The critical chloride concentrations for initiation of corrosion in reinforcing bar (rebar) are essential input parameters for service life predictions of reinforced concrete structures. For highway infrastructure, the specified service life is currently 75 to 120 years depending on the jurisdiction. Different techniques have been employed to determine these critical concentrations because of the many factors influencing the corrosion initiation. The current standard methods, e.g., ASTM G109, require weeks or months of testing and are often not logistically feasible for testing large numbers of specimens in different conditions in a reasonable time frame. The authors have proposed a potentiodynamic polarization technique for a rapid throughput assessment of the critical chloride concentration of different grades of stainless steel reinforcing bars in synthetic concrete pore solution corresponding to a specific concrete mixture design. This method was successfully employed in identifying the influence of alloying composition (Ni, Mo, Mn), testing solution, and rebar surface finish on their critical chloride concentration. The critical concentrations of Ni-containing stainless steel grades were higher than the Mn-containing grade by values greater than 13.5 pct by mass of solution. Mo only improved the pitting resistance and resulting critical chloride concentrations of the duplex grades, by 17 pct by mass of solution, but not the austenitic grades. The critical chloride concentrations of tested bars with processing flaw were lower by 13 pct by mass of solution. Sulfate addition and increment, as measured in pore solution expressed from cement pastes, in synthetic pore solution were found to increase the threshold values of these rebar grades by 4 to 8 pct by mass of solution.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Concrete Corrosion and Durability · Concrete and Cement Materials Research · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. [1] J. T. Pérez-Quiroz, J. Terán, M. J. Herrera, M. Martínez, and J. Genescá, J. Constr. Steel Res., 2008, vol. 64, pp. 1317–24.10.1016/j.jcsr.2008.07.024 ↗
2. [2] M. Mistry, C. Koffler, and S. Wong, Int. J. Life Cycle Assess., 2016, vol. 21, pp. 1637–44.10.1007/s11367-016-1080-2 ↗
3. A. Knudsen, O. Klinghoffer, and T. Skovsgaard, Arminox Stainless, Denmark, 1999.
4. G. Markeset, S. Rostam, and O. Klinghoffer, Nor. Build. Res. Inst. (Nordic Innov. Cent. Proj. - 04118), 2006, vol. Report 405.
5. [5] A. Bautista, G. Blanco, and F. Velasco, Cem. Concr. Res., 2006, vol. 36, pp. 1922–30.10.1016/j.cemconres.2005.10.009 ↗
6. [6] B. Elsener, D. Addari, S. Coray, and A. Rossi, Mater. Corros., 2011, vol. 62, pp. 111–19.10.1002/maco.201005826 ↗
7. N.E. Hakiki, S. Boudin, B. Rondot, and M. Da Cunha Belo, Corros. Sci., 1995, vol. 37, pp. 1809–22.10.1016/0010-938X(95)00084-W ↗
8. N.E. Hakiki, M. Da Cunha Belo, A.M.P. Simoes, and M.G.S. Ferreira, J. Electrochem. Soc., 1998, vol. 145, pp. 3821–29.10.1149/1.1838880 ↗
9. N.E. Hakiki, M.F. Montemor, M.G.S. Ferreira, and M. da Cunha Belo, Corros. Sci., 2000, vol. 42, pp. 687–702.10.1016/S0010-938X(99)00082-7 ↗
10. [10] G. N. Flint and R. N. Cox, Mag. Concr. Res., 1988, vol. 40, pp. 13–27.10.1680/macr.1988.40.142.13 ↗
11. [11] L. Bertolini, F. Bolzoni, T. Pastore, and P. Pedeferri, Br. Corros. J., 1996, vol. 31, pp. 218–22.10.1179/bcj.1996.31.3.218 ↗
12. [12] L. Veleva, M. A. Alpuche-Aviles, M. K. Graves-Brook, and D. O. Wipf, J. Electroanal. Chem., 2002, vol. 537, pp. 85–93.10.1016/S0022-0728(02)01253-6 ↗
13. [13] C. M. Abreu, M. J. Cristóbal, R. Losada, X. R. Nóvoa, G. Pena, and M. C. Pérez, J. Electroanal. Chem., 2004, vol. 572, pp. 335–45.10.1016/j.jelechem.2004.01.015 ↗
14. [14] L. Bertolini and P. Pedeferri, Corrosion Reviews, 2002, vol. 20. p. 129.10.1515/CORRREV.2002.20.1-2.129 ↗
15. L. Bertolini, M. Gastaldi, P. Pedeferri, and E. Redaelli, 15th International Corrosion Congress, 2002, paper 382.
16. A. Bautista, G. Blanco, and F. Velasco, VII National Materials Congress, June 2004.
17. [17] T. J. Mesquita, E. Chauveau, M. Mantel, N. Kinsman, and R. P. Nogueira, Metall. Mater., 2013, vol. 66, pp. 173–78.
