Effects of Aluminization Via Thermo-Chemical Diffusion on the Wear Behavior of Structural Materials for High-Temperature Gas-Cooled Reactors
Source abstract
Abstract
We explore the effects of thermo-chemical aluminization on wear resistance of candidate alloys Incoloy 800HT and Inconel 617 for high-temperature gas-cooled reactor (HTGR) components. Aluminized samples were conditioned for 22 days in a once-through helium loop to simulate oxidizing conditions of HTGRs. The tribological performance of unconditioned and conditioned samples was tested using pin-on-disk tribometer in an air environment at 750 °C for 800HT and 900 °C for 617. Aluminized 800HT exhibited superior wear resistance compared to that of the as-received 800HT due to harder Fe-Al intermetallic compounds that formed at the surface of the alloy. Aluminized 617 exhibited wear resistance superior to that of the as-received 617 at higher loads but inferior resistance at lower loads. Conditioned 800HT as well as aluminized and then conditioned 800HT exhibited negligible wear when the protective oxide remained intact during tribotesting. When the oxide wore through, aluminized and then conditioned 800HT exhibited superior wear resistance compared to that of conditioned 800HT due to the increased hardness of intermetallic zones. Aluminized and then conditioned 617 exhibited inferior wear resistance compared to that of conditioned 617 due to significant ceramic wear of the aluminum oxide. Connections between surface hardness, chemical composition, initial friction coefficients, and wear resistance are established.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced materials and composites · Metal Alloys Wear and Properties · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Cliff Davis: Implementation of Molten Salt Properties into RELAP5-3D/ATHENA, 2005.10.2172/910991 ↗
2. Richard N. Wright: Kinetics of Gas Reactions and Environmental Degradation in NGNP Helium, 2006.10.2172/911710 ↗
3. 3 W.J. Quadakkers and H. Schuster: Nuclear Technology, 1984, vol. 66, pp. 383–91.10.13182/NT84-A33441 ↗
4. 4 C. Cabet, A. Terlain, P. Lett, L. Guétaz, and J.-M. Gentzbittel: Materials and Corrosion, 2006, vol. 57, pp. 147–53.10.1002/maco.200503901 ↗
5. 5 C. Jang, D. Lee, and D. Kim: International Journal of Pressure Vessels and Piping, 2008, vol. 85, pp. 368–77.10.1016/j.ijpvp.2007.11.010 ↗
6. 6 W.J. Quadakkers: Materials and Corrosion, 1985, vol. 36, pp. 335–47.10.1002/maco.19850360802 ↗
7. K. Natesan, A. Purohit, and S.W. Tam: Materials Behavior in HTGR Environments, 2003.
8. 8 M.S. Rahman, J. Ding, A. Beheshti, X. Zhang, and A.A. Polycarpou: Wear, 2019, vol. 436–437, p. 203022.10.1016/j.wear.2019.203022 ↗
9. 9 M.S. Rahman, J. Ding, A. Beheshti, X. Zhang, and A.A. Polycarpou: Tribology International, 2018, vol. 123, pp. 372–84.10.1016/j.triboint.2018.03.021 ↗
10. 10 M. Akbari-Garakani and M. Mehdizadeh: Materials & Design, 2011, vol. 32, pp. 2695–700.10.1016/j.matdes.2011.01.017 ↗
11. 11 A. Korashy, H. Attia, V. Thomson, and S. Oskooei: Tribology International, 2020, vol. 145, p. 106155.10.1016/j.triboint.2019.106155 ↗
12. 12 J. Liu, R. Han, L. Zhang, and H. Guo: Wear, 2007, vol. 262, pp. 442–52.10.1016/j.wear.2006.06.014 ↗
13. 13 M.S. Rahman, K. Polychronopoulou, and A.A. Polycarpou: Wear, 2020, vol. 462–463, p. 203508.10.1016/j.wear.2020.203508 ↗
14. 14 A. Schnaas and H.J. Grabke: Oxid Met, 1978, vol. 12, pp. 387–404.10.1007/BF00612086 ↗
15. 15 Irwin Singer: Applications of Surface Science, 1984, vol. 18, pp. 28–62.10.1016/0378-5963(84)90037-0 ↗
16. V. Pauly, C. Tesch, J. Kern, M. Clark, D. Grierson, D. Singh, O. Ajayi, and K. Sridharan: J. Nucl. Mater., 2019, vol. 522, pp. 311–23. Image reprinted from Journal of Nuclear Materials, Volume 522, V. Pauly et al, High-temperature tribological behavior of structural materials after conditioning in impure-helium environments for high-temperature gas-cooled reactor applications, Page 314, 2019, with permission from Elsevier.10.1016/j.jnucmat.2019.05.025 ↗
