Halo Formation During Solidification of Refractory Metal Aluminide Ternary Systems

N. D’Souza, L. M. Feitosa, G. D. West, H. B. Dong

Abstract

Abstract The evolution of eutectic morphologies following primary solidification has been studied in the refractory metal aluminide (Ta-Al-Fe, Nb-Al-Co, and Nb-Al-Fe) ternary systems. The undercooling accompanying solid growth, as related to the extended solute solubility in the primary and secondary phases can be used to account for the evolution of phase morphologies during ternary eutectic solidification. For small undercooling, the conditions of interfacial equilibrium remain valid, while in the case of significant undercooling when nucleation constraints occur, there is a departure from equilibrium leading to unexpected phases. In Ta-Al-Fe, an extended solubility of Fe in σ was observed, which was consistent with the formation of a halo of μ phase on primary σ. In Nb-Al-Co, a halo of C14 is formed on primary CoAl, but very limited vice versa. However, in the absence of a solidus projection it was not possible to definitively determine the extended solute solubility in the primary phase. In Nb-Al-Fe when nucleation constraints arise, the inability to initiate coupled growth of NbAl3 + C14 leads to the occurrence of a two-phase halo of C14 + Nb2Al, indicating a large undercooling and departure from equilibrium.
Source: crossref · Quality: baseline

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Quasicrystal Structures and Properties · Solidification and crystal growth phenomena