18. [18] T. J. Mesquita, E. Chauveau, M. Mantel, N. Kinsman, and R. P. Nogueira, Mater. Chem. Phys., 2011, vol. 126, pp. 602–06.10.1016/j.matchemphys.2011.01.013 ↗
19. [19] W. H. Hartt, NACE Corros. Expo, 2012, vol. 9312, pp. 754–61.
20. C. B. Van Niejenhuis, Thesis from Univ. of Waterloo, Ontario, 2015.
21. [21] I. G. Ogunsanya and C. M. Hansson, Materialia, 2019, vol. 6, pp. 100321.10.1016/j.mtla.2019.100321 ↗
22. [22] I. G. Ogunsanya and C. M. Hansson, Materialia, 2019, vol. 8, pp. 100491.10.1016/j.mtla.2019.100491 ↗
23. S. Randstrom, M. Almen, R. Pettersson, and M. Adair, Proceedings in Structural Faults and Repair, 2010.
24. [24] L. Tang, J. M. Frederiksen, U. M. Angst, R. Polder, M. C. Alonso, B. Elsener, D. Hooton, and J. Pacheco, RILEM Tech. Lett., 2018, vol. 3, pp. 25.10.21809/rilemtechlett.2018.55 ↗
25. [25] S. Goñi and C. Andrade, Cem. Concr. Res., 1990, vol. 20, pp. 525–39.10.1016/0008-8846(90)90097-H ↗
26. [26] M. Kouřil, P. Novák, and M. Bojko, Cem. Concr. Res., 2010 vol. 40, pp. 431–36.10.1016/j.cemconres.2009.11.005 ↗
27. [27] G. K. Glass and N. R. Buenfeld, Corrosion Science, 1997, vol. 39, pp. 1001–13.10.1016/S0010-938X(97)00009-7 ↗
28. [28] U. Angst, B. Elsener, C. K. Larsen, and Ø. Vennesland, Cem. Concr. Res., 2009, vol. 39, pp. 1122–38.10.1016/j.cemconres.2009.08.006 ↗
29. [29] C. Alonso, C. Andrade, M. Castellote, and P. Castro, Cem. Concr. Res., 2000, vol. 30, pp. 1047–55.10.1016/S0008-8846(00)00265-9 ↗
30. B. B. Hope and A. K. C. Ip, ACI Mater. J., 1987, vol. 84, pp. 306–14.
31. [31] K. W. J. Treadaway, R. N. Cox, and B. L. Brown, Proc. Inst. Civ. Eng. Part 1, 1989, vol. 86, pp. 305–31.
32. [32] W. Morris, A. Vico, and M. Vazquez, Electrochim. Acta, 2004, vol. 49, pp. 4447–53.10.1016/j.electacta.2004.05.001 ↗
33. [33] W. Morris, A. Vico, M. Vazquez, and S. R. De Sanchez, Corros. Sci., 2002, vol. 44, pp. 81–99.10.1016/S0010-938X(01)00033-6 ↗
34. [34] M. D. A. Thomas, Mag. Concr. Res., 1996, vol. 48, pp. 265–79.10.1680/macr.1996.48.177.265 ↗
35. [35] M. D. A. Thomas and P. B. Bamforth, Cem. Concr. Res., 1999, vol. 29, pp. 487–95.10.1016/S0008-8846(98)00192-6 ↗
36. [36] P. Sandberg, Cem. Concr. Res., 1999, vol. 29, pp. 473–77.10.1016/S0008-8846(98)00191-4 ↗
37. C. M. Hansson and B. Sorensen, Corrosion Rates of Steel in Concrete – ASTM intl., 1990, pp. 3–17.10.1520/STP25011S ↗
38. [38] J. Williamson and O. B. Isgor, Corros. Sci., 2016, vol. 106, pp. 82–95.10.1016/j.corsci.2016.01.027 ↗
39. [39] P. Ghods, O. B. Isgor, G. Mcrae, and T. Miller, Cem. Concr. Compos., 2009, vol. 31, pp. 2–11.10.1016/j.cemconcomp.2008.10.003 ↗
40. [40] H. B. Gunay, P. Ghods, O. B. Isgor, G. J. C. Carpenter, and X. Wu, Appl. Surf. Sci., 2013, vol. 274, pp. 195–202.10.1016/j.apsusc.2013.03.014 ↗
41. [41] C. B. Van Niejenhuis, I. G. Ogunsanya, and C. M. Hansson, ACI Mater. J., 2018, vol. 117, pp. 21–28.
