Precipitation in Nb-Stabilized Ferritic Stainless Steel Investigated with in-situ and ex-situ Transmission Electron Microscopy
Source abstract
Abstract
A Nb-stabilized Fe-15Cr-0.45Nb-0.010C-0.015N ferritic stainless steel is studied with transmission electron microscopy (TEM) to investigate the morphology and kinetics of precipitation. $$\hbox{Nb}x\hbox{(C,N)}_y$$ and MnS precipitates are present in the steel in the initial condition. Ex-situ TEM analysis is performed on samples heat treated at 973 K, 1073 K, 1173 K, and 1273 K (700 °C, 800 °C, 900 °C, and 1000 °C). Within this temperature range, both $$\hbox{Fe}_2\hbox{Nb}$$ and $$\hbox{Fe}3\hbox{Nb}3\hbox{X}x$$ (with X = C or N) precipitates form. $$\hbox{Fe}_2$$ Nb is observed at 1073 K (800 °C). $$\;\hbox{Fe}3\hbox{Nb}3\hbox{X}x$$ precipitates form at the grain boundaries between 973 K and 1273 K (700 °C and 1000 °C). Up to at least 1173 K (900 °C) their fraction increases with time and temperature, but at 1273 K (1000 °C) they lose stability with respect to $$\hbox{Nb}x\hbox{(C,N)}y.$$ With in-situ TEM, no phase transition is observed between room temperature and 1243 K (970 °C). At 1243 K (970 °C) the precipitation of $$\hbox{Fe}3\hbox{Nb}3\hbox{X}x$$ is observed in the neighborhood of a dissolving $$\hbox{Nb}_2$$ (C,N) precipitate. For sections of grain boundaries where no $$\hbox{Nb}_x\hbox{(C,N)}_y$$ precipitates are present, $$\hbox{Fe}_3\hbox{Nb}_3\hbox{X}x$$ does not form. It is concluded that the precipitation of $$\hbox{Fe}3\hbox{Nb}3\hbox{X}_x$$ is directly related to the dissolution of $$\hbox{Nb}_2$$ (C,N) through the redistribution of C or N.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · High Temperature Alloys and Creep · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (9)
Show source-provided references
1. Fujita N., Ohmura K., Kikuchi M., Suzuki T., Funaki S., Hiroshige I (1996) Scripta Metall. Mater., 35(6): 705-7010.1016/1359-6462(96)00214-X ↗
2. Miyazaki A., Takao K., Furukimi O (2002). ISIJ Int., 42(8): 916-2010.2355/isijinternational.42.916 ↗
3. Fujita N., Ohmura K., Yamamoto A. (2003). Mater. Sci. Eng., A351: 272-8110.1016/S0921-5093(02)00831-6 ↗
4. Chassagne F., Mithieux J.D., Schmitt J.H. (2006). Steel Res. Int., 77(9-10): 680-8510.1002/srin.200606447 ↗
5. Sim G.M., Ahn J.C., Hong S.C., Lee K.J., Lee K.S. (2005). Mater. Sci. Eng., A396: 159-6510.1016/j.msea.2005.01.030 ↗
6. Fujita N., Kikuchi M., Ohmura K. (2009). ISIJ Int., 43(12): 1999-200610.2355/isijinternational.43.1999 ↗
7. Holleck H., Thümmler F. (1967). Mon. Chem., 98: 133-3410.1007/BF00901107 ↗
8. Lü F.X., Jack K.H. (1985). J. Less Common Met., 114(1): 123-2710.1016/0022-5088(85)90396-0 ↗
9. Moelans N., Blanpain B., Wollants P. (2006). Acta Mater., 54(4): 1175-8410.1016/j.actamat.2005.10.045 ↗