journal article·2018-09-25

Effects of chip pretreatment and feeding segments on specific energy and pulp quality in TMP production

Christer Sandberg, Erik Nelsson, Birgitta A. Engberg, Jan-Erik Berg, Per Engstrand

Publisher page

Abstract

Abstract Increased wood softening and refining intensity have earlier been utilized to improve refining efficiency in mechanical pulping. We have evaluated a combination of increased softening by low dose sulphite chip pretreatment and increased intensity by feeding segment design in a TMP line for production of high quality printing papers. Norway spruce wood chips were preheated, compressed in an Impressafiner and impregnated with water or sodium sulphite solutions (Na2SO3 charges 3.6 and 7.2 kg/t). Chips were refined in two parallel 68” double disc refiners using two different refining conditions: standard bidirectional segments at normal production rate (9 t/h) and feeding segments at increased production rate (11.1–12.1 t/h). The feeding segments enabled a 30 % increase in production rate. Refining with feeding segments at 12.1 t/h production rate combined with chip pretreatment with 3.6 kg/t sodium sulphite reduced the specific energy 360 kWh/t (19 %) compared to refining with standard segments and no pretreatment. Pulp properties were similar for the two configurations. The combination of feeding segments and chip pretreatment with water reduced the specific energy 180 kWh/t (9 %). Implementation of most of the technology presented has reduced the electrical energy use for the mill by approximately 80 GWh/year.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Lignin and Wood Chemistry · Advanced Cellulose Research Studies · Recycling and Waste Management Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Holmen Paper AB , Paper Product Development , SE-601 88 Norrköping , Sweden

Now at HEAD Engineering AB , Enspännarvägen 1 , SE-131 52 Nacka Strand , Sweden

Mid Sweden University , FSCN , Department of Chemical Engineering , SE-851 70 Sundsvall , Sweden

Funding

Knowledge Foundation · Energimyndigheten

References (51)

