Formation of Cobalt Oxide Nanotubes: Effect of Intermolecular Hydrogen Bonding between Co(III) Complex Precursors Incorporated onto Colloidal Templates
Source abstract
Abstract
Several water-soluble cobalt(III) complexes were employed as precursors to form cobalt oxide nanostructures. These complexes were incorporated into polyelectrolyte multilayers precoated onto colloidal particles, followed by calcination. Cobalt complexes with strong intermolecular hydrogen bonding form one-dimensional Co 3 O 4 nanotube structures. Short Co 3 O 4 nanotubes with defects and broken spheres are formed when cobalt complexes with weak or no intermolecular hydrogen bonding are used. The sites for disulfide bond formation present on some complexes were found to be unessential for the nanotube formation.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Polymer Surface Interaction Studies · Conducting polymers and applications · Dendrimers and Hyperbranched Polymers
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Department of Chemistry and Biochemistry, California State University, Los Angeles, Los Angeles, California 90032
References (26)
Show source-provided references
1. Martin C. R. · Science · 1994 · 266 · 196110.1126/science.266.5193.1961 ↗
2. Lieber C. M. · Solid State Commun. · 1998 · 107 · 61610.1016/S0038-1098(98)00209-9 ↗
3. Martin C. R. · Chem. Mater. · 1996 · 8 · 1746
4. Rao C. N. R. · Chemphyschem · 2001 · 2 · 105
5. Iijima S. · Nature · 1991 · 354 · 5810.1038/354056a0 ↗
6. Odom, T. W.; Hafner, J. H.; Lieber, C. M.Scanning probe microscopystudies of carbon nanotubes; Dresselhaus, M. S., Dresselhaus, G., Avouris, P. H., Ed.; Springer-Verlag Berlin: Berlin, Germany, 2001, pp 173−211.10.1007/3-540-39947-X_8 ↗
7. Bachtold A. · Science · 2001 · 294 · 132010.1126/science.1065824 ↗
8. O'Loughlin J. L. · J. Phys. Chem. B · 2001 · 105 · 192410.1021/jp0037100 ↗
9. Tenne R. · Nature · 1992 · 360 · 44610.1038/360444a0 ↗
10. Feldman Y. · Science · 1995 · 267 · 225
11. Loiseau A. · Phys. Rev. Lett. · 1996 · 76 · 474010.1103/PhysRevLett.76.4737 ↗
12. Krumeich F. · J. Am. Chem. Soc. · 1999 · 121 · 833110.1021/ja991085a ↗
13. Kasuga T. · Langmuir · 1998 · 14 · 316310.1021/la9713816 ↗
14. Pu L. · Angew. Chem., Int. Ed. Eng. · 2001 · 40 · 1493
15. Nakamura H. · J. Am. Chem. Soc. · 1995 · 117 · 2652
16. Li Y. · J. Am. Chem. Soc. · 2001 · 123 · 9905
17. Ghadiri M. R. · Nature · 1993 · 366 · 32710.1038/366324a0 ↗
18. Hong B. H. · J. Am. Chem. Soc. · 2001 · 123 · 74910.1021/ja003582t ↗
19. Jung J. H. · Nano Lett. · 2002 · 2 · 20
20. Wang D. · Chem. Mater. · 2001 · 13 · 371
21. Mayya K. S. · Nano Lett. · 2001 · 1 · 73010.1021/nl015622c ↗
22. Shi X. · Langmuir · 2002 · 18 · 910
23. Mw 0
24. Precursors · Inorg. Chem. · 1975 · 14 · 148110.1021/ic50149a008 ↗
25. Huang E. · Langmuir · 2001 · 17 · 1224
26. AFM images were collected in the contact mode with a Molecular Imaging (Phoenix, AZ) atomic force microscope. TEM measurements were performed on a JEOL JEM-2000 FX microscope operated at 200 kV. It is also capable of determining the electron diffraction pattern. SEM measurements were carried out with a Cambridge Stereoscan 250 instrument operated at 20 kV that is equipped with a Link energy-dispersive X-ray analyzer. The XRD measurements were carried out using a Rigaku X-ray diffractometer (Cu Ka radiation, 50 kV, 70 mA). PS particles incorporating cobalt complexes were placed onto silicon wafers, air-dried, and calcined for the XRD analysis.