Effect of Strain Hardened Inner Surface Layers on Stress Corrosion Cracking of Type 316 Stainless Steel in Simulated PWR Primary Water
Source abstract
Abstract
In this study, the relationship between SCC growth rate and Vickers hardness for Type 316 stainless steel at various temperatures in simulated PWR primary water was investigated. In addition, IGSCC growth measurements were conducted using so-called functionally graded cold-rolled specimens made of Type 316 stainless steel, in simulated PWR primary water. Residual stress measurements were performed using the contour and slitting methods on the functionally graded cold-rolled specimens. The contour method measurements found highly tensile stress (350 MPa) toward the surface of the side with a larger thickness reduction and low-magnitude stress elsewhere. The purpose of these latter specimens was to evaluate the effect of heavily cold-worked layers on the inner surface of components made of Type 316 stainless steel on the possibility that IGSCC could penetrate through the wall thickness. The test data showed that the work-hardened inner surface does not always have a detrimental effect on SCC susceptibility. However, if any surface cracks exist within the work-hardened inner surface layer of any components, the stress at the crack tip becomes very large and SCC easily initiates. Nevertheless, even if IGSCC initiates from a heavily cold-worked layer at the inner surface, IGSCC growth rate in Type 316 stainless steel was found to eventually become negligibly small or arrests in the soft base material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Non-Destructive Testing Techniques · Fusion materials and technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (40)
Show source-provided references
1. P.L. Andresen, T.M. Angeliu, L.M. Young, W.R. Catlin, R.M. Horn: Proc. 10th Int. Conf. Environ. Degrad. Mater. Nuclear Power Syst.—Water Reactors Aug. 5–9, CD-Rom. Lake Tahoe, Nevada. 2001.
2. Home Page of The Kansai Electric Power Co.INC. http://www.kepco.co.jp/corporate/pr/2008/__icsFiles/afieldfile/2008/02/04/0204_2j_01.pdf, 2008.
3. T. Shoji, K. Sakaguchi, Z. Lu, S. Hirano, Y. Hasegawa, T. Kobayashi, K. Fujimoto, Y. Nomura: Proc. Int. Symp. FONTEVRAUD 7, 2010, Paper No. A103, CD-ROM.
4. T. Shoji: Proc. 11th Int. Conf. Environ. Degrad. Mater. Nuclear Power Syst. Water React. Aug. 10–14, Stevenson, Washington, 2003. pp. 588–99.
5. P.L. Andresen, P.W. Emigh, M.M. Morra, R.M. Horn: Proc. 11th Int. Conf. Environ. Degrad. Mater. Nuclear Power Syst. Water React. Aug. 10–14, Stevenson, Washington, 2003, pp. 816–33.
6. T. Shoji, G. Li, J. Kwon, S. Matsushima, Z. Lu: Proc. 11th Int. Conf. Environ. Degrad. Mater. Nuclear Power Syst. Water React. Aug. 10–14, Stevenson, Washington, 2003, pp. 834–44.
7. M.L. Castano Martin, M.S. Garcia Redondo, G. Diego Velasco, D. Gomez Briceno: Proc. 11th Int. Conf. Environ. Degrad. Mater. Nuclear Power Syst. Water React. Aug. 10–14, Stevenson, Washington, 2003, pp. 845–51.
8. D. Tice, N. Platts, K. Rigby, J. Stairmand, H. Fairbrother: Proc. 12th Int Conf. Environ. Degrad. Mater. Nuclear Power Syst. Water React. Aug. 14–18, Salt Lake City, Utah, 2005, pp. 1037–1048
9. K. Arioka, T. Yamada, T. Terachi, G. Chiba: Pro. FONTEVRAUD 6, Paper No. A001-T03a, CD-ROM, 2006.
10. L. Tribouilloy, F. Vaillant, J.-M. Olive, M. Puiggali, L. Legras, T. Couvant, J.-M.Boursier, Y. Rouillon, C. Amzallag: Proc. 13th Int Conf. Environ. Degrad. Mater. Nuclear Power Syst. Water React. Aug. 19–23, Whistler, British Columbia, CD-Rom, 2007.
