Aging Degradation of Austenitic Stainless Steel Weld Probed by Electrochemical Method and Impact Toughness Evaluation

Raghuvir Singh, Goutam Das, B. Mahato, P. K. Singh

Publisher page

Abstract

The present study discriminates the spinodal decomposition and G-phase precipitation in stainless steel welds by double loop electrochemical potentio-kinetic reactivation method and correlates it with the degradation in toughness property. The welds produced with different heat inputs were aged up to 10,000 hours at 673 K to 723 K (400 to 450 °C) and evaluated subsequently for the degree of sensitization (DOS) and impact toughness. The DOS values obtained were attributed to the spinodal decomposition and precipitation of G-phase. Study shows that the DOS correlates well with the impact toughness of the 304LN weld. Prolonged aging at 673 K and 723 K (400 °C and 450 °C) increased the DOS values while the impact toughness was decreased. The weld fabricated at 1 kJ/mm of heat input, produced higher DOS, compared to that at 3 kJ/mm. The geometrical location along the weld is shown to influence the DOS; higher values were obtained at the root than at the topside of the weld. Vermicular and columnar microstructure, in addition to the spinodal decomposition and G-phase precipitation, observed in the root side of the weld appear risky for the impact toughness.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · High Temperature Alloys and Creep

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (32)

