Intelligent Strategy of Lithium Metal Reconstruction through Generation of a Protective Layer and Regulating Lithium Deposition
Source abstract
Abstract
Lithium metal has been considered as the most promising anode for next-generation batteries. However, its high reactivity with electrolyte and the growth of lithium dendrites hamper the application of lithium metal-based batteries. Herein, we demonstrate that lithium polyphosphides (Li x PPs) can be dissolved in diethyl carbonate (DEC) and used as a reconditioner for generating a protective layer and regulating deposition of the Li metal anode. Since Li x PPs are reduced prior to Li deposition in the lithiation process, their product can be a uniform and tight layer at the surface of the Li metal. The in situ-formed protection layer has superhigh Li ionic conductivity, and its thickness can be easily controlled by tuning the amount of Li x PPs, thus facilitating the interface stability. The Li–Li symmetry batteries show stable cycling performance at 2 mA cm –2 and 1 mAh cm –2 over 5000 h. Interestingly, it exhibits a self-healing function on scratched Li metal.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Battery Materials · Extraction and Separation Processes · Advanced Battery Materials and Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Chemical Engineering and Technology
Tianjin University
Jiangsu Key Laboratory for Chemistry of Low-Dimensional Materials
Huaiyin Normal University
Quzhou Institute for Innovation in Resource Chemical Engineering
Funding
Natural Science Foundation of Tianjin Municipality · National Key Research and Development Program of China · National Natural Science Foundation of China · Municipal Key R&D Program of Ningbo
References (34)
Show source-provided references
1. 10.1038/s41560-018-0199-810.1038/s41560-018-0199-8 ↗
2. 10.1002/adma.20170637510.1002/adma.201706375 ↗
3. 10.1002/adma.20190642710.1002/adma.201906427 ↗
4. 10.1002/adfm.20200282410.1002/adfm.202002824 ↗
5. 10.1021/acsenergylett.3c0050510.1021/acsenergylett.3c00505 ↗
6. 10.1021/acs.nanolett.8b0129510.1021/acs.nanolett.8b01295 ↗
7. 10.1021/acs.nanolett.0c0454610.1021/acs.nanolett.0c04546 ↗
8. 10.1021/acsenergylett.4c0134510.1021/acsenergylett.4c01345 ↗
9. 10.1002/smll.20231213210.1002/smll.202312132 ↗
10. 10.1021/acs.nanolett.0c0108510.1021/acs.nanolett.0c01085 ↗
11. 10.1021/acs.nanolett.1c0362410.1021/acs.nanolett.1c03624 ↗
12. 10.1016/j.esci.2022.02.00210.1016/j.esci.2022.02.002 ↗
13. 10.1021/acs.nanolett.3c0076410.1021/acs.nanolett.3c00764 ↗
14. 10.1039/D4EE01766H10.1039/D4EE01766H ↗
15. 10.1016/j.esci.2021.12.00310.1016/j.esci.2021.12.003 ↗
16. 10.1021/acs.nanolett.4c0173810.1021/acs.nanolett.4c01738 ↗
17. 10.1002/adma.20230867510.1002/adma.202308675 ↗
18. 10.1038/s41560-023-01387-510.1038/s41560-023-01387-5 ↗
19. 10.1002/adfm.20200083110.1002/adfm.202000831 ↗
20. 10.1002/smm2.120010.1002/smm2.1200 ↗
21. 10.1021/acsenergylett.3c0113410.1021/acsenergylett.3c01134 ↗
22. 10.1039/C8TA05102J10.1039/C8TA05102J ↗
23. 10.1021/acsnano.8b0034810.1021/acsnano.8b00348 ↗
24. 10.1016/j.ensm.2021.02.03010.1016/j.ensm.2021.02.030 ↗
25. 10.1002/adma.20060259210.1002/adma.200602592 ↗
26. 10.1002/zaac.20210035810.1002/zaac.202100358 ↗
27. 10.1103/PhysRevB.47.1386110.1103/PhysRevB.47.13861 ↗
28. 10.1016/S0038-1098(99)00369-510.1016/S0038-1098(99)00369-5 ↗
29. 10.1039/C8TA09057B10.1039/C8TA09057B ↗
30. 10.1016/0167-2738(94)90298-410.1016/0167-2738(94)90298-4 ↗
31. 10.1016/j.nanoen.2019.01.03510.1016/j.nanoen.2019.01.035 ↗
32. 10.1021/acs.chemmater.5b0420810.1021/acs.chemmater.5b04208 ↗
33. 10.1002/adma.20240357010.1002/adma.202403570 ↗
34. 10.1038/s41467-024-48889-810.1038/s41467-024-48889-8 ↗