Shot-Peening Effect on High Cycling Fatigue of Al-Cu Alloy
Source abstract
Abstract
The present work was aimed at evaluating the effects of shot-peening on the high cycle fatigue performance of the age-hardening aircraft alloy Al 2024 at different almen intensities. Shot-peening to full coverage (100 pct) was performed using spherically conditioned cut wire (SCCW 14) with an average shot size of 0.36 mm and at almen intensities of 0.1, 0.2, and 0.3 mmA. After applying the various mechanical surface treatments, the changes in the surface and near-surface layer properties such as microhardness, residual stress-depth profiles, and surface roughness were determined. The microhardness, surface roughness, and the residual stresses increased proportionally with the almen intensity. Electropolitically polished conditions were used as reference in the mechanically surface treated specimens. A significant improvement was seen in the fatigue performance of the 0.1 mmA.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Surface Treatment and Residual Stress · Metal Alloys Wear and Properties · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (14)
Show source-provided references
1. Morabito A E, Chrysochoos A, Dattoma V. and Galietti U. Analysis of heat sources accompanying the fatigue of 2024 T3 aluminum alloys. Int J Fatigue, 2007; (29): 977–984.10.1016/j.ijfatigue.2006.06.015 ↗
2. Asquith D T, Yerokhin A L, Yates J R, Matthews A. Effect of combined shot-peening and PEO treatment on fatigue life of 2024 Al alloy. Thin Solid Films. 2006; 515(3): 1187-1191.10.1016/j.tsf.2006.07.123 ↗
3. P.V. Petroyiannisa, A.T. Kermanidisa, R. Akidb, C.A. Rodopoulosb, S.G. Pantelakis: Int J Fatigue, 2005, vol. 27, pp. 817–827.10.1016/j.ijfatigue.2004.12.007 ↗
4. Pavlou D G. A phenomenological fatigue damage accumulation rule based on hardness increasing, for the 2024 -T42 aluminum. Eng Struct. 2002; (24): 1363–1368.10.1016/S0141-0296(02)00055-X ↗
5. M.L. Pastor, X. Balandraud, M. Grédiac, and J.L. Robert: Infrared Phys. Technol., 2008, vol. 51, pp. 505–515.10.1016/j.infrared.2008.01.001 ↗
6. Ludian T, Wagner L. Effect of age-hardening conditions on high-cycle fatigue performance of mechanically surface treated Al 2024. Mater Sc Eng A. 2007; 468 (470): 210–213.10.1016/j.msea.2006.07.169 ↗
7. Wahab M A, Park J H, Alam M S, Pang S S. Effect of corrosion prevention compounds on fatigue life in2024-T3 aluminum alloy. J. of Mater Proc Technol. 2006; (174): 211–217.10.1016/j.jmatprotec.2006.01.009 ↗
8. Merati Ali. A study of nucleation and fatigue behavior of an aerospace aluminum alloy 2024-T3. Int J Fatigue. 2005; (27): 33–44.10.1016/j.ijfatigue.2004.06.010 ↗
9. H.D. Gopalakrishna, H.N. Narasimha Murthy, M. Krishna, M.S. Vinod, A.V. Suresh: Eng. Fail. Anal, 2010, vol. 17, pp. 361–368.10.1016/j.engfailanal.2009.08.002 ↗
10. A.T. Kermanidis, P.V. Petroyiannis, S.G. Pantelakis: Theor. Appl. Fract. Mech., 2005, 43, pp. 121–132.10.1016/j.tafmec.2004.12.008 ↗
11. Gupta V K, Agnew S R. Measuring the effect of environment on fatigue crack-wake plasticity in aluminum alloy 2024 using electron backscatter diffraction. Mater Sci Eng A. 2008; (494): 36–46.10.1016/j.msea.2007.09.082 ↗
12. H. Ngiau, and D. Kujawski: Int J Fatigue, 2001, vol. 23, pp. 807–815.10.1016/S0142-1123(01)00033-0 ↗
13. Mohamed A, El-Madhoun Y, Bassim M N. The effet of tempering on low yle fatigue behavior of Al-2024. J Mater Pro Tehnol. 2005; (162–163): 362–366.10.1016/j.jmatprotec.2005.02.111 ↗
14. I. Altenberger, V. Schulze, and A. Niku Lari (eds): in Shot Peening and Other Mechanical Surface Treatment, IITT-International, Marne la Vallee, 2005, p. 144.