Abstract Understanding the growth of whiskers or high aspect ratio features on substrates can be aided when the crystallography of the feature is known. This study has evaluated three methods that utilize electron backscatter diffraction (EBSD) for the determination of the crystallographic growth direction of an individual whisker. EBSD has traditionally been a technique applied to planar, polished samples, and thus the use of EBSD for out-of-surface features is somewhat more difficult and requires additional steps. One of the methods requires the whiskers to be removed from the substrate resulting in the loss of valuable physical growth relationships between the whisker and the substrate. The other two techniques do not suffer this disadvantage and provide the physical growth information as well as the crystallographic growth directions. The final choice of method depends on the information required. The accuracy and the advantages and disadvantages of each method are discussed.
Source: crossref · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Electronic Packaging and Soldering Technologies · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (18)
Show source-provided references
1. 10.1063/1.166133310.1063/1.1661333 ↗
2. 10.1016/0026-0800(82)90028-310.1016/0026-0800(82)90028-3 ↗
3. 10.1016/S0304-3991(01)00137-110.1016/S0304-3991(01)00137-1 ↗
4. Oxford Instruments (n.d.). Growth direction and analysisof nanostructures by EBSD. Available at: http://www.oxford-instruments.com/products/x-ray-microanalysis/ebsd/ebsd-applications/Pages/Growth%20direction%20and%20orientation%20analysis%20of%20nanostructures.pdf.
5. 10.1063/1.243415310.1063/1.2434153 ↗
6. 10.1021/nl062442010.1021/nl0624420 ↗
7. 10.4028/www.scientific.net/MSF.467-470.46510.4028/www.scientific.net/MSF.467-470.465 ↗
8. 10.1021/cm071213r10.1021/cm071213r ↗
9. 10.1021/jp045556d10.1021/jp045556d ↗
10. 10.1016/B978-0-408-10642-9.50007-610.1016/B978-0-408-10642-9.50007-6 ↗
11. 10.1016/j.actamat.2005.07.01610.1016/j.actamat.2005.07.016 ↗
12. 10.1111/j.1365-2818.2007.01854.x10.1111/j.1365-2818.2007.01854.x ↗
13. 10.1016/0036-9748(74)90244-010.1016/0036-9748(74)90244-0 ↗
14. 10.1063/1.221535410.1063/1.2215354 ↗
15. 10.1088/0022-3727/41/10/10200510.1088/0022-3727/41/10/102005 ↗
16. Examination of nickel underlayer as a tin whisker mitigator
17. 10.1007/978-1-4615-0215-910.1007/978-1-4615-0215-9 ↗
18. 10.1063/1.172982910.1063/1.1729829 ↗