42. [42] I. G. Ogunsanya and C. M. Hansson, RILEM Tech. Lett., 2018, vol. 3, pp. 75–83.10.21809/rilemtechlett.2018.70 ↗
43. [43] A. Poursaee and C. M. Hansson, Cem. Concr. Res., 2009, vol. 39, pp. 391–400.10.1016/j.cemconres.2009.01.015 ↗
44. [44] R. D. Moser, P. M. Singh, L. F. Kahn, and K. E. Kurtis, Corros. Sci., 2012, vol. 57, pp. 241–53.10.1016/j.corsci.2011.12.012 ↗
45. [45] L. T. Mammoliti, L. C. Brown, C. M. Hansson, and B. B. Hope, Cem. Concr. Res., 1996, vol. 26, pp. 545–50.10.1016/0008-8846(96)00018-X ↗
46. [46] A. Poursaee, Electrochim. Acta, 2010 vol. 55, pp. 1200–06.10.1016/j.electacta.2009.10.004 ↗
47. [47] L. Bertolini and M. Gastaldi, Mater. Corros., 2011, vol. 62, pp. 120–29.10.1002/maco.201005774 ↗
48. [48] V. S. Raja and A. Ramkumar, Br. Corros. J., 1996, vol. 31, pp. 153–57.10.1179/000705996798114653 ↗
49. [49] A. Di Schino and J. M. Kenny, J. Mater. Sci. Lett., 2002, vol. 21, pp. 1969–71.10.1023/A:1021625117639 ↗
50. [50] G. Rondelli, B. Vicentini, and A. Cigada, Mater. Corros., 1995, vol. 46, pp. 628–32.10.1002/maco.19950461104 ↗
51. [51] I. G. Ogunsanya and C.M. Hansson, Corrosion, 2020, vol. 76, pp. 114-30.10.5006/3360 ↗
52. [52] A. Poursaee, Concr. Res. Lett., 2010, vol. 1, pp. 90–97.
53. [53] M. F. Hurley and J. R. Scully, Corrosion, 2006, vol. 62, pp. 892–904.10.5006/1.3279899 ↗
54. [54] C. B. Van Niejenhuis, S. Walbridge, and C. M. Hansson, J. Mater. Sci., 2016, vol. 51, pp. 362–74.10.1007/s10853-015-9387-0 ↗
55. [55] I. G. Ogunsanya and C. M. Hansson, Corrosion, 2017, vol. 74, pp. 134–43.10.5006/2370 ↗
56. [56] D. B. McDonald, M. R. Sherman, D. W. Pfeifer, and Y. P. Virmani, Concrete International, 1995, vol. 17, pp. 65–70.
57. P. Pedeferri, L. Bertolini, F. Bolzoni, and T. Pastore, Proceedings of the International Seminar: The State of the Art of the Repair and Rehabilitation of Reinforced Concrete Structures, 1998, p. 192.
58. B. Sorensen, P. B. Jensen, and E. Maahn, cited in C.L. Page, K.W.J. Treadaway, P.B. Bamworth, Applied Science, 1990, pp. 601–10.
59. [59] M. C. García-Alonso, J. A. González, J. Miranda, M. L. Escudero, M. J. Correia, M. Salta, and A. Bennani, Cem. Concr. Res., 2007, vol. 37, pp. 1562–69.10.1016/j.cemconres.2007.08.010 ↗
60. [60] H. Mahmoud, M. Sanchez, and M. C. Alonso, J. Solid State Electrochem., 2015, vol. 19, pp. 2961–72.10.1007/s10008-015-2908-6 ↗
61. S. G. Balakumaran, R. E. Weyers, and M. C. Brown, Linear Cracking in Bridge Decks, Final Report VTRC 18-R13, Virginia Dep. Transp. March 2018.