurface damage and increasing laser damage resistance of fused silica optical surface
Source abstract
Abstract
Abstract HF-based wet deep etching is an effective method for improving the laser damage resistance of fused silica optics. However, the fact that the etching process involves HF reaction makes the operation very unsafe. Potassium hydroxide (KOH) has recently shown great potential to outperform the more commonly used HF-acid as an etchant for the damage resistance enhancement of fused silica optical surface. In this paper, we present a detailed investigation into how the KOH-based shallow etching process affects the polished surface of fused silica. The results show that KOH-based etching does a good job at exposing the subsurface damage and increasing the laser damage threshold of fused silica while keeping the surface roughness nearly unchanged. Potential factors that limit the further increase in surface damage threshold of fused silica are also delved. The study offers an exciting option for fabricating high-quality fused silica optics with shallow wet etching under higher safety conditions that cannot be achieved with conventional HF-based wet etching approaches.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Laser Material Processing Techniques · Advanced Surface Polishing Techniques · Surface Roughness and Optical Measurements
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (30)
Show source-provided references
1. Ignition on the National Ignition Facility: a path towards inertial fusion energy10.1088/0029-5515/49/10/104022 ↗
2. Subsurface defects of fused silica optics and laser induced damage at 351 nm10.1364/OE.21.012204 ↗
3. Progress in the understanding of fracture related laser damage of fused silica
4. Sub-surface mechanical damage distributions during grinding of fused silica10.1016/j.jnoncrysol.2006.09.012 ↗
5. The distribution of subsurface damage in fused silica10.1117/12.638821 ↗
6. Oxygen plasma etching of fused silica substrates for high power laser optics10.1016/j.apsusc.2018.05.105 ↗
7. Optimum inductively coupled plasma etching of fused silica to remove subsurface damage layer10.1016/j.apsusc.2015.07.168 ↗
8. Combined technique of elastic magnetorheological finishing and HF etching for high-efficiency improving of the laser-induced damage threshold of fused silica optics10.1364/AO.53.000598 ↗
9. Capping a glass thin layer on the etched surface via plasma chemical vapor deposition for improving the laser damage performance of fused silica10.1364/OE.27.002268 ↗
10. Mitigation of organic laser damage precursors from chemical processing of fused silica10.1364/OE.22.029568 ↗
11. High fluence laser damage precursors and their mitigation in fused silica10.1364/OE.22.005839 ↗
12. HF-Based etching processes for improving laser damage resistance of fused silica optical surfaces10.1111/j.1551-2916.2010.04112.x ↗
13. The effect of HF/NH4F etching on the morphology of surface fractures on fused silica10.1016/j.jnoncrysol.2009.01.037 ↗
14. Subsurface defects characterization and laser damage performance of fused silica optics during HF-etched process10.1016/j.optmat.2013.11.022 ↗
15. Effects of deep wet etching in HF/HNO3 and KOH solutions on the laser damage resistance and surface quality of fused silica optics at 351 nm10.1364/OE.25.004607 ↗
16. Optimisation of ultrafast laser assisted etching in fused silica10.1364/OE.26.024343 ↗
17. Comparison of fabrication methods for microstructured deep UV multimode waveguides based on fused silica
18. Selective, laser-induced etching of fused silica at high scan-speeds using KOH10.2961/jlmn.2014.02.0009 ↗
19. Advanced mitigation process (AMP) for improving laser damage threshold of fused silica optics10.1038/srep31111 ↗
20. Effects of combined process of reactive ion etching and dynamic chemical etching on UV laser damage resistance and surface quality of fused silica optics10.1364/OE.26.018006 ↗
21. ISO 11254: an international standard for the determination of the laser-induced damage threshold10.1117/12.180881 ↗
22. Origins of a damage-induced green photoluminescence band in fused silica revealed by time-resolved photoluminescence spectroscopy10.1364/OME.7.002888 ↗
23. Impact of heat treatment on NBOHC luminescence of OH-containing and H2-impregnated fused silica for deep-ultraviolet applications10.1016/j.jlumin.2019.01.028 ↗
24. Correlation between 193nm absorption and photoluminescence-related defects for fused silica materials10.1364/OME.8.000775 ↗
25. Damage growth characteristics of different initial damage sites of fused silica under 355nm small laser beam irradiation10.1016/j.optlastec.2013.10.006 ↗
26. Optical defects produced in fused silica during laser-induced breakdown10.1063/1.1573364 ↗
27. Green luminescence in silica glass: a possible indicator of subsurface fracture10.1063/1.3693393 ↗
28. SiO2: Ge photoluminescence: detailed mapping of the excitation-emission UV pattern10.1103/PhysRevB.57.3718 ↗
29. Salh · 2011
30. Reaction ion etching process for improving laser damage resistance of fused silica optical surface10.1364/OE.24.000199 ↗