Investigation of Hot Workability and Microstructure Evolution of VGCNFs-Reinforced Aluminum Matrix Composites
Source abstract
Abstract
Isothermal compression experiments of vapor-grown carbon nanofiber (VGCNF)-reinforced aluminum matrix (VGCNF/Al) composites and pure aluminum (Al) were conducted at deformation temperatures from 573 K to 723 K and strain rates from 0.01 to 1 s−1. It was found that the VGCNF/Al composites and pure Al had depressed dynamic recrystallization percent in the high-power dissipation efficiency regions. Upon comparing the processing maps for different strains, it was found that the high-power dissipation efficiency regions of the VGCNF/Al composites and pure Al moved from the low strain rate region to the high strain rate region. The kernel average misorientation images showed that there were lots of low-angle grain boundaries in the high strain rate region. The low-angle grain boundaries did not have enough time to transform into high-angle grain boundaries, resulting in a depressed percentage of dynamic recrystallization. The addition of VGCNFs led to an increased low-angle grain boundary density. As a result, the phenomenon of high-power dissipation regions in the high strain rate regions correspond to the low percentage of dynamic recrystallization was more obvious.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Microstructure and mechanical properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. C.S. Zhang, C.X. Wang, R. Guo, G.Q. Zhao, L. Chen: J. Alloys Compd., 2019, vol. 773, pp. 59-70.10.1016/j.jallcom.2018.09.263 ↗
2. Z.Y. Liu, B.L. Xiao, W.G. Wang, Z.Y. Man: Compos Part A: Appl Sci Manufac., 2017, vol. 94, pp. 189-198.10.1016/j.compositesa.2016.11.029 ↗
3. B. Liao, L.F. Cao, X.D. Wu, Y. Zou, G.J. Huang, P. Rometsch, J. Couper, Q. Liu: Mater., 2019, vol. 12, pp. 311-326.10.3390/ma12020311 ↗
4. Z.F. Xu, Y.B. Choi, K. Matsugi, D.C. Li, G. Sasak: Mater. Trans., 2009, vol. 9, pp. 2160-2164.
5. Z.F. Xu, Y.B. Choi, K. Matsugi, D.C. Li, G. Sasak: Mater. Trans., 2010, vol. 3, pp. 510-515.
6. K.C. Chang, Z.F. Xu, K. Matsugi, G. Sasaki: Mater. Trans., 2009, vol. 6, pp. 1510-1518.10.2320/matertrans.MRA2008350 ↗
7. Q.Y. Zhao, F. Yang, R. Torrens, L. Bolzoni: Mater. Des., 2019, vol. 169, pp. 1-16.
8. B.N. Sahoo, S.K. Panigrahi: J. Alloys Compd., 2019, vol. 776, pp. 865-882.10.1016/j.jallcom.2018.10.276 ↗
9. K.K. Wang, X.P. Li, Q.L. Li, G.G. Shu, G.Y. Tang: Mater. Sci. Eng. A, 2017, vol. 696, pp. 248-256.10.1016/j.msea.2017.03.013 ↗
10. Y.E. Tang, X.P. Guo: Metall. Trans. A, 2018, vol. 49, pp. 4884-4994.10.1007/s11661-018-4794-x ↗
11. J.P. Liu, G.L. Fan, Z.Q. Tian, Q. Guo, Y.S. Su, Z.Q. Li, D.B. Xiong: Compos Part A: Appl Sci Manufac., 2019, vol. 116, pp. 54-61.10.1016/j.compositesa.2018.10.022 ↗
12. M.M.H. Athar, R. Mahmudi: Mater. Sci. Eng. A, 2019, vol. 759, pp. 745-753.10.1016/j.msea.2019.05.101 ↗
13. L. Zhang, Q.D. Wang, G.P. Liu, W. Guo, H.Y. Jiang, W.J. Ding: Mater. Sci. Eng. A, 2017, vol. 707, pp. 315-324.10.1016/j.msea.2017.09.056 ↗
14. H.D. Zhang, Y. Liu, F. Zhang, D. Zhang, H.X. Zhu, T.X. Fan: Metall. Trans. A, 2018, vol. 49A, pp. 2202-2212.10.1007/s11661-018-4547-x ↗
15. P.L. Narayana, C.L. Li, J.K. Hong, S.W. Choi, C.H. Park, S.W. Kim, S.E. Kim, N.S. Reddy, J.T. Yeom: Met. Mater. Int., 2019, vol. 25, pp. 1063-1071.10.1007/s12540-018-00237-4 ↗
16. G.W. Bo, F.L. Jiang, Z.Y. Dong, G. Wang, H. Zhang: Mater. Sci. Eng. A, 2019, vol. 755, pp. 147-157.10.1016/j.msea.2019.04.009 ↗
17. G. Wang, D.W. Bian, L.Y. Kou, X.J. Zhu: Mater. Res. Express, 2019, vol. 6, 096527.10.1088/2053-1591/ab2d07 ↗
18. M. Bambach, A. Emdadi, I. Sizova, U. Hecht, F. Pyczak: Intermetallics, 2018, vol. 101, pp. 44-55.10.1016/j.intermet.2018.07.004 ↗
19. J.W. Lee, H.W. Son, S.K. Hyun: J. Alloys Compd., 2019, vol. 774, pp. 1081-1091.10.1016/j.jallcom.2018.09.255 ↗
20. Y.H. Duan, P. Li, L.S. Ma, R.Y. Li: Metall. Trans. A, 2017, vol. 48A, pp. 3419-3431.10.1007/s11661-017-4090-1 ↗
21. N. Kaibo, Z.H. Zhu, K.K. Deng, T. Wang, J.G. Han: Nanomaterials, 2019, vol. 9, pp. 57-75.10.3390/nano9010057 ↗
22. L. Li, H. Li, W. Jiang, Z.Y. Pan, Y. Wang, T. Wang: JOM, 2019, vol. 71, pp. 2033-2039.10.1007/s11837-018-3309-y ↗
23. Y. Tong, G.Z. Quan, J. Zhao, Q. Liu, W. Xiong, R.J. Shi: Mater. Res., 2019, vol. 22, e20190131.10.1590/1980-5373-mr-2019-0131 ↗
24. A. Łukaszek-Sołek, T. Śleboda, J. Krawczyk, S. Bednarek, M. Wojtaszek: J. Alloys Compd., 2019, vol. 797, pp. 174-184.10.1016/j.jallcom.2019.05.094 ↗
25. Q.H. Zang, H.S. Yu, Y.S. Lee, M.S. Kim, H.W. Kim: Mater. Charact., 2019, vol. 151, pp. 404-413.10.1016/j.matchar.2019.03.019 ↗
