The diffusion bonding of a Si3N4-TiN composite with Ni, INVAR (Fe-Ni alloy), and IN600 (Ni-Cr-Fe alloy) interlayers has been investigated between 1100 °C and 1350 °C, under argon or nitrogen atmosphere. For the chosen bonding conditions, the Si3N4 phase of the composite reacts with the interlayer phase, leading to the release of silicon and nitrogen, whereas the TiN phase remains stable. The bonding mechanisms with nickel and INVAR (Ni-Fe alloy) interlayers are rather similar. Released silicon diffuses into the reaction layer and into the interlayer, forming a solid solution, whereas the released nitrogen remains gaseous. The bonding rate depends then on the elimination rate of nitrogen from the reaction interface. The thermal stability of these joints is very high up to 1100 °C. However, the interfacial porosity and the internal stresses created by the high nitrogen pressure are pernicious for the mechanical strength. The bonding mechanism with IN600 (Ni-Fe-Cr alloy) interlayer is rather different. The released nitrogen can form nitrides with interlayer elements (Cr, Al). Released silicon diffuses into the reaction layer and forms silicides. The joint porosity is less significant for the IN600 interlayer, which suggests a good mechanical strength. However, the formation of silicide is pernicious, because of the brittleness of these phases.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Metal and Thin Film Mechanics · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. K.H. Suzuki, H. Yoshida, and S. Yamaguki: U.S. Patent No. 4, 613, 455, 1986.
2. C.H. Murtry, W.D.G. Boecker, S.G. Seshadri, J.S. Zanghi, and J.E. Garnier: Am. Ceram. Soc. Bull., 1987, vol. 66, p. 325.
3. M. Higuchi, M. Miyake, H. Kakeuchi, and E. Kamjo: U.S. Patent 4, 659, 508, 1987.
4. C. Martin, P. Mathieu, and B. Cales: Proc. Symp. on Ceramic Materials Research, E-MRS Spring Conf., R.J. Brook, Strasbourg, 1988, ed., Elsevier, Amsterdam, 1989, pp. 107–11.
5. A. Bellosi, S. Guicciardi, and A. Tampieri: J. Eur. Ceram. Soc., 1992, vol. 9, pp. 83–93.10.1016/0955-2219(92)90049-J ↗
6. L. Esposito, A. Bellosi, and G. Celotti: Acta Mater., 1997, vol. 45 (12) pp. 5087–97.10.1016/S1359-6454(97)00154-7 ↗
7. R.H. Vegter and G. Den Ouden: J. Mater. Sci., 1998, vol. 33, pp. 4525–30.10.1023/A:1004400318343 ↗
8. K. Suganuma, K. Niihara, and F. Fujita: J. Less-Common Met., 1990, vol. 158, pp. 59–69.10.1016/0022-5088(90)90431-I ↗
9. E. Heikinheimo, A. Kodenstsov, J.A. Van Beek, J.T. Klomp, and F.J.J. Van Loo: Acta Metall. Mater., 1992, vol. 40, suppl., pp. S111-S119.10.1016/0956-7151(92)90270-O ↗
10. J.T. Klomp: in Designing Interfaces for Technological Applications: Ceramic-Ceramic, Ceramic-Metal Joining, S. D. Peteves, ed., 1989, pp. 127–43.
11. J.T. Klomp: in Chemistry and Kinetic Aspects of Metal Ceramic Diffusion Bonding, Joining Ceramics, Glass and Metal, W. Kraft, ed., 1989, pp. 55–64.
12. M.E. Brito, H. Yokoyama, Y. Hirotsu, and Y. Mutoh: Iron Steel Inst. Jpn. Int., 1989, vol. 29 (3), pp. 253–58.10.2355/isijinternational.29.253 ↗
13. F.J.J. Van Loo, J.H. Gulpen, and A. Kodentsov: Joining Ceramics, Glass and Metal, H. Krappitz and H. A. Schaeffer, eds., 1993, pp. 3–14.
14. K. Suganuma, T. Okamoto, and M. Shimada: High Temp. High Pressures, 1985, vol. 16, pp. 627–35.
15. K. Suganuma, M. Shimada, T. Okamoto, and M. Koizumi: BCS, 1984, vol. 34.
16. M. Koizumi, M. Takagi, K. Suganum, Y. Miyamoto, and T. Okamoto: in High Tech Ceramics, P. Vincenzini, ed., Amsterdam, 1987, Elsevier, Amsterdam, 1987, pp. 1233–39.
17. M. Courbière, M. Kinoshita, and I. Kondoh: in Joining Ceramics, Glass and Metal, W. Kraft, ed., 1989, pp. 95–102.
18. J.C. Schuster, F. Weitzer, J. Bauer, and H. Nowotny: Mater. Sci. Eng., 1988, vols. A105–A106, pp. 201–06.10.1016/0025-5416(88)90497-1 ↗
19. I. Gotman and E.Y. Gutmanas: J. Mater. Sci. Lett., 1989, vol. 8, pp. 1103–06.10.1007/BF01730502 ↗
20. I. Gotman and E.Y. Gutmanas: Proc. World Conf. on Powder Metallurgy, London, July 2–6, 1990.
21. J.C. Schuster: J. Mater. Sci., 1988, vol. 23, pp. 2792–96.10.1007/BF00547452 ↗
22. J. Vleugels, T. Laoui, K. Vercammen, J.P. Celis, and O. Van Der Biest: Mater. Sci. Eng., 1994, vol. A187, pp. 177–82.10.1016/0921-5093(94)90345-X ↗
23. G. Ceccone and S.D. Peteves: Proc. 3rd Euro-Ceramics, P. Duran & J.F. Fernandez, eds., 1993, Faenza Editrice Iberica S.L., San Vicente, Spain, vol. 3, pp. 337–42.
24. R.L. Mehan, M.R. Jackson, M.D. McConnell, and N. Lewis: J. Mater. Sci., 1983, vol. 18, pp. 508–14.10.1007/BF00560640 ↗
25. M. Nakamura and S.D. Peteves: J. Am. Ceram. Soc., 1990, vol. 73 (5), pp. 1221–27.10.1111/j.1151-2916.1990.tb05183.x ↗
26. S.D. Peteves, M. Moulaert, and M.G. Nicholas: Metall. Trans. A, 1992, vol. 23A, pp. 1773–81.10.1007/BF02804370 ↗
27. J. Vleugels and O. Van Ver Biest: J.Am. Ceram. Soc., 1995, vol. 78 (11), pp. 3002–08.
28. Smithel Metals Reference Book, 7th ed., E.A. Brandes, and G.B. Brook, eds, Butterworth-Heinemann, Oxford, 7th ed., 1992.
29. M.J. Bennet and M.R. Houlton: J. Mater. Sci., 1979, vol. 14 (1), pp. 1984–96.10.1007/BF01028343 ↗
30. S. Hertzman and M. Jarl: Metall. Trans. A, 1987, vol. 18A, pp. 1745–52.10.1007/BF02646206 ↗
31. K. Frisk: Metall. Trans. A, 1990, vol. 21A, pp. 2477–88.10.1007/BF02646992 ↗
32. T. Shimoo, K. Okamura, and M. Itoh: J. Mater. Sci., 1998, vol. 33, pp. 5169–75.10.1023/A:1004475702702 ↗