Surface Modification of AISI 1045 Carbon Steel by the Electrolytic Plasma Process

M.R. Bayati, R. Molaei, K. Janghorban

Publisher page

Abstract

The electrolytic plasma process (EEP) was employed for surface modification of 1045 carbon steel for the first time, which resulted in a harder surface. Surface composition of the samples at different depths was evaluated by energy dispersive X-ray spectroscopy (EDS) and X-ray photoelectron spectroscopy (XPS), which revealed diffusion of Cr from the bath to ~15 μm beneath the surface of the samples during the test time of 10 minutes. The effects of applied voltage, test duration, and electrolyte concentration on the hardness and microstructure of the samples were investigated by microhardness measurements and optical microscopy. It was concluded that surface hardness as well as depth hardness of the samples increased with the applied voltage, test duration, and electrolyte concentration.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Magnesium Alloys: Properties and Applications · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. A. Heuer and S. Collins: Metall. Mater. Trans. A, 2009, vol. 40A, p. 1767.10.1007/s11661-009-9904-3 ↗
2. A.J. Perry and J.N. Matossian: Metall. Mater. Trans. A, 1998, vol. 29A, pp. 593–610.10.1007/s11661-998-0141-y ↗
3. S. Kou, D.K. Sun, and Y.P. Le: Metall. Mater. Trans. A, 1983, vol. 14A, pp. 643–53.10.1007/BF02643780 ↗
4. S.F. Luk, T.P. Leung, W.S. Miu, and I. Pashby: J. Mater. Proc. Technol., 1999, vol. 91, pp. 245–49.10.1016/S0924-0136(98)00441-5 ↗
5. P.M. Unterweiser, H.E. Boyer, and J.J. Kubbs: Heat Treater’s Guide: Standard Practices and Procedures for Steel, ASM, Metals Park, OH, 1982.
6. P. Gupta, G. Tenhundfeld, E.O. Daigle, and D. Ryabkov: Surf. Coat. Technol., 2007, vol. 25, pp. 8746–60.10.1016/j.surfcoat.2006.11.023 ↗
7. X. Nie, C. Tsotsos, A. Wilson, A.L. Yerokhin, A. Leyland, and A. Matthews: Surf. Coat. Technol., 2001, vol. 139, pp. 135–42.10.1016/S0257-8972(01)01025-8 ↗
8. T. Paulmier, J.M. Bell, and P.M. Fredericks: Surf. Coat. Technol., 2007, vol. 201, pp. 8771–81.10.1016/j.surfcoat.2006.07.066 ↗
9. A.L. Yerokhin, V.V. Lyubimov, and R.V. Ashitkof: Ceram. Int., 1998, vol. 24, pp. 1–6.10.1016/S0272-8842(96)00067-3 ↗
10. A.D. Pogrebnjak, O.P. Kul’ment’eva, A.P. Kobzev, Y.N. Tyurin, S.I. Golovenko, and A.G. Boiko: Tech. Phys. Lett., 2003, vol. 29, pp. 312–15.10.1134/1.1573301 ↗
11. X. Nie, Q. Hao, and J. Wei: J. Wuhan Univ. Technol., 1996, vol. 11, pp. 28–35.
12. M. Tarakci, K. Korkmaz, Y. Gencer, and M. Usta: Surf. Coat. Technol., 2005, vol. 199, pp. 205–12.10.1016/j.surfcoat.2005.02.117 ↗
13. A.L. Yerokhin, X. Nie, A. Leyland, A. Matthews, and S.J. Dowey: Surf. Coat. Technol., 1999, vol. 122, pp. 73–93.10.1016/S0257-8972(99)00441-7 ↗