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. M. F. X. Gigliotti Jr., G. A. Colligan, G. L. F. Powell, Mater. Trans., 1970, Vol. 1, pp. 891–97.
2. M. McLean, Directionally Solidified Materials for High Temperature Service. The Metal Society, Pittsburgh, 1983, p. 55.
3. P. Cerba, M. Vilasi, B. Malaman, J. Steinmetz, J. Alloys Compd, 1993, Vol. 201, pp. 57–60.10.1016/0925-8388(93)90861-G ↗
4. G. Ghosh, G. B. Olson, Acta Mater., 2007, Vol. 55, pp. 3281–3303.10.1016/j.actamat.2007.01.036 ↗
5. H.T. Pang, N. D’Souza, H.B. Dong, H.J. Stone, C.M.F. Rae, Met. Mater. Trans. A., 2016, Vol. 47A, pp. 889-90610.1007/s11661-015-3252-2 ↗
6. N. D’Souza, S. Simmonds, G.D. West, H.B. Dong, Met. Mater. Trans. A., 2013, Vol. 44A, pp. 4764-73.10.1007/s11661-013-1816-6 ↗
7. G. Brewster, N. D’souza, K.S. Ryder, S. Simmonds, and H.B. Dong: Met. Mater. Trans. A., 2012, vol. 43A, pp. 1288–1302.10.1007/s11661-011-1027-y ↗
8. G. Sauthoff, Intermetallics, 2008, Vol. 8, pp. 469–81.
9. L. Machon, G. Sauthoff, Intermetallics, 1996, Vol. 4, pp. 1101–1109.10.1016/0966-9795(96)00023-4 ↗
10. B. E. Sundquist, R. Bruscato, L. F. Mondolfo, J. Inst. Met., 1962 Vol. 91, p. 204
11. W. Kurz, D. J. Fisher, Fundamentals of Solidification, 1986, Trans Tech Publications Ltd., stafa zurich pp. 134–36
12. M. H. Burden, J. D. Hunt, J. Cryst. Growth, 1974, Vol. 22, pp. 109–16.10.1016/0022-0248(74)90127-4 ↗
13. K. A. Jackson, J. D. Hunt, Trans. Met. Soc., AIME, 1966, Vol. 236, pp. 1129–42.
14. J. D. Hunt, S-Z Lu, Handbook of Crystal Growth, 1994, Vol. 2. Ed. D. T. J. Hurle, pp. 1113–66.
15. M. D. Nave, A. K. Dahle, D. H. StJohn, Acta Mater. 2002, vol. 50, pp. 2837–49.10.1016/S1359-6454(02)00104-0 ↗
16. S. M. Li, B. L. Jiang, B. L. Ma, H. Z. Fu, J. Cryst. Growth, 2007, vol. 299, pp. 178–83.10.1016/j.jcrysgro.2006.10.255 ↗
17. K. W. Li, X. B. Wang, C. M. Li, W. X. Wang, S. P. Chen, D. Q. Gong, L. L. Cui, High Temp. Mater. Proc., 2015, vol. 34, pp. 479–85.
18. K. W. Li, S. M. Li, Y. L. Xue, H. Z. Fu, J. Cryst. Growth, 2012, vol. 357, pp. 30–34.10.1016/j.jcrysgro.2012.07.042 ↗
19. N. D’Souza, L. M. Feitosa, G. D. West, N. G. Jones, H. B. Dong, J. Alloy Comp., 2017, vol. 398, pp. 375–83.10.1016/j.jallcom.2016.12.149 ↗
20. L.M. Feitosa, N. D’Souza, G.D. West, H.B. Dong, Met. Mater. Trans. A., 2017, Vol. 48A, pp. 3811-14.
21. D. Welton, N. D’Souza, J. Kelleher, S. Gardner, Z.H. Dong, G.D. West, H.B. Dong, Met. Mater. Trans. A., 2015, vol. 46A, pp. 4298-15.10.1007/s11661-015-3046-6 ↗
22. V. Raghavan, J. Phase Eqlb. Diff., 2013, vol. 34, pp. 328–49.10.1007/s11669-013-0239-9 ↗
23. V. T. Witusiewicz et al, J. Mat. Sci., 2013, Vol. 48, pp. 377–12.10.1007/s10853-012-6755-x ↗
24. N. D’Souza, R. Beanland, C. Hayward, H. B. Dong, Acta Mater., 2011, vol. 59, pp. 1003–1013.10.1016/j.actamat.2010.10.031 ↗
25. M. Palm, C. He, O. Dovbenko, F. Stein, J. C. Schuster, J. Phase Eqlb. Diff., 2012, vol. 33, pp. 210–21.10.1007/s11669-012-0042-z ↗
26. O. Dovbenko, F. Stein, M. Palm, O. Prymak, Intermetallics, 2010, vol. 18, pp. 2191–2207.10.1016/j.intermet.2010.07.004 ↗
27. C. He, F. Stein, M. Palm, J. All. Comp., 2015, vol. 637, pp. 361–75.10.1016/j.jallcom.2015.02.182 ↗
28. F. Stein, C. He, O. Prymak, S. Voβ, I. Wossack, Intermetallics, 2015, vol. 59, pp. 43–58.10.1016/j.intermet.2014.12.008 ↗
29. C. He, Y. Qin, F. Stein, J. Phase. Eqlb., Diff., 2017, Vol. 38, pp. 771–87.10.1007/s11669-017-0566-3 ↗
30. C. Guo, T. Wu, C. Li, Z. Du, CALPHAD, 2107, vol. 57, pp. 78–87.10.1016/j.calphad.2017.03.005 ↗
31. W. J. Boettinger, U. R. Kattner, D. K. Banerjee, Modelling and Casting of Advanced Solidification Processes (MCWASP), VIII, Eds. B. G. Thomas, C. Beckermann, TMS, 1998, pp. 159–70.
32. E.C. Kurum, H.B. Dong, J.D. Hunt, Met. Mater. Trans. A, 2005, 36A, pp. 3103-10.10.1007/s11661-005-0082-7 ↗
33. N. D’Souza, H.B. Dong, Scripta Materialia, 2007, 56, pp. 41-44.10.1016/j.scriptamat.2006.08.060 ↗
34. D. G. McCartney, J. D. Hunt, R. M. Jordan, Met. Mater. Trans. A, 1980, vol. 11A, pp. 1243–49.10.1007/BF02653477 ↗
35. D. R. F. West, N. Saunders, Ternary Phase Diagrams in Materials Science, 2002, 3rd ed., Maney Publishing, Leeds, pp. 67–68