Thermodynamic analysis of growth of iron oxide films by MOCVD using tris(t-butyl-3-oxo-butanoato)iron(III) as precursor
Source abstract
Abstract
Thermodynamic calculations, using the criterion of minimization of total Gibbs free energy of the system, have been carried out for the metalorganic chemical vapour deposition (MOCVD) process involving the β-ketoesterate complex of iron [tris(t-butyl-3-oxo-butanoato)iron(III) or Fe(tbob)3] and molecular oxygen. The calculations predict, under different CVD conditions such as temperature and pressure, the deposition of carbon-free pure Fe3O4, mixtures of different proportions of Fe3O4 and Fe2O3, and pure Fe2O3. The regimes of these thermodynamic CVD parameters required for the deposition of these pure and mixed phases have been depicted in a ‘CVD phase stability diagram’. In attempts at verification of the thermodynamic calculations, it has been found by XRD and SEM analysis that, under different conditions, MOCVD results in the deposition of films comprising pure and mixed phases of iron oxide, with no carbonaceous impurities. This is consistent with the calculations.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Roughness and Optical Measurements · Power Transformer Diagnostics and Insulation · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Apátiga L M and Castaño V M 2006 Thin Solid Films 496 57610.1016/j.tsf.2005.08.344 ↗
2. Bernard C, Pons C M, Blanquet E and Madar R 1999 MRS Bull. 24 2710.1557/S0883769400052155 ↗
3. Dhar S, Dharmaprakash M S and Shivashankar S A 2008 Bull. Mater. Sci. 31 6710.1007/s12034-008-0012-6 ↗
4. Eriksson G 1971 Acta Chem. Scand. 25 651
5. Fujii T, Takano M, Katano R and Bando Y 1989 J. Appl. Phys. 66 316810.1063/1.344154 ↗
6. Kang S Y, Choi K H, Lee S K, Hwang C S and Kim H J 2000 J. Electrochem. Soc. 147 116110.1149/1.1393330 ↗
7. Kingery W D, Bowen H K and Uhlmann D R 1976 Introduction to ceramics (New York: John Wiley and Sons)
8. Lee J Y, Kang B C, Jung D Y and Boo J H 2007 J. Vac. Sci. Technol. B25 151
9. Mane A U and Shivashankar S A 2003 J. Crystal Growth 254 36810.1016/S0022-0248(03)01156-4 ↗
10. Mathur S, Veith M, Sivakov V, Shen H, Huch V, Hartmann U and Gao H B 2002 Chem. Vap. Depos. 8 27710.1002/1521-3862(20021203)8:6<277::AID-CVDE277>3.0.CO;2-8 ↗
11. Mathur S, Sivakov V, Shen H, Barth S, Cavelius C, Nilsson A and Kuhn P 2006 Thin Solid Films 502 8810.1016/j.tsf.2005.07.249 ↗
12. Mukhopadhyay S, Shalini K, Lakshmi R, Devi A and Shivashankar S A 2002a Surf. Coat. Technol. 150 20510.1016/S0257-8972(01)01540-7 ↗
13. Mukhopadhyay S, Shalini K, Devi A and Shivashankar S A 2002b Bull. Mater. Sci. 25 39110.1007/BF02708016 ↗
14. Ottosson M and Carlsson J 1996 Surf. Coat. Technol. 78 28610.1016/0257-8972(95)02415-8 ↗
15. Paranjape M A, Mane A U, Raychaudhuri A K, Shalini K, Shivashankar S A and Chakravarty B R 2002 Thin Solid Films 413 810.1016/S0040-6090(02)00446-7 ↗
16. Park S, Lim S and Choi H 2006 Chem. Mater. 18 515010.1021/cm0601990 ↗
17. Pflitsch C, Viefhaus D, Bergmann U, Kravets V, Nienhaus H and Atakan B 2006 J. Electrochem. Soc. 153 C54610.1149/1.2205179 ↗
18. Shalini K, Subbanna G N, Chandrasekaran S and Shivashankar S A 2003 Thin Solid Films 424 5610.1016/S0040-6090(02)00903-3 ↗
19. Stringfellow G B 1989 Organometallic vapour phase epitaxy-theory and practice (New York: Academic Press) Ch. 3
20. Urs U K, Shalini K, Dharmaprakash M S, Shivashankar S A and Row T N G 2000 Acta Crystallogr. C56 e448