The role of metal nanoparticles and nanonetworks in alloy degradation
Source abstract
Abstract
Oxide scale, which is essential to protect structural alloys from high-temperature degradation such as oxidation, carburization and metal dusting, is usually considered to consist simply of oxide phases. Here, we report on a nanobeam X-ray and magnetic force microscopy investigation that reveals that the oxide scale actually consists of a mixture of oxide materials and metal nanoparticles. The metal nanoparticles self-assemble into nanonetworks, forming continuous channels for carbon transport through the oxide scales. To avoid the formation of these metallic particles in the oxide scale, alloys must develop a scale without spinel phase. We have designed a novel alloy that has been tested in a high-carbon-activity environment. Our results show that the incubation time for carbon transport through the oxide scale of the new alloy is more than an order of magnitude longer compared with commercial alloys with similar chromium content.
Source: europepmc · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Catalytic Processes in Materials Science · nanoparticles nucleation surface interactions · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (31)
Show source-provided references
1. Ricker, R. E. Cost of corrosion. Science 252, 1232–1232 (1991).10.1126/science.252.5010.1232-a ↗
2. Brindle, R. & Winkel, D. Energy impacts of corrosion, energy efficiency and renewable energy annual report and presentation (2005), .
3. Zeng, Z. & Natesan, K. Relationship between the growth of carbon nanofilaments and metal dusting corrosion. Chem. Mater. 17, 3794–3801 (2005).10.1021/cm050712u ↗
4. Young, D. J. Metal dusting reaction mechanisms. Mater. Sci. Forum. 522, 15–26 (2006).10.4028/www.scientific.net/MSF.522-523.15 ↗
5. Jakobi, D. & Gommans, R. Typical failures in pyrolysis coils for ethylene cracking. Mater. Corros. 54, 881–886 (2003).10.1002/maco.200303731 ↗
6. Yamamoto, Y. et al. Creep-resistant, Al2O3-forming austenitic stainless steels. Science 316, 433–436 (2007).10.1126/science.1137711 ↗
7. Thurmer, K., Williams, E. & Reutt-Robey, J. Autocatalytic oxidation of lead crystallite surfaces. Science 297, 2033–2035 (2002).10.1126/science.297.5589.2033 ↗
8. Stierle, A. et al. X-ray diffraction study of the ultrathin Al2O3 layer on NiAl(110). Science 303, 1652–1656 (2004).10.1126/science.1094060 ↗
9. Wolf, I. & Grabke, H. J. A study on the solubility and distribution of carbon in oxides. Solid State Commun. 54, 5–10 (1985).10.1016/0038-1098(85)91021-X ↗
10. Hochman, R. F. in Proc. Symp. on Properties of High-Temperature Alloys with Emphasis on Environmental Effects (eds Foroulis, Z. A. & Pettit, F. S.) 715–732 (The Electrochemical Society, New Jersey, 1977).
11. Zeng, Z. & Natesan, K. Initiation of metal-dusting pits and a method to mitigate metal-dusting corrosion. Oxid. Met. 66, 1–20 (2006).10.1007/s11085-006-9032-z ↗
12. Baker, B. A., Hartmann, V. W., Shoemaker, L. E., McCoy, S. A. & Rajendran, S. A new nickel-base alloy for metal dusting resistance. Trans. Ind. Inst. Met. 56, 327–333 (2003).
13. Ackermann, H. et al. Metal dusting in low-NOx recirculation burners for fuel oil. Corros. Eng. Sci. Technol. 40, 233–238 (2005).10.1179/174327805X66281 ↗
14. Korkhaus, J. Failure mechanisms and material degradation processes at high temperatures in ammonia synthesis. Corros. Eng. Sci. Technol. 40, 204–210 (2005).10.1179/174327805X66245 ↗
15. Albertsen, J. Z., Grong, O., Mathiesen, R. H. & Schmid, B. Metallurgical investigation of metal dusting corrosion in plant-exposed nickel-based alloy 602CA. Corros. Eng. Sci. Technol. 40, 239–243 (2005).10.1179/174327805X66290 ↗
16. Nishiyama, Y., Otsuka, N. & Kudo, T. Metal dusting behaviour of Cr–Ni steels and Ni-base alloys in a simulated syngas mixture. Corros. Sci. 48, 2064–2083 (2006).10.1016/j.corsci.2005.08.008 ↗
17. Zhang, J., Cole, D. M. I. & Young, D. J. Alloying with copper to reduce metal dusting of nickel. Mater. Corros. 56, 756–764 (2005).10.1002/maco.200503876 ↗
18. Szakalos, P., Pettersson, R. & Hertzman, S. An active corrosion mechanism for metal dusting on 304L stainless steel. Corros. Sci. 44, 2253–2270 (2002).10.1016/S0010-938X(02)00053-7 ↗
19. Schneider, A., Viefhaus, H., Inden, G., Grabke, H. J. & Mullerlorenz, E. M. Influence of H2S on metal dusting. Mater. Corros. 49, 336–339 (1998).10.1002/(SICI)1521-4176(199805)49:5<336::AID-MACO336>3.0.CO;2-1 ↗
20. Di Gabriele, F., Stott, F. H. & Liu, Z. Effect of experimental conditions on the metal dusting phenomenon in several commercial nickel-base alloys. Mater. Corros. 58, 81–86 (2007).10.1002/maco.200603989 ↗
21. Grabke, H. J. Mechanisms and prevention of corrosion in carbonaceous gases. Mater. Sci. Forum 369, 101–108 (2001).10.4028/www.scientific.net/MSF.369-372.101 ↗
22. Wagner, C. Theory of the tarnishing process. Z. Phys. Chem. B21, 25–41 (1933).10.1515/zpch-1933-2105 ↗
23. Maak, F. & Wagner, C. Mindestgehalte von Legierungsbestandteilen für die Bildung von Oxydschichten hoher Schutzwirkung gegen Oxydation bei höheren Temperaturen. Mater. Corros. 12, 273–277 (1961).10.1002/maco.19610120502 ↗
24. Bergner, D. Diffusion of C, N and O in metals, diffusion in metals and alloys. Proc. Int. Conf. 671, 223–240 (1983).
25. Quadakkers, W. J, Piron-Abellan, J., Shemet, V. & Singheiser, L. Metallic interconnectors for solid oxide fuel cells—a review. Mater. High Temp. 20, 115–127 (2003).
26. Renner, F. U. et al. Initial corrosion observed on the atomic scale. Nature 439, 707–710 (2006).10.1038/nature04465 ↗
27. Schmutz, P. & Frankel, G. S. Corrosion study of AA2024-T3 by scanning Kelvin probe force microscopy and in situ atomic force microscopy scratching. J. Electrochem. Soc. 145, 2295–2306 (1998).10.1149/1.1838634 ↗
28. Buchanan, K. S., Zhu, X. B., Meldrum, A. & Freeman, M. R. Ultrafast dynamics of a ferromagnetic nanocomposite. Nano Lett. 5, 383–387 (2005).10.1021/nl0482377 ↗
29. Thayer, P. C. The Electrical Properties of Iron–Chromium Spinel, thesis for Degree of Doctor of Philosophy, Colorado State Univ., Fort Collins, Colorado (1972).
30. Natesan, K. & Zeng, Z. Argonne National Laboratory Report, ANL-07/30, 68–72, October, (2007).
31. Muller, F. & Kleppa, O. J. Thermodynamics of formation of chromite spinels. J. Inorg. Nucl. Chem. 35, 2673–2678 (1973).10.1016/0022-1902(73)80497-X ↗