Abstract
The aim of this work is to investigate the effect of thermal creep during vacuum drying of spent fuel rods on hydride reorientation and their delayed hydride cracking (DHC) susceptibility. To these ends, we analyzed Tsai’s thermal creep results of irradiated Zircaloy-4 cladding segments from two pressurized water reactors and Simpson and Ells’ observation where zirconium alloy cladding tube failed during long-term storage at room temperature. On cooling under 190 MPa, the spent fuel rods crept to 3.5 pct strain during vacuum drying showed large radial hydrides, while the ones crept to 0.35 pct strain had very fine radial hydrides. Thus, it is suggested that prior creep deformation promotes hydride reorientation in spent fuel rods on cooling after vacuum drying. Evidence for this suggestion is provided by a model experiment. Considering Kim’s DHC model and experimental facts showing precipitation of hydrides even at room temperature at stress raisers, we suggest that spent fuel rods would fail by DHC in dry storage if stress raisers are present inside the cladding on cooling to below 180 °C, and then axial splits of the failed spent fuel rods would occur by DHC due to fuel expansion by UO2 oxidation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Nuclear Materials and Properties · Nuclear reactor physics and engineering · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. M.E. Cunningham, E.P. Simonen, R.T. Allemann, I.S. Levy, and R.F. Hazolton: PNL-6364, Pacific Northwest Laboratory, Richland, 1987.
2. M. Peehs, F. Garzarolli, and W. Goll: IAEA-TECDOC-1089, International Atomic Energy Agency, Vienna, 1999, pp. 313–24.
3. R.E. Einziger, C.L. Brown, G.P. Hornseth, and C.G. Interrante: Radwaste Solutions, 2005, vol. 12, pp. 44–57.
4. H. Tsai and M.C. Billone: J. ASTM Int., 2006, vol. 3, pp. 632–47.10.1520/JAI12425 ↗
5. Y.S. Kim, S.B. Ahn, and Y.M. Cheong: J. Alloys Compd., 2007, vol. 429, pp. 221–26.10.1016/j.jallcom.2006.09.034 ↗
6. IAEA-TECDOC-1293, “Long Term Storage of Spent Nuclear Fuel-Survey and Recommendations,” Final Report of a Co-ordinated Research Project 1994–1997, International Atomic Energy Agency, Vienna, 2002.
7. C.J. Simpson and C.E. Ells: J. Nucl. Mater., 1974, vol. 52, pp. 289–95.10.1016/0022-3115(74)90174-3 ↗
8. Y.B. Yun, Y.S. Kim, K.S. Im, Y.M. Cheong, and S.S. Kim: J. Kor. Nucl. Soc., 2003, vol. 35, pp. 529–36.
9. Y.S. Kim, S.J. Kim, and K.S. Im: J. Nucl. Mater., 2004, vol. 335, pp. 387–96.10.1016/j.jnucmat.2004.07.046 ↗
10. J.F.R. Ambler: Zirconium in the Nuclear Industry, ASTM STP 824, D.G. Frank and R.B. Adamson, eds., ASTM, Philadelphia, PA, 1984, pp. 653–74.
11. A.C. Wallace, G.K. Shek, and O.E. Lepik: Zirconium in the Nuclear Industry; 8th Int. Symp., ASTM STP 1023, L.F.P. Van Swam and C.M. Eucken, eds., ASTM, Philadelphia, PA, 1989, pp. 66–88.10.1520/STP18858S ↗
12. Y.S. Kim, S.B. Ahn, K.S. Kim, and Y.M. Cheong: Key Eng. Mater., 2006, vols. 326–328, pp. 919–22.10.4028/www.scientific.net/KEM.326-328.919 ↗
13. R. Choubey and M.P. Puls: Metall. Mater. Trans. A, 1994, vol. 25A, pp. 993–1004.10.1007/BF02652274 ↗
14. Y.S. Kim: Mater. Sci. Eng., 2007, vols. 468–70, pp. 281–87.10.1016/j.msea.2006.09.123 ↗
15. Z.L. Pan, I.G. Ritchie, and M.P. Puls: J. Nucl. Mater., 1996, vol. 228, pp. 227–37.10.1016/S0022-3115(95)00217-0 ↗
16. H.K. Birnbaum, M.L. Grossbeck, and M. Amano: J. Less-Common Met., 1977, vol. 49, pp. 357–70.10.1016/0022-5088(76)90048-5 ↗
