Effect of service-simulated aging on the microstructure and properties of casing casting steel (1CrMoV) vis-à-vis remnant life assessment
Source abstract
Abstract
In many cases, it was observed that service-exposed material delivers creep life comparable to unaged material. To understand the mechanism, a 1Cr-1Mo-¼ V casing casting steel has been given service-simulated aging treatment covering up to 150,000 hours. Room-temperature tensile strength, hardness, and fracture appearance transition temperature are evaluated for each time-temperature slot. Stress-rupture tests have been carried out following isostress methodology. Microstructural changes subsequent to aging and after stress rupture tests are evaluated by using scanning electron microscopy (SEM) and transmission electron microscopy (TEM). The results have shown that, though there is a drop in mechanical properties of aged material, stress-rupture property behaved differently. Life steadily declines at intermediate simulation aging conditions up to 100,000 hours, but improves on further aging (≡ 150,000 hours). Thus, extrapolated rupture life at 530 °C (service temperature) produced a “C” shape plot in aging time vs rupture life. Metallographic observation revealed that, at intermediate aging condition, metastability and transitional behavior of alloy carbides are responsible for the drop in rupture life. On the contrary, improvement in rupture strength at the extreme aged condition (≡ 150,000 hours) is attributed to the stable carbides, viz. MC, M23C6, in-situ formation of (V, Mo)C (“H” type), and secondary precipitation of MC and M2C, in a ferrite matrix possessing relatively low density dislocation network.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · High Temperature Alloys and Creep · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (56)
Show source-provided references
1. M.F. Ashby and B.F. Dyson: Proc. “Advances in Fracture Research” ICF6, S.R. Valluri et al., eds., 1984, vol. 1, p. 3.
2. R.M. Goldhoff and H.J. Beattie, Jr.: Trans. TMS-AIME, 1965, vol. 233, p. 1743.
3. M.C. Murphy and G.D. Branch: JISI, 1969, Oct., p. 1347.
4. R.L. Kluch: Mater. Sci. Eng., 1978, vol. 35, p. 239.10.1016/0025-5416(78)90126-X ↗
5. J.R. Yang, C.Y. Huang, C.N. Yang, and J.L. Horng: Mater. Characterization, 1993, vol. 30, p. 75.10.1016/1044-5803(93)90011-J ↗
6. J.J. Bodjin, J.W. Freeman, and I.A. Rohrig: Trans. ASME, 1966, vol. 14, p. 14.
7. T.M. Cullen, I.A. Rohrig, and J.W. Freeman: J. Basic Eng., 1966, Sept., p. 669.
8. L.H. Tofts and R.A. Marsden: Proc. Conf. on the Structural Processes in Creep, Iron and Steel Institute, Institute of Metals, London, 1963, p. 276.
9. G. Crevecoeur: private communication, Association Vincotte, Brussels, Belgium, 1985, p. 45.
10. A. Fugi, M. Kitagawa, H. Umaki, and H. Inai: Mater. Sci. Eng., A, 1991, vol. 143, p. 231.10.1016/0921-5093(91)90742-6 ↗
11. M. Nakashiro, S. Kihara, F. Kishimoto, and T. Fujimori: Iron Steel Inst. Jpn. Int., 1990, vol. 30 (10), p. 823.10.2355/isijinternational.30.823 ↗
12. Y. Sugita, Y. Kato, T. Yokoyama, T. Sada, F. Sasuyama, and N. Nishimura: Iron Steel Inst. Jpn. Int., 1990, vol. 30 (10), p. 895.10.2355/isijinternational.30.895 ↗
13. K. Fujiyama, K. Kimura, M. Muramatsu, and M. Yamada: Iron Steel Inst. Jpn. Int., 1990, vol. 30 (10), p. 869.10.2355/isijinternational.30.869 ↗
14. D. Fang, Z. Gao, and K. Zhang: Int. J. Pressure Vessels Piping, 1999, No. 76, p. 209.10.1016/S0308-0161(98)00141-0 ↗
15. B. Walser: Proc. “Heat and Mass Transfer in Metallurgical System,” D. Spalding and N.H. Afgan, eds., Hemisphere Publishing Corp., Washington, 1981, p. 673.
16. W. Bendick, K. Harmann, and M. Tettke: Proc. LIPREX-89, Corp. R&D, BHEL, Hyderabad, 1989, Sect. 4B.4, p. 1.
17. K.M. Chowdary, S.A. Bashu, K. Singh, and S.C. Bose: Proc. LIPREX—89, Corp. R&D, BHEL, Hyderabad, 1989, Sect, 7B.1, p. 1.
18. J. Ewald and E.E. Muehle: Proc. LIPREX-89, Corp. R&D, BHEL, Hyderabad, 1989 Sect. 1.2, p. 1.
19. K.H. Mayer: Proc. LIPREX-89, Corp. R&D, BHEL, Hyderabad, 1989, Sect. 4A.4, p. 1.
20. A. Joarder, D.S. Sarma, and N.S. Cheruvu: Metall. Trans. A, 1991, vol. 22A, pp. 1811–20.10.1007/BF02646505 ↗
21. R.V. Hart: Met. Technol., 1976, Jan., p. 1.
22. R. Viswanathan and J. Foulds: J. Pressure Vessel Technol., 1998, vol. 120, p. 105.10.1115/1.2842227 ↗
23. B.J. Cane: Proc. Symp. “Creep Resistant Steels for Power Plants”, Corp. R&D, BHEL, 1983, p. 15.
24. S.C. Bose and K. Singh: Technical Report. No. RD/MTL/SCB/03/95, Corp. R&D, BHEL, Hyderabad, 1995.
25. D.R.G. Mitchell and C.J. Moss: J. Mater. Eng. Performance, 1998, vol. 7 (5), p. 621.10.1361/105994998770347477 ↗
26. J. Maguire and D.J. Gooch: Proc. Int. Conf. Life Assessment and Extension, Institute Voor Lastechniek, The Hague, Netherlands, June 1988, p. 116.
