journal article·2000-06

Solidification characteristics of the Al-8.3Fe-0.8V-0.9Si alloy

K. L. Sahoo, C. S. Sivaramakrishnan, A. K. Chakrabarti

Publisher page

Abstract

Studies of solidification behavior have been conducted on cast Al-Fe-V-Si alloys. The first phase to precipitate during solidification of an Al-8.3Fe-0.8V-0.9Si alloy is Al3Fe(V,Si), which is isostructural with the Al3Fe phase. Thereafter, the solidification proceeds through several invariant reactions. The final invariant reaction is associated with a pronounced arrest. The temperature of this arrest is a function of the cooling rate and modification treatment, with magnesium added as an Al-20 pct Mg or Ni-20 pct Mg master alloy. The coarse iron aluminide precipitates in a slow-cooled (>1 °C/s) cast structure transform to a ten-armed, star-like morphology upon chill casting the melt (cooling rate >10 °C/s) from 900 °C or upon water quenching from above 800 °C. Treatment with magnesium refines the morphology, size, and distribution of iron aluminide precipitates in slow-cooled alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Solidification and crystal growth phenomena · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. M.N. Srinivasan and S.D. Little: Scripta Metall. Mater., 1995, vol. 32 (8), pp. 1153–58.10.1016/0956-716X(95)00117-E ↗
2. H. Fredriksson, M. Hillert, and N. Lange: J. Inst. Met., 1973, vol. 101, pp. 285–99.
3. D. Apelian, G.K. Sigworth, and K.R. Whalar: AFS Trans., 1984, vol. 92, pp. 297–307.
4. J.E. Gruzleski: AFS Trans., 1992, vol. 100, pp. 285–93.
5. S.G. Shabestari and J.E. Gruzleski: AFS Trans., 1995, vol. 103, pp. 285–93.
6. E.J. Kubel, Jr.: Adv. Mater. Processes, 1986, vol. 12, pp. 43–49.
7. E.J. Lavernia, J.D. Ayers, and T.S. Srivatsan: Int. Mater. Rev., 1992, vol. 37, pp. 1–44.10.1179/imr.1992.37.1.1 ↗
8. B.L. Tuttle: Mod. Casting, 1985, Nov., p. 39.
9. D.J. Skinner: in Dispersion Strengthen Al Alloys, Y.W. Kim and W.M. Griffith, eds., TMS, Warrendale, PA, 1988, pp. 181–97.
10. L. Ananthanarayan, F.H. Samuel, and J.E. Gruzleski: AFS Trans., 1992, vol. 100, pp. 383–91.
11. L. Ananthanarayanan, F.H. Samuel, and J.E. Gruzleski: Metall. Mater. Trans. A, 1994, vol. 25A, pp. 1761–73.
12. S. Gowri and F.H. Samuel: Metall. Mater. Trans. A, 1994, vol. 25A, pp. 437–48.10.1007/BF02647989 ↗
13. T. Turmezey, V. Stefariay, and A. Griger: Key Engineering Materials, Trans Tech Publications, Aedermannsdorf, Switzerland, 1989, vols. 38–39, pp. 43–64.
14. J.D. Cotton and M.J. Kaufman: Metall. Trans. A, 1991, vol. 22A, pp. 927–34.10.1007/BF02659002 ↗
15. K. Sampath and W.A. Baeslack: Weld. J., 1993, vol. 72 (8), pp. 416s-427s.
16. R.M.K. Young and T.W. Clayne: Scripta Metall., 1981, vol. 15, pp. 1211–16.10.1016/0036-9748(81)90301-X ↗
17. P.M. Skjerpe: Technical Report No. 820160-4, Sentralinstituff for Industriell Forskning, 1982.
18. Ping Liu, T. Thorvaldsson, and G.L. Dunlop: Met. Sci. Eng., 1986, vol. 2, pp. 1009–18.
19. V.G. Rivlin and G.V. Raynor: Int. Mater. Rev., 1981, No. 3, pp. 133–52.10.1179/imtr.1981.26.1.133 ↗
20. H.W.L. Philips and P.C. Varley: J. Inst. Met., 1943, vol. 69, pp. 317–50.
21. D. Munson: Inst. Met., 1967, vol. 97, pp. 217–19.