17. S.Q. Shi, G.K. Shek, and M.P. Puls: J. Nucl. Mater., 1995, vol. 218, pp. 189–201.10.1016/0022-3115(94)00405-6 ↗
18. Y.S. Kim: J. Press. Vessel Technol., 2009, vol. 131, p. 011401.
19. M. Aomi, T. Baba, T. Miysashita, K. Kammimura, T. Yoshida, Y. Shinohara, and T. Takeda: J. ASTM Int., 2008, vol. 5, JAI 101262.10.1520/JAI101262 ↗
20. Y.S. Kim: Metall. Mater. Int., 2005, vol. 11, pp. 29–38.10.1007/BF03027481 ↗
21. Y.S. Kim, K.S. Kim, and Y.M. Cheong: J. Nucl. Sci. Technol., 2006, vol. 43, pp. 1120–27.10.3327/jnst.43.1120 ↗
22. R.L. Eadie and C.E. Coleman: Scripta Metall., 1989, vol. 23, pp. 1865–70.10.1016/0036-9748(89)90473-0 ↗
23. M.P. Puls, L.A. Simpson, and R. Dutton: in Fracture Problems and Solutions in the Energy Industry, L.A. Simpson, ed., Pergamon Press, Oxford, United Kingdom, 1982, pp. 13–25.
24. M.P. Puls: Metall. Trans. A, 1990, vol. 21A, pp. 2905–17.10.1007/BF02647211 ↗
25. Y.S. Kim: J. Nucl. Mater., 2008, vol. 378, pp. 30–34.10.1016/j.jnucmat.2008.04.011 ↗
26. C.D. Cann and A. Atrens: J. Nucl. Mater., 1980, vol. 88, pp. 42–50.10.1016/0022-3115(80)90384-0 ↗
27. S. Mishra and M.M. Asundi: Zirconium in Nuclear Applications, ASTM STP 551, ASTM, Philadelphia, PA, 1974, pp. 63–71.10.1520/STP32104S ↗
28. G.J.C. Carpenter and J.F. Watters: J. Nucl. Mater., 1978, vol. 73, pp. 190–97.10.1016/0022-3115(78)90559-7 ↗
29. J.J. Kearns: J. Nucl. Mater., 1967, vol. 22, pp. 292–303.10.1016/0022-3115(67)90047-5 ↗
30. J.H. Root and R.W.L. Fong: J. Nucl. Mater., 1996, vol. 232, pp. 75–85.10.1016/0022-3115(96)00379-0 ↗
31. R.E. Einziger, H. Tsai, M. Billone, and B.A. Hilton: Nucl. Technol., 2003, vol. 144, pp. 186–200.10.13182/NT03-A3439 ↗
32. L.E. Herranz and F. Feria: Prog. Nucl. Energy, 2009, vol. 51, pp. 201–06.10.1016/j.pnucene.2008.09.006 ↗
33. R.E. Einziger and J.A. Cook: Nucl. Technol., 1985, vol. 69, pp. 55–71.10.13182/NT85-A33595 ↗
34. R.E. Einziger and R.V. Strain: Nucl Technol., 1986, vol. 75, pp. 82–95.10.13182/NT86-A15979 ↗
35. J. Nakamura, T. Otomo, T. Kikuchi, and S. Kawasaki: J. Nucl. Sci. Technol., 1995, vol. 32, pp. 321–32.10.3327/jnst.32.321 ↗
36. R.L. Yang: Proc. 2004 International Meeting on LWR Fuel Performance, ANS, Orlando, FL, 2004, pp. 565–75.
37. G. Lysell and V. Grigoriev: Proc. 9th Int. Symp. Environmental Degradation in Nuclear Power Systems–Water Reactors, F.P. Ford and G.S. Was, eds., TMS, Warrendale, PA, 1999, pp. 1169–75.10.1002/9781118787618.ch123 ↗
38. L.A. Simpson and K. Nuttal: Proc. 3rd Int. Symp. on Zirconium in the Nuclear Industry, ASTM STP 633, ASTM, Philadelphia, PA, 1977, pp. 608–29.