Investigation on Hot Workability of Ti-37 At Pct Nb Alloy Based on Processing Map and Microstructural Evolution
Source abstract
Abstract
Ti-37 at pct Nb alloy has been successfully applied to engineering fields because of its excellent superconductivity and perfect ductility. The TiNb alloy is necessary to optimize hot processing parameters and further investigate hot workability. Consequently, a processing map of TiNb alloy is constructed based on dynamic material modeling via stress–strain curves at 700 °C to 1000 °C and 0.0005 to 0.5 s−1. The results show that one appropriate working domain is where the temperature range is about 765 °C to 910 °C and the strain rate is simultaneously < 0.0007 s−1, and another appropriate working domain is where the temperature range is about 960 °C to 1000 °C and simultaneously the strain rate range is about 0.002 to 0.1 s−1. Microstructures of TiNb samples, which are deformed in the instability processing domain with the high strain rate of 0.5 s−1, are further characterized to reveal dependence of the processing map on microstructures, and thus it is found that dynamic recovery and incomplete dynamic recrystallization cannot effectively improve the heterogeneous microstructure of TiNb alloy samples during deformation under a high strain rate. In addition, θ- and γ-fiber textures are found in the deformed TiNb specimens, and high deformation temperature contributes to the formation of the θ-fiber texture.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgy and Material Forming · Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. [1] Y.W. Chai, H.Y. Kim, H. Hosoda and S. Miyazaki: Acta Mater., 2009, vol. 57, pp. 4054-4064.10.1016/j.actamat.2009.04.051 ↗
2. [2] B. Sun, X.L. Meng, Z.Y. Gao, W. Cai and L.C. Zhao: J. Alloy Compd., 2017, vol. 715, pp. 16-20.10.1016/j.jallcom.2017.04.275 ↗
3. [3] S. Santra, T. Davies, G. Matthews, J. Liu, C.R.M. Grovenor and S.C. Speller: Mater. Des., 2019, vol. 176, pp. 107836.10.1016/j.matdes.2019.107836 ↗
4. [4] T. Schild, J. L. Duchateau: Physica C, 1998, vol. 310, pp. 247-252.10.1016/S0921-4534(98)00470-5 ↗
5. [5] P. Bruzzone, B. Stepanov and E. Zapretilina: Fusion Eng Des., 2005, vol. 75-79, pp. 111-115.10.1016/j.fusengdes.2005.06.091 ↗
6. [6] J.F. Li, P.X. Zhang, X.H. Liu, J.S. Li, Y. Feng, S.J. Du, T.C. Wang, W.T. Liu, G. Grunblatt, C. Verwaerde and G.K. Hoang: Physica C, 2008, vol. 468, pp. 1840-1842.10.1016/j.physc.2008.05.096 ↗
7. [7] H.Y. Kim, J.I. Kim, T. Inamura, H. Hosoda and S. Miyazaki: Mater. Sci. Eng. A, 2006, vol. 438-440, pp. 839-843.10.1016/j.msea.2006.02.136 ↗
8. [8] H.Y. Kim, Y. Ikehara, J.I. Kim, H. Hosoda and S. Miyazaki: Acta Mater., 2006, vol. 54, pp. 2419-2429.10.1016/j.actamat.2006.01.019 ↗
9. [9] Y. Guo, K. Georgarakis, Y. Yokoyama and A.R. Yavari: J. Alloy Compd., 2013, vol. 571, pp. 25-30.10.1016/j.jallcom.2013.03.192 ↗
10. [10] I.V. Okulov, A.S. Volegov, H. Attar, M. Bönisch, S. Ehtemam-Haghighi, M. Calin and J. Eckert: J. Mech. Behav. Biomed., 2017, vol. 65, pp. 866-871.10.1016/j.jmbbm.2016.10.013 ↗
11. [11] Q.K. Meng, J.S. Zhang, Y.F. Huo, Y.W. Sui, J.Y. Zhang, S. Guo and X.Q. Zhao: J. Alloy Compd., 2018, vol. 45, pp. 579-585.10.1016/j.jallcom.2018.02.259 ↗
12. [12] A. Bahador, E. Hamzah, K. Kondoh, T.A.A. Bakar, F. Yusof, H. Imai, S.N. Saud and M.K. Ibrahim: Mater. Des., 2017, vol. 118, pp. 152-162.10.1016/j.matdes.2016.12.048 ↗
13. [13] M.N. Wilson: Cryogenics, 2008, vol. 48, pp. 381-395.10.1016/j.cryogenics.2008.04.008 ↗
14. [14] F. Mokdad, D.L. Chen, Z.Y. Liu, D.R. Ni, B.L. Xiao and Z.Y. Ma: Mater. Sci. Eng. A, 2017, vol. 702, pp. 425-437.10.1016/j.msea.2017.07.028 ↗