26. T.Y. Kwak, W.J. Kim: J. Mater. Process. Technol., 2019, vol. 35, pp. 181-191.
27. Q.H. Zang, H.S. Yu, Y.S. Lee, M.S. Kim, H.W. Kim: J. Alloys Compd., 2018, vol. 763, pp. 25-33.10.1016/j.jallcom.2018.05.307 ↗
28. W.L. Cheng, Y. Bai, S.C. Ma, L.F. Wang, H.X. Wang, H. Yu: J. Mater. Process. Technol., 2019, vol. 35, pp. 1198-1209.
29. Y. Guo, X.G. Liu, Z.F. Xu, W.Q. Li, G. Sasaki: J. Alloys Compd., 2020, vol. 818, 152923.10.1016/j.jallcom.2019.152923 ↗
30. K.P Rao, C. Dharmendra, K. Suresh, Y. Prasad, M. Gupta, Metals, 2018, vol. 8, pp. 699-712.10.3390/met8090699 ↗
31. N. Li, C.Z. Zhao, Z.H. Jiang, H.X. Zhang: Mater. Charact., 2019, vol. 153, pp. 224-233.10.1016/j.matchar.2019.05.009 ↗
32. N. Srinivasan, Y.V.R.K. Prasad: Metall. Trans. A, 1994, vol. 25, pp. 2275-2284.10.1007/BF02652327 ↗
33. Y.V.R.K. Prasad, K.P. Rao, M. Gupta: Compos. Sci. Technol., 2009, vol. 69, pp. 1070-1076.10.1016/j.compscitech.2009.01.032 ↗
34. A. Emdadi, I. Sizova, M. Bambach, U. Hecht: Intermetallics, 2019, vol. 109, pp. 123-134.10.1016/j.intermet.2019.03.017 ↗
35. C.J. Zhang, Y.Z. Lian, Y.F. Chen, Y.G. Sun, S.Z. Zhang, H. Feng, Y.W. Zhou, P. Cao: Metals, 2019, vol. 9, pp. 481-495.10.3390/met9040481 ↗
36. K. ZyguŁa, M. Wojtaszek, M. Lypchanskyi, T. Slebosa, G. KorpaŁa, U. Prahl: Metall. Trans. A, 2019, vol. 50A, pp. 5314-5323.10.1007/s11661-019-05434-3 ↗
37. Q. Kang, H.T. Jiang, Z. Kuai, Y. Zhang, Y.J. Wang, Z.X. Cai: Mater. Res. Express, 2019, vol. 6, 086526.10.1088/2053-1591/ab1bef ↗
38. K.K. Deng, J.C. Li, F.J. Xu, K.B. Nie, W. Liang: Mater. Des., 2015, vol. 67, pp. 72-81.10.1016/j.matdes.2014.11.006 ↗
39. P. Xiao, Y.M. Gao, F.X. Xu, S.S. Yang, Y.F. Li, B. Li, S.Y. Zhao: J. Alloys Compd., 2019, vol. 798, pp. 1-11.10.1016/j.jallcom.2019.05.244 ↗
40. X.R. Chen, Z.M. Xu, D.F. Fu, H. Zhang, J. Teng, F.L. Jiang: Met. Mater. Int., 2020. https://doi.org/10.1007/s12540-019-00585-9.10.1007/s12540-019-00585-9 ↗
41. J.P. Sun, B.Q. Xu, Z.Q. Zhang, H. Zhou, J. Han, Y.N. Wu, D. Song, Y.C. Yuan, X.R. Zhou, H. Liu, A.B. Ma: J. Alloys Compd., 2020, vol. 817, 152688.10.1016/j.jallcom.2019.152688 ↗
42. Q. Yang, D.L. Cheng, J. Liu,L. Wang, Z. Chen, M.L. Wang, S.Y. Zhong, Y. Wu, G. Ji, H.W. Wang: Mater. Charact., 2019, vol. 155, 109834.10.1016/j.matchar.2019.109834 ↗
43. J.H. Zhang, J.M. Liu, D.S. Xu, J. Wu, L. Xu, R. Yang: J. Mater. Process. Technol., 2019, vol. 35, pp. 2513-2515.
44. W.W. Zhou, Y.C. Fan, X.P. Feng, K. Kikuchi, N. Nomura: Compos Part A: Appl Sci Manufac., 2018, vol. 112, pp. 168-177.10.1016/j.compositesa.2018.06.008 ↗