Show source-provided references
1. Ahrel, I., Bäck, I. (1970) Thermomechanical pulp at Rockhammar, EUCEPA. In: Proc. Symp. Mech. Pulp. Oslo. pp. 83–91.
2. Andersson, S., Sandberg, C., Engstrand, P. (2012) Comparison of mechanical pulps from two stage HC single disc and HC double disc – LC refining. Appita J. 65(1):57–62.
3. Asplund, A., Bystedt, I. (1973) Development of the thermo-mechanical pulping method. In: Int. Mech. Pulping Conf. Stockholm, p. 15:1.
4. Atack, D. (1972) On the characterization of pressurized refiner mechanical pulps. Svensk Papperstidning 75(3):89–94.10.1016/0014-4827(72)90523-X ↗
5. Atack, D., Heitner, C., Stationwala, M.I. (1978) Ultra high yield pulping of eastern black spruce. Svensk Papperstidning 81(5):164–176.
6. Axelson, P., Simonson, R. (1982) Thermomechanical pulping with low addition of sulfite Part 1. Effects of mild sulfite treatment of spruce chips prior to defibration. Svensk Papperstidn. 85(15):R132–R139.
7. Becker, H., Höglund, H., Tistad, G. (1977) Frequency and temperature in chip refining. Pap. Puu 59(3):123–130.
8. Charters, M.T., Ward, R.O. (1973) Elevated temperature refining for high quality mechanical pulp. In: Int. Mech. Pulping Conf. Stockholm. pp. 16:1–16:20.
9. Engberg, B., Berg, J.-E. (2011) A comparative study of models describing high consistency refining. In: Int. Mech. Pulping Conf. Beijing. pp. 96–100.
10. Engstrand, P., Ferritsius, O., Björkqvist, O., Johansson, L. (2015) Mekmassainitiativet för energieffektivitet, e2mp-i. Report series FSCN 2015:58, Mid Sweden University, Sundsvall, ISBN 978-91-88025-56-2. In Swedish.
11. Ferritsius, O., Moldenius, S. (1985) The effect of impregnation method on CTMP properties In: 3rd Int. Symp. Wood Pulp. Chem. Vancouver, Canada, 91–100.
12. Ferritsius, O., Mörseburg, K., Ferritsius, R. (2014) BAT of CTMP and TMP plants with respect to quality development and energy efficiency. In: Int. Mech. Pulping Conf. Helsinki.
13. Gellerstedt, G. (1976) Reactions of lignin during sulfite pulping. Svensk Papperstidning 79(16):537–543.
14. Goring, D. (1963) Thermal softening of lignin, hemicellulose and cellulose. Pulp Paper Mag. Can. 64(12):T517–T528.
15. Heikkurinen, A., Vaarasalo, J., Karnis, A. (1993) Effect of initial defiberization on the properties of refiner mechanical pulp. J. Pulp Pap. Sci. 19(3):119–124.
16. Høydahl, H.-E., Solbakken, M., Dahlquist, G. (1995) TMP for SC grades – A challenge in fiber modelling. In: Int. Mech. Pulping Conf. Montreal, 233–241.
17. Irvine, G.M. (1985) The significance of the glass-transition of lignin in thermomechanical pulping. Wood Sci. Technol. 19:139–149.10.1007/BF00353074 ↗
18. Johansson, L., Peng, F., Simonson, R. (1997) Effects of temperature and sulfonation on shear deformation of spruce wood. Wood Sci. Technol. 31:105–117.10.1007/BF00705926 ↗
19. Karlström, A., Eriksson, K. (2014) Fiber energy efficiency part II: Forces acting on the refiner bars. Nord. Pulp Pap. Res. J. 29(2):332–343.10.3183/npprj-2014-29-02-p332-343 ↗
20. Karlström, A., Eriksson, K., Sikter, D., Gustavsson, M. (2008) Refining models for control purposes. Nord. Pulp Pap. Res. J. 23(1):129–138.10.3183/npprj-2008-23-01-p129-138 ↗
21. Karnis, A. (1994) The mechanism of fibre development in mechanical pulping. J. Pulp Pap. Sci. 20(10):J280–J288.
22. Kerekes, R.J. (2011) Force-based characterization of refining intensity. Nord. Pulp Pap. Res. J. 26(1):14–20.10.3183/npprj-2011-26-01-p014-020 ↗
23. Koran, Z. (1967) Electron microscopy of radial tracheid surface of black spruce separated by tensile failure at various temperatures. Tappi J. 50(2):60–67.
24. Koran, Z. (1981) Energy consumption in mechanical fibre separation as a function of temperature. Pulp Pap. Can. 82(6):TR40–TR44.
25. Kure, K.-A., Dahlqvist, G. (1998) Development of structural fibre properties in high intensity refining – Cross-sectional fibre dimensions are significantly changed in refining. Pulp Pap. Can. 99(7):59–63.
26. Kure, K.-A., Dahlqvist, G., Sabourin, M.J., Helle, T. (1999) Development of spruce fibre properties by a combination of a pressurized compressive pretreatment and high intensity refining. In: Int. Mech. Pulping Conf. Houston. pp. 427–433.
