Abstract
Evaluations of the (infrared)-brazed Ti-6Al-4V and niobium joints using three silver-base braze alloys have been extensively studied. According to the dynamic wetting angle measurement results, the niobium substrate cannot be effectively wetted by all three braze alloys. Because the dissolution of Ti-6Al-4V substrate causes transport of Ti into the molten braze, the molten braze dissolved with Ti can effectively wet the niobium substrate during brazing. For infrared-brazed Ti-6Al-4V/Ag/Nb joint, it is mainly comprised of the Ag-rich matrix. The TiAg reaction layer is observed at the interface between the braze and Ti-6Al-4V substrate. In contrast, Ti-rich, Ag-rich, and interfacial TiAg phases are found in the furnace-brazed specimen. The dominated Ti-rich phase in the joint is caused by enhanced dissolution between the molten braze and Ti-6Al-4V substrate. The infrared-brazed Ti-6Al-4V/72Ag-28Cu/Nb joint is mainly comprised of the Ag-rich matrix and Ag-Cu eutectic. With increasing the brazing temperature or time, the amount of Ag-Cu eutectic is decreased, and the interfacial Cu-Ti reaction layer(s) is increased. The infrared brazed joint has the highest average shear strength of 224.1 MPa. The averaged shear strength of the brazed joint is decreased with increasing brazing temperature or time, and its fracture location changes from the braze alloy into the interfacial reaction layer(s) due to excessive growth of the Cu-Ti intermetallics. The infrared-brazed Ti-6Al-4V/95Ag-5Al/Nb joint is composed of Ag-rich matrix and TiAl interfacial reaction layer. With increasing the brazing time, the amount of Ag-rich phase is greatly decreased, and the interfacial reaction layer becomes Ti3Al due to enhanced dissolution of Ti-6Al-4V substrate into the molten braze. The average shear strength of the infrared-brazed joint is 172.8 MPa. Additionally, the existence of an interfacial Ti3Al reaction layer significantly deteriorates the shear strength of the furnace-brazed specimen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Titanium Alloys Microstructure and Properties · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. R. Roger, E.W. Collings, and G. Welsch: Materials Properties Handbook: Titanium Alloys, ASM INTERNATIONAL, Materials Park, OH, 1993.
2. Metals Handbook vol. 2, Properties and Selection: Nonferrous Alloys and Special Purpose Materials, J.R. Davis, ed., AMS INTERNATIONAL, Materials Park, OH, 1990.
3. ASM Handbook, vol. 6, Welding, Brazing and Soldering, D.L. Olson, I.A. Siewert, S. Liu, and G.R. Edwards, eds., ASM INTERNATIONAL, Materials Park, OH, 1993.
4. W.F. Smith: Structure and Properties of Engineering Alloys, McGarw-Hill Inc., New York, NY, 1993.
5. M. Schwartz: Brazing: for the Engineering Technologist, ASM INTERNATIONAL, Materials Park, OH, 1995.
6. M. Schwartz: Brazing, ASM INTERNATIONAL, Metals Park, OH, 1987.
7. G. Humpston and D.M. Jacobson: Principles of Soldering and Brazing, ASM INTERNATIONAL, Materials Park, OH, 1993.
8. N.A. Dececco and J.N. Parks: Welding J., 1953, vol. 32 (11), pp. 1071–81.
9. C.C. Liu, C.L. Ou and R.K. Shiue: J. Mater. Sci., 2002, vol. 37 (11), pp. 2225–35.10.1023/A:1015356930476 ↗
10. T. Takemoto and I. Okamoto: J. Mater. Sci., 1988, vol. 23 (4), pp. 1301–08.10.1007/BF01154593 ↗
11. D.G. Howden and R.W. Monroe: Welding J., 1972, vol. 51 (1), pp. 31–36.
12. R.K. Shiue, S.K. Wu, and S.Y. Chen: Acta Mater., 2003, vol. 51 (7), pp. 1991–2004.10.1016/S1359-6454(02)00606-7 ↗
13. S.W. Lan: Welding J., 1982, vol. 61 (10), pp. 23–28.
14. O. Botstein and A. Rabinkin: Mater. Sci. Eng. A, 1994, vol. A188, pp. 305–15.10.1016/0921-5093(94)90386-7 ↗
15. O. Botstein, A. Schwarzman, and A. Rabinkin, Mater. Sci. Eng. A, 1996, vol. A206, pp. 14–23.10.1016/0921-5093(95)09885-2 ↗
16. H.Y. Chan and R.K. Shiue: J. Mater. Sci. Lett., 2003, vol. 22 (23), pp. 1659–63.10.1023/B:JMSL.0000004642.79837.d1 ↗
17. H.Y. Chan, D.W. Liaw, and R.K. Shiue: Int. J. Refract. Met. Hard Mater., 2004, vol. 22, pp. 27–33.10.1016/j.ijrmhm.2003.11.002 ↗
18. H.Y. Chan, D.W. Liaw, and R.K. Shiue: Mater. Lett., 2004, vol. 58, pp. 1141–46.10.1016/j.matlet.2003.09.007 ↗
19. R.K. Shiue, S.K. Wu, J.M.O. Wang and J.Y. Wang: Metall. Mater. Trans. A, 2000, vol. 31A, pp. 2527–36.10.1007/s11661-000-0197-9 ↗
20. Y.L. Lee, R.K. Shiue, and S.K. Wu: Intermetallics, 2003, vol. 11 (3), pp. 187–95.10.1016/S0966-9795(02)00252-2 ↗
21. R.K. Shiue, S.K. Wu, and C.M. Huang: Metall. Mater. Trans. A, 2002, vol. 33A, pp. 1765–73.10.1007/s11661-002-0185-3 ↗
22. R.K. Shine, S.K. Wu, and C.H. Chan: J. Alloy Compounds, 2004, vol. 372, pp. 148–57.10.1016/j.jallcom.2003.09.155 ↗
23. C.C. Lin, R.B. Chen, and R.K. Shine: J. Mater. Sci., 2001, vol. 36 (9), pp. 2145–50.10.1023/A:1017531730604 ↗
24. T.B. Massalski: Binary Alloy Phase Diagrams, ASM INTERNATIONAL, Materials Park, OH, 1990.
25. P. Villars, A. Prince, and H. Okamoto: Handbook of Ternary Alloy Phase Diagrams, ASM INTERNATIONAL, Materials Park, OH, 1995.