15. [15] J. Lu, Y.L. Song, L. Hua, K.L. Zheng and D.G. Dai: J. Alloy Compd., 2018, vol. 767, pp. 856-869.10.1016/j.jallcom.2018.07.173 ↗
16. [16] H. Rastegari, A. Kermanpur, A. Najafizadeh, D. Porter and M. Somani: J. Alloy Compd., 2015, vol. 626, pp. 136-144.10.1016/j.jallcom.2014.11.170 ↗
17. [17] X.C. Ma, Z.J. An, L. Chen, T.Q. Mao, J.F. Wang, H.J. Long, H.Y. Xue: Mater. Des., 2015, vol. 86, pp. 848-854.10.1016/j.matdes.2015.07.156 ↗
18. [18] W.C. Xu, X.Z. Jin, W.D. Xiong, X.Q. Zeng and D.B. Shan: Mater. Charact., 2018, vol. 135, pp. 154-166.10.1016/j.matchar.2017.11.026 ↗
19. [19] S. Gangolu, A.G. Rao, I. Sabirov, B.P. Kashyap, N. Prabhu and V.P. Deshmukh: Mater. Sci. Eng. A, 2016, vol. 655, pp. 256-264.10.1016/j.msea.2015.12.093 ↗
20. [20] H.L. He, Y.P. Yi, J.D. Cui and S.Q. Huang: Vacuum, 2019, vol. 160, pp. 293-302.10.1016/j.vacuum.2018.11.048 ↗
21. [21] V. Sharma, S.A.S. Namburu, P. Lalwani, C.K. Sagar and A.K. Gupta: Int. J. Refract. Met. H., 2018, vol. 6, pp. 168-179.10.1016/j.ijrmhm.2018.06.009 ↗
22. [22] Q.G. Meng, C.G. Bai and D.S. Xu: J. Mater. Sci. Technol., 2018, vol. 34, pp. 679-688.10.1016/j.jmst.2017.07.015 ↗
23. [23] Y.V.R.K. Prasad, S. Sasidhara and V. K. Sikka: Intermetallics., 2000, vol. 8, pp. 987-995.10.1016/S0966-9795(00)00048-0 ↗
24. [24] H. Ziegler and L. K. Yu: Ingenieur-Archiv, 1972, vol. 41, pp. 89-99.10.1007/BF00533584 ↗
25. [25] C. H. Park, Y. G. Ko, C. S. Lee, K.-T. Park, D.H. Shin and H.S. Lee: Mater. Sci. Forum, 2007, vol. 551-552, pp. 365-372.10.4028/www.scientific.net/MSF.551-552.365 ↗
26. [26] S. Venuqopal and P. V. Sivaprasad: J. Mater. Eng. Perform., 2003, vol. 12, pp. 674-686.10.1361/105994903322692475 ↗
27. [27] Y. V. R. K. Prasad and T. Seshacharyulu: Mater. Sci. Eng. A, 1998, vol. 243, pp. 82-88.10.1016/S0921-5093(97)00782-X ↗
28. [28] O.B. Bembalge and S.K. Panigrahi: Int. J. Mech. Sci., 2021, vol. 191, pp. 106100.10.1016/j.ijmecsci.2020.106100 ↗
29. [29] L. Li and M.Q. Li: Mater. Sci. Eng. A, 2017, vol. 698, pp. 302-312.10.1016/j.msea.2017.05.034 ↗
30. [30] Y.V.R.K. Prasad, K.P. Rao and S. Sasidhara: Hot working guide: a compendium of processing maps, 2nd ed., Materials Park, Ohio: ASM International,1997.
31. [31] Y.V.R.K. Prasad, H.L. Gegel, S.M. Doraivelu, J.C. Malas, J.T. Morgan, K.A. Lark and D.R. Barker: Metall. Trans. A, 1984, vol. 15, pp. 1883-1892.10.1007/BF02664902 ↗
32. [32] Y. Sun, X. Feng, L. Hu, H. Zhang and H. Zhang: J. Alloy Compd., 2018, vol. 53, pp. 256-271.10.1016/j.jallcom.2018.04.225 ↗
33. [33] T.Y. Kwak and W.J. Kim: J. Mater. Sci. Technol., 2019, vol. 35, pp. 181-191.10.1016/j.jmst.2018.06.019 ↗
34. [34] B. Gong, X.W. Duan, J.S. Liu and J.J. Liu: Vacuum, 2018, vol. 155, pp. 345-357.10.1016/j.vacuum.2018.06.022 ↗
35. [35] Y.V.R.K. Prasad and T. Seshacharyulu: Int. Mater. Rev., 1998, vol. 43, pp. 243-258.10.1179/imr.1998.43.6.243 ↗
36. [36] Z.X. Shi, X.F. Yan, C.H. Duan: J. Alloy Compd., 2015, vol. 625, pp. 30-38.10.1016/j.jallcom.2015.08.118 ↗
37. [37] M. Sarebanzadeh, R. Mahmudi and R. Roumina: Mater. Sci. Eng. A, 2015, vol. 637, pp. 155-161.10.1016/j.msea.2015.04.038 ↗
38. [38] L.P. Su, H.Y. Liu, L. Jing, Z.T. Yu, W.X. Wang and L. Zhou: J. Alloy Compd., 2019, vol. 797, pp. 735-743.10.1016/j.jallcom.2019.05.177 ↗
39. [39] F. Zhang, J.L. Sun, J. Shen, X.D. Yan and J. Chen: Mater. Sci. Eng. A, 2014, vol. 613, pp. 141-147.10.1016/j.msea.2014.06.085 ↗
40. [40] Z. Wang, X.N. Wang and Z.S. Zhu: J. Alloy Compd., 2017, vol. 692, pp. 149-154.10.1016/j.jallcom.2016.09.012 ↗
41. [41] K. Huang and R.E. Logé: Mater. Des., 2016, vol. 111, pp. 548-574.10.1016/j.matdes.2016.09.012 ↗
42. [42] E. Ghasemi, A. Zarei-Hanzaki, E. Farabi, K. Tesař, A. Jäger and M. Rezaee: J. Alloy Compd., 2017, vol. 695, pp. 1706-1718.10.1016/j.jallcom.2016.10.322 ↗