27. N.S. Cheruvu: Metall. Trans. A, 1989, vol. 20A, pp. 87–97.10.1007/BF02647496 ↗
28. A. Iseda, Y. Sawaragi, and K. Yoshi Kawa: Iron Steel Inst. Jpn. Int., 1990, vol. 30 (10), p. 862.10.2355/isijinternational.30.862 ↗
29. D.J. Gooch, A. Strang, and S.M. Beech: Proc. Int. Conf. on Remaining Life Assessment, Swansea, Wilshire and Evans, 1993, p. 743.
30. K. Kimura: Parsons—2000, “Advance Materials for 21st Century Turbines and Power Plants,” Proc. 5th Int. Charles Parsons Turbine Conf., Cambridge, United Kingdom, July 3–7, 2000, A. Strang, W.M. Banks, R.D. Conroy, G. MacColvin, J.C. Neal, and S. Simpson, eds., IOM Communication Ltd., London, U.K., p. 590.
31. T. Iwadate, J. Watanabe, and Y. Tanaka: J. Pressure Vessel Technol. Trans. ASME, 1985, vol. 107, p. 230.10.1115/1.3264441 ↗
32. W. Bendick and H. Weber: VGB, KWU-69, Sept. 1989, No. 9, p. 817.
33. T. Wada and V.A. Biss: Metall. Trans. A, 1983, vol. 14A, pp. 845–55.10.1007/BF02644287 ↗
34. W. Zhong-Guang, K. Rakha, P. Nenonen, and C. Laird: Acta Metall., 1985, vol. 33 (12), p. 2129.10.1016/0001-6160(85)90174-9 ↗
35. K.R. Williams: private communication, CERL, Surrey, U.K., 1982, p. 363.
36. B. Walser and A. Rosselet: VGB, KWU-58, May 1978, No. 5, p. 338.10.1215/00182168-58.2.338 ↗
37. K.R. Williams and B. Wilshre: Mater. Sci. Eng., 1981, vol. 47, p. 151.10.1016/0025-5416(81)90221-4 ↗
38. B.J. Cane and K.R. Williams: CEGB Report No. RD/L/R-1965, London, U.K., 1977.
39. B.A. Serior: Mater. Sci. Eng. A, 1988, vol. 103, p. 263.10.1016/0025-5416(88)90516-2 ↗
40. R.B. Carruthers and M.J. Collins: Met. Sci., 1983, vol. 17, p. 107.10.1179/030634583790421050 ↗
41. N. Gope, T. Mukherjee, and D.S. Sarma: Metall. Trans. A, 1992, vol. 23A, pp. 2193–204.10.1007/BF02646012 ↗
42. J.H. Woodhead and A.G. Quarrel: J. Iron Steel Inst., 1965, June, p. 605.
43. K.R. Williams and B.J. Cane: Mater. Sci. Eng., 1979, vol. 38, p. 199.10.1016/0025-5416(79)90124-1 ↗
44. J.M. Silcock: Met. Sci., 1983, vol. 17, p. 101.10.1016/0036-9748(83)90079-0 ↗
45. R. Singh and S. Banarjee: Mater. Sci. Eng. A, 1991, vol. 132, p. 203.10.1016/0921-5093(91)90376-X ↗
46. K.R. Williams: Proc. Int. Conf. on Creep and Fracture of Engineering Materials and Structures, B. Witshire and D.J. Owen, eds., Pine Ridge Press, Swansea, 1981, p. 489.
47. D.A. Miller, W.J. Plumbridge, and R.A. Bartlett: Met. Sci., 1981, vol. 15, p. 413.10.1016/0036-9748(81)90221-0 ↗
48. Y. Kadoya and T. Goto: Iron Steel Inst. Jpn. Int., 1990, vol. 30 (10), p. 829.10.2355/isijinternational.30.829 ↗
49. K. Tokuno, R. Uemori, and K. Itoh: Scripta Metall., 1991, vol. 25 (4), p. 871.10.1016/0956-716X(91)90240-2 ↗
50. D.A. Woodford and R.M. Goldhoff: Mater. Sci. Eng., 1969, vol. 5, p. 303.10.1016/0025-5416(70)90023-6 ↗
51. B.J. Cane and C.J. Middleton: Met. Sci., 1981, vol. 15, p. 295.10.1179/030634581790426831 ↗
52. “Residual Life Assessment Method,” Report, M. Brear and P. McCarthy, eds., Electrical Research Association, Swansea, United Kingdom, Feb. 1990.
53. C.J. Bolton, B.F. Dyson, and K.R. Williams: Mater. Sci. Eng., 1980, vol. 46, p. 572.10.1016/0025-5416(80)90178-0 ↗
54. K. Kimura, H. Kushima, F. Abe, K. Yagi, and H. Irie: Proc. 4th Int. Charles Parsons, Turbine Conf., New Castle upon Tyne, United Kingdom, Nov. 4–6, 1997, A. Starng et al., eds., IOM, London, U.K., p. 257.
55. A. Strang and V. Vodarek: in Microstructure of High Temperature Materials—I, A. Strang, ed., 1997, p. 31.
56. A.K. Ray, Y.N. Tiwari, R.K. Sinha, S. Choudhuri, and R. Singh: Eng. Failure Analysis, Pergamon, Oxford, U.K., 2000, vol. 7, p. 359.