journal article·2013-01

Retardation of the Cu5Zn8 Phase Fracture and Improvement of Shear Strength of the Sn-9 wt pct Zn/Cu Interface by Inserting an Electroless Palladium Layer

Po-Hsun Lee, Chi-Pu Lin, Chih-Ming Chen

Publisher page

Abstract

A uniform layer of the Cu5Zn8 phase is formed at the Sn-9 wt pct Zn (Sn-9Zn)/Cu interface after reflow at 503 K (230 °C) but fractures very severely during subsequent solid-state aging at 443 K (170 °C). Such a severe fracture of an interfacial intermetallic compound deteriorates the integrity of joint interface and leads to excessive atomic interdiffusion as well as intermetallic compound growth. In the current study, it was observed that by inserting an electroless palladium (Pd) layer at the Sn-9Zn/Cu interface, a Pd2Zn9 phase is formed between Cu5Zn8 and Sn-9Zn solders. This Pd2Zn9 phase exhibits higher microstructural stability at the interface during solid-state aging and effectively retards the fracture of the Cu5Zn8 phase. The integrity of the Sn-9Zn/Cu interface is improved remarkably. Mechanical tests reveal that the shear strength of the Sn-9Zn/Cu joint is enhanced by inserting an electroless Pd layer at the interface.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. M. Date, K.N. Tu, T. Shoji, M. Fujiyoshi, and K. Sato: J. Mater. Res., 2004, vol. 19, pp. 2887–96.10.1557/JMR.2004.0371 ↗
2. K. Suganuma and K.S. Kim: J. Mater. Sci.: Mater. Electron., 2007, vol. 18, pp. 121–27.10.1007/s10854-006-9018-2 ↗
3. C.M. Chen and C.H. Chen: J. Electron. Mater., 2007, vol. 36, pp. 1363–71.10.1007/s11664-007-0226-1 ↗
4. C.H. Chen, C.P. Lin, and C.M. Chen: J. Electron. Mater., 2009, vol. 38, pp. 61–69.10.1007/s11664-008-0554-9 ↗
5. C.W. Huang and K.L. Lin: J. Mater. Res., 2004, vol. 19, pp. 3560–68.10.1557/JMR.2004.0458 ↗
6. T. Ichitsubo, E. Matsubara, K. Fujiwara, M. Yamaguchi, H. Irie, S. Kumamoto, and T. Anada: J. Alloy. Compd., 2005, vol. 392, pp. 200–05.10.1016/j.jallcom.2004.09.043 ↗
7. C.Y. Chou, S.W. Chen, and Y.S. Chang: J. Mater. Res., 2006, vol. 21, pp. 1849–56.10.1557/jmr.2006.0229 ↗
8. J.W. Yoon and S.B. Jung: J. Mater. Res., 2006, vol. 21, pp. 1590–99.10.1557/jmr.2006.0198 ↗
9. Y.W. Yen, P.H. Tsai, Y.K. Fang, S.C. Lo, Y.P. Hsieh, and C. Lee: J. Alloy. Compd., 2010, vol. 503, pp. 25–30.10.1016/j.jallcom.2010.04.241 ↗
10. W.H. Wu, C.S. Lin, S.H. Huang, and C.E. Ho: J. Electron. Mater., 2010, vol. 39, pp. 2387–96.10.1007/s11664-010-1351-9 ↗
11. Y.W. Yen, P.H. Tsai, Y.K. Fang, B.J. Chen, and C.P. Lee: J. Alloy. Compd., 2012, vol. 517, pp. 111–17.10.1016/j.jallcom.2011.12.046 ↗
12. J.Y. Wang, C.F. Lin, and C.M. Chen: Scripta Mater., 2011, vol. 64, pp. 633–36.10.1016/j.scriptamat.2010.12.006 ↗
13. C.Y. Chou and S.W. Chen: Acta Mater., 2006, vol. 54, pp. 2393–2400.10.1016/j.actamat.2006.01.014 ↗