17. 17 B.W. Lee: Int. J. Mod. Phys. B, 2018, vol. 32, p. 1840056.10.1142/S0217979218400568 ↗
18. A. Bensely, A. Prabhakaran, D. MohanLal, and G. Nagarajan: Cryogenics, 2005, vol. 45, pp. 747–54.10.1016/j.cryogenics.2005.10.004 ↗
19. 19 C. Chen, D.Y. Li, and C.J. Shang: Electrochimica Acta, 2009, vol. 55, pp. 118–24.10.1016/j.electacta.2009.08.016 ↗
20. 20 F. Haftlang, A. Habibolahzadeh, and M.H. Sohi: Applied Surface Science, 2015, vol. 329, pp. 240–7.10.1016/j.apsusc.2014.12.140 ↗
21. J.P. Lebrun: in Thermochemical Surface Engineering of Steels. Elsevier, Amsterdam; 2015, pp. 633–47.10.1533/9780857096524.4.633 ↗
22. 22 R. Sharghi-Moshtaghin, H. Kahn, Y. Ge, X. Gu, F.J. Martin, P.M. Natishan, R.J. Rayne, G.M. Michal, F. Ernst, and A.H. Heuer: Metall and Mat Trans A, 2010, vol. 41, pp. 2022–32.10.1007/s11661-010-0299-y ↗
23. 23 Q.Y. Zhang, Y. Zhou, J.Q. Liu, K.M. Chen, J.G. Mo, X.H. Cui, and S.Q. Wang: Wear, 2015, vol. 344–345, pp. 22–31.10.1016/j.wear.2015.10.017 ↗
24. 24 E. Hao, Y. An, X. Zhao, H. Zhou, and J. Chen: Applied Surface Science, 2018, vol. 462, pp. 194–206.10.1016/j.apsusc.2018.08.111 ↗
25. 25 D. Kukla, M. Kopec, Z.L. Kowalewski, D.J. Politis, S. Jóźwiak, and C. Senderowski: Materials, 2020, vol. 13, p. 3863.10.3390/ma13173863 ↗
26. 26 A. Günen, K.M. Döleker, M.E. Korkmaz, M.S. Gök, and A. Erdogan: Surface and Coatings Technology, 2021, vol. 409, p. 126906.10.1016/j.surfcoat.2021.126906 ↗
27. 27 J.-K. Chen, S.-F. Chen, and C.-S. Huang: ISIJ Int., 2012, vol. 52, pp. 127–33.10.2355/isijinternational.52.127 ↗
28. 28 Q.Y. Zhang, Y. Zhou, J.Q. Liu, K.M. Chen, J.G. Mo, X.H. Cui, and S.Q. Wang: Metall and Mat Trans A, 2016, vol. 47, pp. 2232–42.10.1007/s11661-016-3414-x ↗
29. 29 R. Prescott and M.J. Graham: Oxid Met, 1992, vol. 38, pp. 233–54.10.1007/BF00666913 ↗
30. 30 R.S. Dutta, S. Majumdar, A. Laik, K. Singh, U.D. Kulkarni, I.G. Sharma, and G.K. Dey: Surface and Coatings Technology, 2011, vol. 205, pp. 4720–5.10.1016/j.surfcoat.2011.04.038 ↗
31. 31 E. Arslan, Y. Totik, E.E. Demirci, Y. Vangolu, A. Alsaran, and I. Efeoglu: Surface and Coatings Technology, 2009, vol. 204, pp. 829–33.10.1016/j.surfcoat.2009.09.057 ↗
32. 32 H.J. Lee, S.H. Kim, H. Kim, and C. Jang: Applied Surface Science, 2016, vol. 388, pp. 483–90.10.1016/j.apsusc.2015.11.162 ↗
33. V. Pauly, J. Kern, M. Clark, D.S. Grierson, and K. Sridharan: Tribol. Int., 2020, p. 106715. Images and table reprinted from Tribology International, Volume 154, V. Pauly et al, Wear Performance of incoloy 800HT and inconel 617 in various surface conditions for high-temperature gas-cooled reactor components, Page 106715 314, 2020, with permission from Elsevier.10.1016/j.triboint.2020.106715 ↗
34. 34 S.W. Green and F.H. Stott: Corrosion Science, 1992, vol. 33, pp. 345–59.10.1016/0010-938X(92)90065-B ↗
35. 35 S. Salari, M.S. Rahman, A.A. Polycarpou, and A. Beheshti: Materials Science and Engineering: A, 2020, vol. 788, p. 139539.10.1016/j.msea.2020.139539 ↗
36. Z. Liang, Y. Gui, and Q. Zhao: Mater. Res. Express, 2020, vol. 7, p. 016548.10.1088/2053-1591/ab6388 ↗
37. 37 M. Archana, Ch.J. Rao, S. Ningshen, and J. Philip: J. of Materi Eng and Perform, 2021, vol. 30, pp. 931–43.10.1007/s11665-020-05367-8 ↗
38. 38 J. Chin, W.R. Johnson, and K. Chen: Thin Solid Films, 1982, vol. 95, pp. 85–97.10.1016/0040-6090(82)90585-5 ↗
39. 39 I. Sah, S.H. Kim, and C. Jang: Met. Mater. Int., 2016, vol. 22, pp. 1033–40.10.1007/s12540-016-6218-z ↗
40. 40 Y. Zhang, D.P. Mohanty, P. Seiler, T. Siegmund, J.J. Kruzic, and V. Tomar: International Journal of Plasticity, 2017, vol. 96, pp. 264–81.10.1016/j.ijplas.2017.05.007 ↗
41. 41 D. Kim, I. Sah, H.J. Lee, S. Hong, and C. Jang: Surface and Coatings Technology, 2014, vol. 244, pp. 15–2210.1016/j.surfcoat.2014.01.009 ↗