Effects of partial recrystallization on high-cycle fatigue deformation and crack generation of a nitrogen-strengthened 32Mn-7Cr austenitic steel at liquid-nitrogen temperature
Source abstract
Abstract
To achieve higher fatigue resistance against subsurface crack generation, both the refinement of grain structure and the introduction of mobile dislocations on various slip systems have been shown to be effective in the 32Mn-7Cr austenitic steel. A novel treatment which consisted of cold grooved rolling and partial recrystallization was introduced to modify the microstructure. High-cycle fatigue properties and fatigue-crack generation were investigated for both the solution-treated (ST) and the partially recrystallized (PR) materials at 77 K. The PR material displayed higher fatigue strength than the ST material, especially in the high-cycle regime. No subsurface crack generation was detected for the PR material; however, it appeared in the lower peak stress and/or in the longer-life range for the ST material. Intergranular facets formed a subsurface crack initiation site in the ST material. Since the dislocation structure that developed in the fatigued PR material assisted homogeneous and multidirectional plastic deformation, the localized deformation and/or the stress concentration at the grain boundaries by coplanar arrays were believed to be relieved. Therefore, intergranular cracking due to incompatibility at a grain boundary may disappear.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Microstructure and Mechanical Properties of Steels · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. O. Umezawa and K. Nagai: Iron Steel Inst. Jpn. Int., 1997, vol. 37, pp. 1170–79.10.2355/isijinternational.37.1170 ↗
2. O. Umezawa and K. Nagai: Metall. Mater. Trans. A, 1998, vol. 29A, pp. 809–22.10.1007/s11661-998-0272-1 ↗
3. H. Yokoyama, O. Umezawa, K. Nagai, T. Suzuki, and K. Kokubo: Metall. Mater. Trans. A, 2000, vol. 31A, pp. 2793–805.10.1007/BF02830339 ↗
4. O. Umezawa and K. Nagai: Metall. Mater. Trans. A, 1998, vol. 29A, pp. 3017–28.10.1007/s11661-998-0209-8 ↗
5. O. Umezawa, K. Nagai, and K. Ishikawa: Tetsu-to-Hagané, 1990, vol. 76, pp. 924–31 (in Japanese).10.2355/tetsutohagane1955.76.6_924 ↗
6. H. Kitagawa, S. Takahashi, C.M. Suh, and S. Miyashita: in Fatigue Mechanisms, ASTM STP 675, J.T. Fong, ed., ASTM, Philadelphia, PA, 1979, pp. 420–49.10.1520/STP35901S ↗
7. O. Umezawa, K. Nagai, and K. Ishikawa: Tetsu-to-Hagané, 1989, vol. 75, pp. 159–66 (in Japanese).10.2355/tetsutohagane1955.75.1_159 ↗
8. Y. Murata, K. Koyama, Y. Matsumoto, M. Morinaga, and N. Yukawa: Iron Steel Inst. Jpn. Int., 1990, vol. 30, pp. 927–36.10.2355/isijinternational.30.927 ↗
9. F. Abe, H. Araki, and T. Noda: Mater. Sci. Technol., 1988, vol. 4, pp. 885–93.10.1179/mst.1988.4.10.885 ↗
10. R. Miura, H. Nakajima, Y. Takahashi, and K. Yoshida: Advances in Cryogenic Engineering Materials, Plenum Press, New York, NY, 1984, vol. 30, pp. 245–52.10.1007/978-1-4613-9868-4_30 ↗
11. K. Kanazawa, M. Kimura, and S. Nishjima: NRIM Material Strength Data Sheet—Technical Document, NRIM, Tsukuba, 1996, No. 14 (in Japanese).
12. M. Klesnil and P. Lukas: Fatigue of Metallic Materials, 2nd ed., Elsevier, Amsterdam, 1992.
13. R.K. Steele and A.J. McEvily: Eng. Fract. Mech., 1976, vol. 8, pp. 31–37.10.1016/0013-7944(76)90075-8 ↗
14. M.F. Ashby: Phil. Mag., 1970, vol. 21, pp. 399–424.10.1080/14786437008238426 ↗
15. A.M. Freudenthal: Eng. Fract. Mech., 1974, vol. 6, pp. 775–93.10.1016/0013-7944(74)90072-1 ↗
16. P. Neuman: Acta Metall., 1969, vol. 17, pp. 1219–25.10.1016/0001-6160(69)90099-6 ↗
17. J.W. Morris, Jr., S.K. Hwang, K.A. Yuschenko, V.I. Belotzerkovetz, and O.G. Kvanevskii: Advances in Cryogenic Engineering Materials, Plenum Press, New York, NY, 1978, vol. 24, pp. 91–102.10.1007/978-1-4613-9853-0_8 ↗
18. Y. Tomota and S. Shibuki: Iron Steel Inst. Jpn. Int., 1990, vol. 30, pp. 663–65.10.2355/isijinternational.30.663 ↗
19. H. Tanaka, N. Kondo, K. Fujita, and K. Shibata: Iron Steel Inst. Jpn. Int., 1990, vol. 30, pp. 646–55.10.2355/isijinternational.30.646 ↗
20. H. Mughrabi: in Investigations and Applications of Severe Plastic Deformation, NATO Science Partnership Sub-Series, T.C. Lowe and R.Z. Valiev, eds., 2000, vol. 80, Kluwer Academic Publishers, Dordrecht, pp. 241–53.
21. A. Vinogradov and S. Hashimoto: Mater. Trans., 2001, vol. 42, pp. 74–84.10.2320/matertrans.42.74 ↗