Stress Corrosion and Corrosion Fatigue Crack Growth of Zr-Based Bulk Metallic Glass in Aqueous Solutions
Source abstract
Abstract
Crack-propagation tests on a bulk metallic glass (BMG), Zr55Cu30Ni5Al10, were conducted either in aqueous sodium chloride (NaCl) solutions or in high-purity water under sinusoidal cyclic loading or sustained loading. Although the crack growth rate in high-purity water was almost identical to that in air, the rate in the NaCl solution was much higher than that in air, even in a very low concentration of NaCl such as 0.01 mass pct. In a 3.5 mass pct NaCl solution, the time-based crack growth rate during cyclic loading, da/dt, was determined by the maximum stress-intensity factor, K max, but was almost independent of the loading frequency and the stress ratio, and the rate was close to that of stress corrosion cracking (SCC) under a sustained loading.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications · Phase-change materials and chalcogenides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. W.L. Johnson: Curr. Opin. Solid State Mater. Sci., 1996, vol. 1, pp. 383–86.10.1016/S1359-0286(96)80029-5 ↗
2. H.J. Leamy, H.S. Chen, and T.T. Wang: Metall. Trans., 1972, vol. 3, pp. 699–708.10.1007/BF02642754 ↗
3. V. Schroeder, C.J. Gilbert, and R.O. Ritchie: Scripta Mater., 1998, vol. 38, pp. 1481–85.10.1016/S1359-6462(98)00089-X ↗
4. W.H. Peter, R.A. Buchanan, C.T. Liu, P.K. Liaw, M.L. Morrison, J.A. Horton, C.A. Carmichael, Jr., and J.L. Wright: Intermetallics, 2002, vol. 10, pp. 1157–62.10.1016/S0966-9795(02)00130-9 ↗
5. M. Ishida, H. Takeda, N. Nishiyama, K. Amiya, K. Kita, Y. Shimizu, D. Watanabe, E. Fukushima, Y. Saotome, and A. Inoue: Materia Jpn., 2005, vol. 44, pp. 431–33.10.2320/materia.44.431 ↗
6. Y. Nakai and S. Hosomi: Mater. Trans., 2007, vol. 48, pp. 1770–73.10.2320/matertrans.MJ200758 ↗
7. Y. Nakai, N. Sei, and B.K. Kim: Key Eng. Mater., 2007, vols. 345–346, pp. 259–62.10.4028/www.scientific.net/KEM.345-346.259 ↗
8. Y. Nakai, K. Sakai, and K. Nakagawa: Adv. Eng. Mater., 2008, vol. 10, pp. 1026–29.10.1002/adem.200800141 ↗
9. Y. Nakai and M. Seki: J. Soc. Mater. Sci., Jpn., 2007, vol. 56, pp. 229–35.10.2472/jsms.56.229 ↗
10. Y. Nakai and M. Seki: Key Eng. Mater., 2008, vols. 378–379, pp. 317–28.10.4028/www.scientific.net/KEM.378-379.317 ↗
11. V. Schroeder, C.J. Gilbert, and R.O. Ritchie: Scripta Mater., 1999, vol. 40, pp. 1057–61.10.1016/S1359-6462(99)00067-6 ↗
12. R.O. Ritchie, V. Schroeder, and C.J. Gilbert: Intermetallics, 2000, vol. 8, pp. 469–75.10.1016/S0966-9795(99)00155-7 ↗
13. V. Schroeder and R.O. Ritchie: Acta Mater., 2006, vol. 54, pp. 1785–94.10.1016/j.actamat.2005.12.006 ↗
14. A. Kawashima, H. Kurishita, H. Kimura, and A. Inoue: Mater. Trans., 2007, vol. 48, pp. 1969–72.10.2320/matertrans.MRP2007085 ↗
15. R.W. Hertzberg: Deformation and Fracture Mechanics of Engineering Materials, 2nd ed., John Wiley & Sons, New York, NY, 1983, p. 439.
16. Y. Nakai, A. Alavi, and R.P. Wei: Metall. Trans. A, 1988, vol. 19A, pp. 543–48.10.1007/BF02649268 ↗
17. R.P. Wei: Fatigue Mechanisms, ASTM STP 675, J.T. Fong, ed., ASTM, West Conshohocken, PA, 1979, pp. 816–40.
18. V. Schroeder, C.J. Gilbert, and R.O. Ritchie: Mater. Sci. Eng., A, 2001, vol. 317, pp. 145–52.10.1016/S0921-5093(01)01157-1 ↗
19. M.L. Morrison, R.A. Buchanan, P.K. Liaw, B.A. Green, G.Y. Wang, C.T. Liu, and J.A. Horton: Mater. Sci. Eng., A, 2007, vol. 467, pp. 198–206.10.1016/j.msea.2007.03.106 ↗
20. D. Suh and R.H. Dauskardt: Scripta Mater., 2000, vol. 42, pp. 233–40.10.1016/S1359-6462(99)00337-1 ↗