27. Kure, K.-A., Sabourin, M.J., Dahlqvist, G., Helle, T. (2000) Adjusting refining intensity by changing refiner plate design and rotational speed – Effects on structural fibre properties. J. Pulp Pap. Sci. 26:346–352.
28. Lai, Y.-Z., Iwamida, T. (1993) Effect of Chemical Treatments on Ultra-High-Yield Pulping. 1. Fibre Separation. Wood Sci. Technol. 27:195–203.10.1007/BF00192816 ↗
29. Lindholm, C.A., Kurdin, J.A. (1999) Chemimechanical pulping. In: Sundholm, J, Papermaking Science and Technology, Mechanical Pulping. Fapet Oy, Helsinki. pp. 223–249.
30. Lunan, W.E., Harris, G., Franzen, R. (1983) High Pressure Refining and Brightening in Thermomechanical Pulping. In: Tappi Pulping Conf. pp. 239–253.
31. McCrum, N.G., Read, B.E., Williams, G. (1967) Anelastic and Dielectric Effects. In: Polymeric Solids. Wiley, New York. pp. 1–25.
32. Miles, K.B. (1990) Refining intensity and pulp quality in high consistency chip refining. Pap. Puu 72(5):508–514.
33. Miles, K.B., May, W.D., Karnis, A. (1991) Refining intensity, energy consumption and pulp quality in two-stage chip refining. Tappi J. 74(3):221–230.
34. Muhić, D., Huhtanen, J. P., Sundström, L., Sandberg, C., Ullmar, M., Vuorio, P, Engstrand, P. (2011) Energy efficiency in double disc refining – Influence of intensity by segment design. Nord. Pulp Pap. Res. J. 26(3):224–231.10.3183/npprj-2011-26-03-p224-231 ↗
35. Murton, K., Duffy, G. (2005) The influence of pulp residence time on refining intensity and pulp quality. Appita J. 58(1):64–71.
36. Nelsson, E., Sandberg, C., Hildén, L., Daniel, G. (2012) Pressurised compressive chip pre-treatment of Norway spruce with a mill scale Impressafiner. Nord. Pulp Pap. Res. J. 27(1):56–62.10.3183/npprj-2012-27-01-p056-062 ↗
37. Nelsson, E., Sandberg, C., Svensson-Rundlöf, E., Engstrand, P., Fernando, D., Daniel, G. (2015) Low dosage sulphite pretreatment in a modern TMP-line. Nord. Pulp Pap. Res. J. 30(4):591–598.10.3183/npprj-2015-30-04-p591-598 ↗
38. Nurminen, I. (1999) Influence of refining temperature and intensity (disc rotating speed) on TMP energy consumption and pulp and fibre fraction properties. In: Int. Mech. Pulping Conf.. Houston. pp. 333–345.
39. Nygaard, J. (1997) Energy aspects on mechanical pulp, chemical pulp and recycled fibres. In: Int. Mech. Pulping Conf. Stockholm. pp. 17–27.
40. Omholt, I., Miles, K.B. (2008a) Preheating and Refining of Mechanical Pulp at High Temperature. Part I: Fibre Separation and Initial Development. J. Pulp Pap. Sci. 34(1):39–45.
41. Omholt, I., Miles, K.B. (2008b) Preheating and Refining of Mechanical Pulp at High Temperature. Part II: Final pulp properties. J. Pulp Pap. Sci. 34(1):46–50.
42. Sabourin, M.J. (2000) Evaluation of a compressive pretreatment process on TMP properties and energy requirements – It extends the quality and energy benefits of low-energy TMP processes. Pulp Pap. Can. 101(2):50–56.
43. Sabourin, M., Xu, E., Cort, B., Boileau, I., Waller, A. (1997) Optimizing residence time, temperature and speed to improve TMP pulp properties and reduce energy. Pulp Pap. Can. 98(4):38–45.
44. Salmén, L., Fellers, C. (1982) Fundamentals of energy consumption during viscoelastic and plastic deformation of wood. Trans. Tech. Sect. CPPA 8(4):TR93–TR99.
45. Schniewind, A.P., Barrett, J.D. (1972) Wood as a linear orthotropic viscoelastic material. Wood Sci. Technol. 6(1):43–57.10.1007/BF00351807 ↗
46. Stationwala, M.I. (1994) Production of high-quality and low-energy chemithermomechanical pulp. Tappi J. 77(2):113–119.
47. Strand, B.C., Falk, B., Moqvist, A., Jacksom, M. (1993) The effect of production rate on specific energy consumption in high consistency chip refining. In: Int. Mech. Pulping Conf. Oslo. pp. 143–151.
48. Sundholm, J., Heikkurinen, A., Mannström, B. (1988) The role of rate of rotation and frequency in refiner mechanical pulping. Pap. Puu 5:446–451.
49. Uhmeier, A., Salmén, L. (1996) Repeated large radial compression of heated spruce. Nord. Pulp Pap. Res. J. 11(3):171–177.10.3183/npprj-1996-11-03-p171-176 ↗
50. Wiberg, R., Forslund, M. (2011) Energiförbrukning i massa- och pappersindustrin (Energy use in the pulp- and paper industry 2011). In: Skogsindustrierna. Stockholm, Sweden. [in Swedish].
51. Widehammar, S. (2004) Stress-strain relationships for spruce wood: Influence of strain rate, moisture content and loading direction. Exp. Mech. 44(1):44–48.10.1007/BF02427975 ↗