Oxide dispersion strengthening of nickel electrodeposits for microsystem applications
Source abstract
Abstract
Oxide dispersion strengthened nickel (ODS-Ni) electrodeposits were fabricated to net shape using the lithography, electroforming, and molding (LIGA) process in a nickel sulfamate bath containing a suspension of 10 nm diameter Al2O3 particulates. Mechanical properties were compared to baseline specimens fabricated using an identical sulfamate bath chemistry without the particulates. Results revealed that the as-deposited ODS-Ni exhibited significantly higher yield strength and ultimate tensile strength (∼50 pct) than the baseline material. This increase in as-deposited strength was attributed to Orowan strengthening. The ODS-Ni also showed improved retention of room-temperature strength after annealing over a range of temperatures up to 600 °C. Nanoindentation measurements revealed that the properties of the dispersion-strengthened deposit were uniform through its thickness, even in narrow, high aspect ratio structures. Microscopy revealed that this resistance to anneal softening was due to an inhibition of grain growth in the presence of the oxide dispersion. At elevated temperatures, the strength of the ODS-Ni was approximately 3 times greater than that of the baseline material although with a significant reduction in hot ductility.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electrodeposition and Electroless Coatings · Metal and Thin Film Mechanics · Anodic Oxide Films and Nanostructures
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. E. Becker, W. Ehrfeld, D. Munchmeyer, H. Betz, A. Hueberger, S. Pontgratz, W. Gashauser, H.J. Michel, and R. von Siemens: Naturwissenschaften, 1982, vol. 69 (11), p. 520.10.1007/BF00463495 ↗
2. N. Rajan, C.A. Zorman, S. Stefanescu, and T.P. Kicher: J. Microelectromech. Systems, 1991, vol. 8 (3), p. 251.10.1109/84.788628 ↗
3. W.C. Wenzel and G. Gerlach: Sensors Actuators, 1999, vol. 77, p. 14.10.1016/S0924-4247(98)00377-X ↗
4. L. Fan, H. Last, R. Wood, B. Dudley, C. Khan Malek, and Z. Ling: Microsystem Technol., 1998, vol. 4, p. 168.10.1007/s005420050123 ↗
5. L.T. Romankiw: Electrochimica Acta, 1997, vol. 42, p. 2985.10.1016/S0013-4686(97)00146-1 ↗
6. S.M. Spearing: Acta Mater., 2000, vol. 48, p. 179.10.1016/S1359-6454(99)00294-3 ↗
7. W.H. Safrenak: The Properties of Electrodeposited Metals and Alloys, 2nd ed., American Electroplaters and Surface Finishers Soc., Orlando, FL, 1986, pp. 253–374.
8. W.R. Wearmouth and K.C. Belt: Plating Surf. Finishing, 1979, vol. 66 (10), p. 53.
9. J.W. Dini, H.R. Johnson, and L.A. West: Plating Surf. Finishing, 1978, vol. 65 (2), p. 36.
10. J.J. Kelly, S.H. Goods, and N.Y.C. Yang: Chem. Solid State Lett., 2003, vol. 6 (6), pp. C88-C91.10.1149/1.1567532 ↗
11. W.B. Stephenson, Jr.: Plating, 1966, vol. 53, p. 183.
12. E. Orowan: Dislocations in Metals, AEVIE, Warrendale, PA, 1954, p. 69.
13. G.E. Deiter: Mechanical Metallurgy, McGraw-Hill, New York, NY, 1961, p. 144.
14. V.P. Greco: Plating Surf. Finishing, 1989, vol. 76, p. 68.
15. C.A. Addison and E.C. Kedward: Trans. Inst. Met. Finishing, 1977, vol. 55, p. 1.10.1080/00202967.1977.11870402 ↗
16. M. Thoma: Plating Surf. Finishing, 1984, vol. 71, p. 51.
17. F.K. Sautter: J. Electrochem. Soc., 1963, vol. 110, p. 557.10.1149/1.2425813 ↗
18. X.M. Ding, N. Merk, and B. Ilschner: J. Mater. Sci., 1998, vol. 33, p. 803.10.1023/A:1004370602721 ↗
19. X.M. Ding, N. Merk, and B. Ilschner: J. Chi. Soc. Mech. Eng., 1997, vol. 18, p. 145.
20. J. Foster and B. Cameron: Trans. Inst. Metal Finishing, 1976, vol. 54, p. 178.10.1080/00202967.1976.11870395 ↗
21. C. White and J. Foster: Trans. Inst. Metal Finishing, 1981, vol. 59, p. 8.10.1080/00202967.1981.11870553 ↗
22. D.T. Schmale, RJ. Bourcier, and T.E. Buchheit: Report No. SAIND97-1608, Sandia National Laboratories, Albuquerque, NM, 1997.
23. T.E. Buchheit, D.A. LaVan, J.R. Michael, T.R. Christenson, and S.E. Leith: Metall. Mater. Trans. A, 2002, vol. 33A, p. 539.10.1007/s11661-002-0116-3 ↗
24. J.I. Goldstein: Scanning Electron Microscopy and X-ray Microanalysis, Kluwer Academic/Plenum Publishing, New York, NY, 2003, p. 558.10.1007/978-1-4615-0215-9 ↗
25. M.W. Phaneuf: Micron, 1999, vol. 30, p. 221.10.1016/S0968-4328(98)00044-4 ↗
26. S.H. Goods, J.J. Kelly, and N.Y.C. Yang: Microsystem Tech., 2004, in press.
27. P.G. Kotula, M.R. Keenan, and J.R. Michael: Microsc. Microanal., 2003, vol. 9, p. 1.10.1017/S1431927603030058 ↗
28. J.C. Russ: Practical Stereology, Plenum Press, New York, NY, 1986, pp. 35–55.10.1007/978-1-4899-3533-5_3 ↗
29. Technical Product Specification, Nickel 200,201 and DURANICKEL Alloy 301, #4M 8-88 IAI-47, Inco Alloys International, Inc., Huntington, WV, 1988.
30. S.H. Goods and L.M. Brown: Acta Metall., 1979, vol. 27, p. 1.10.1016/0001-6160(79)90051-8 ↗
31. S.H. Goods and W.D. Nix: Acta Metall., 1978, vol. 26, p. 739.10.1016/0001-6160(78)90024-X ↗
32. Flow and Fracture at Elevated Temperatures, R. Raj, ed., ASM, Metals Park, OH, 1985.
33. H. Reidel: Fracture at High Temperatures, Springer-Verlag, New York, NY, 1986.