Show source-provided references
1. M. J. Povich and P. Rao: Corrosion, 1978, vol. 34, pp. 269–75.10.5006/0010-9312-34.8.269 ↗
2. M. J. Povich: Corrosion, 1978, vol. 34, pp. 60–65.10.5006/0010-9312-34.2.60 ↗
3. T. M. Devine: Acta Metall., 1988, vol. 36, pp. 1491–1501.10.1016/0001-6160(88)90216-7 ↗
4. O. K. Chopra and A. S. Rao: J. Press. Vessel. Technol.,2016, vol. 138(4):040801–040801-24. doi:10.1115/1.4031909.10.1115/1.4031909 ↗
5. C. Pareige, S. Novy, S. Saillet, P. Pareige: J. Nucl. Mater., 2011, vol. 411, pp. 90–96.10.1016/j.jnucmat.2011.01.036 ↗
6. Li Shilei, Yanli Wang, Li Shuxiao, Hailong Zhang, Fei Xui, Xitao Wang: Mater. Des., 2013, vol. 50, pp. 886–92.10.1016/j.matdes.2013.02.061 ↗
7. P. H. Pumphrey, K. N. Akhurst: Mater. Sci. Technol., 1990, vol. 6, pp. 211-19.10.1179/mst.1990.6.3.211 ↗
8. M. Hattestrand, P. Larsson, G. Chai, J. Nilson, J. Odqvist: Mater. Sci. Eng., 2009, vol.A 499, pp. 489–92.10.1016/j.msea.2008.09.021 ↗
9. Jun Wang, Hong Zou, Cong Li, Shaoyu Qiu, Baoluo Shen: Mater. Charact., 2008, vol. 59, pp. 587–91.10.1016/j.matchar.2007.04.018 ↗
10. Ikushia Hamada and Kiyoshi Yamauchi: Metall. Mater. Trans., 2002, vol. 33A, pp. 1743–54.10.1007/s11661-002-0183-5 ↗
11. J.D. Tucker, M.K. Miller and G.A. Young: Acta Mater., 2015, vol. 87, pp. 15–2410.1016/j.actamat.2014.12.012 ↗
12. O. K. Chopra and H.M. Chung: Proceedings of 3rd Conference on Environmental Degradation of Materials in Nuclear Power Systems-Water Reactors, TMS-AIME, Warrendale, 1988, pp. 737–48.
13. K. Chandra, V. Kain, V. Bhutani, V. S. Raja, R. Tewari, G.K. Dey, J. K. Chakravarty: Mater. Sci. Eng., 2012, vol. A 534, pp. 163-75.10.1016/j.msea.2011.11.055 ↗
14. C. J. Park and H. S. Kwon: Corros. Sci., 2002, vol. 44, pp. 2817–30.10.1016/S0010-938X(02)00079-3 ↗
15. K. H. Lo, C. T. Kwok, W. K. Chan, D. Zeng: Corros. Sci., 2012, vol. 55, pp. 267–71.10.1016/j.corsci.2011.10.027 ↗
16. K. Chandra, V. Kain, V. S. Raja, R. Tewari, G.K. Dey: Corros. Sci., 2012, vol. 54, pp. 278–90.10.1016/j.corsci.2011.09.031 ↗
17. ASTM E23-12c: Standard Test Methods for Notched Bar Impact Testing of Metallic Materials, West Conshohocken, 2013, pp. 19428–2959.
18. R. Singh, G. Das, P. K. Singh, and I. Chattoraj: Metall. Matter. Trans. A 2009, vol. 40A, pp. 1219-34.10.1007/s11661-009-9803-7 ↗
19. I. Gowrishankar, A.K. Bhaduri, V. Seetharaman, D.D.N. Verma, and D.R.G. Achar: Weld. J., 1987, vol. 66, pp. 147s–54s.
20. L. F. M. Martins, R.L. Plaut, and A.F. Padilha: ISIJ Int., 1998, vol. 38 (6), pp. 572–79.10.2355/isijinternational.38.572 ↗
21. Raghuvir Singh, B. R. Kumar, A. Kumar, P.K. Dey, and I. Chattoraj: Metall. Mater. Trans. A, 2003, vol. 43A, pp. 986–1003.
22. Hiroshi Abe and Y. Watanabe: Metall. Mater. Trans. A, 2008, vol. 39A, pp. 1392-98.10.1007/s11661-008-9511-8 ↗
23. Orlando Soriano-Vargas, Erika O. Avila-Davila, Victor M. Lopez-Hirata, Nicolas Cayetano-Castro, Jorge L. Gonzalez-Velazquez: Mater. Sci. Eng. A, 2010, vol. 527, pp. 2910–14.10.1016/j.msea.2010.01.020 ↗
24. M. K. Miller, J. M. Hyde, M. G. Hetherington, A. Cerezeo, G. D. W. Smith, C. M. Elliot: Acta Metall. Matter.1995, vol.43 (9), pp. 3385–3401.10.1016/0956-7151(95)00040-3 ↗
25. A. Mateo, L. Llanes, and M. Anglada: J. Mater. Sci., 1997, vol. 32 (17), pp. 4533–40.10.1023/A:1018669217124 ↗
26. E. R. Szumachowski, and H. F. Reid: Weld. J., 1979, vol. 58 (2), pp. 34s-44s.
27. M. Du Toit and P. C. Pistorius: Weld. J., 2003, vol. 82 (8), pp. 219s–24s.
28. A. M. Galloway, N. A. McPherson, and T. N. Baker: Proceedings of IMechE Vol. 225 Part L: J. Materials: Design and Applications, an Evaluation of Weld Metal Nitrogen Retention and Properties in 316LN Austenitic Stainless Steel, 225(2), 2011, pp. 61–69.10.1177/0954420711398608 ↗
29. W. T. DeLong: Weld. J., 1974, vol. 53(7), pp. 273s–86s.
30. T. A. Siewert: Weld. J. 1985, vol. 6S (3), pp. 23–28.
31. G. K. Bouse and M. R. Behrendt: in Mechanical Properties of Micro cast-X Alloy 718 Fine Grain Investment Castings, Superalloy 718, E. Loria, ed., TMS, 1989, pp. 319–24.10.7449/1989/Superalloys_1989_319_328 ↗
32. Osamu Kamiya, Kazuo Kumagai, and Yasushi Kikuchi: Weld. Int. 1992, vol. 6, pp. 606-11.10.1080/09507119209548250 ↗