11. M. Ando, K. Nakata, M. Itow, N. Tanaka, M. Koshiishi, R. Obata, Y. Miwa, Y. Kaji, M. Hayakawa: Proc. 13th Int Conf. Environ. Degrad. Mater. Nuclear Power Syst. Water React. Aug. 19–23, Whistler, British Columbia, CD-Rom, 2007.
12. Y. Takeda, Z. Lu, T. Adachi, Q. Peng, J. Kuniya, T. Shoji: Proc. ASME 2010 Pressure Vessels Piping Division/K-PVP Conf. PVP2010, July 18–22, Bellevue, Washington, CD-Rom, 2010.
13. N. Matsubara, T. Kobayashi, K. Fujimoto, Y. Nomura, N. Chigusa, S. Hirano: Proc. Int. Symp. FONTEVRAUD 7, Sept. 26–30, Avignon, France, CD-Rom, 2010.
14. P.Andresen, P.Ford, Material Science and Engineering, (1988), A103, pp.167-184.10.1016/0025-5416(88)90564-2 ↗
15. R.C.Newman, Corrosion, (1994), Vol. 50, pp.682-686.10.5006/1.3293544 ↗
16. P.M. Scott: Proc. 9th Int. Symp. on Environ. Degrad. Mater. in Nucl. Power Syst. Water React. TMS, 1999, pp. 3–14.
17. S. Yaguchi, T.Yonezawa: Trans. Jpn Soc. Mech. Eng. Ser. A, (2012), Vol. 78, Issue 788, pp. 547-563.10.1299/kikaia.78.547 ↗
18. W.Kuang, G.Was, C.Miller, M.Kaufman, T.Alarm, B.Gwalani, R.Banerjee, Corrosion Science, (2018), Vol. 130, pp. 126-137.10.1016/j.corsci.2017.11.002 ↗
19. F.Meng, Z. Lu, T.Shoji, J.Wang, E.H.Han, W.Ke, Corrosion Science, (2011), Vol. 53, pp.2558-2565.10.1016/j.corsci.2011.04.013 ↗
20. T. Yonezawa, N. Sasaguri, K. Onimura: Proc. 1988 JAIF Int. Conf. Water Chem. Nucl. Power Plants Operat. Exp. New Technol. Manag. April, Tokyo, Japan Atomic Industrial Forum, 1988, pp. 490–96.
21. J.Chen, Z.Lu, Q.Xiao, X.Ru, J.Ma, T.Shoji, Journal of Nuclear Materials, (2017), Vol. 496, pp.313-324.10.1016/j.jnucmat.2017.10.005 ↗
22. F. Hosseinzadeh, M. B. Toparli, and P. J. Bouchard, J. Pressure Vessel Technology, (2012), 134, 210.1115/1.4004626 ↗
23. M. Kerr, M. R. Hill, and M. D. Olson, Corrosion, (2013), 69, 975-8510.5006/0832 ↗
24. M. R. Hill, M. D. Olson, and A. T. DeWald, J. Pressure Vessel Technology, (2016), 138, 011404
25. United States Nuclear Regulatory Commission, Office of Nuclear Reactor Regulation, “Cracking in Pressurizer Safety and Relief Nozzles and in Surge Line Nozzles (IN 2004-11),” 2004.
26. M. D. Olson, A. T. DeWald, M. R. Hill, S. L. McCracken: Proc. ASME 2016 Press. Vessels Piping Division Conf. Vancouver, BC, Canada 2016.
27. G. S. Schajer and M. B. Prime, Journal of Engineering Materials and Technology, (2006), Vol. 128, pp. 375-382.10.1115/1.2204952 ↗
28. C. Aydıner and M. B. Prime, J. Eng. Mater. Technol. (2013), 135, 6
29. M. B. Prime, Journal of Engineering Materials and Technology, (2001), Vol. 123, No. 2, pp. 162–168.10.1115/1.1345526 ↗
30. M. B. Prime and A. T. DeWald: Practical Residual Stress Measurement Methods, G. S. Schajer, ed., Wiley, West Sussex, UK, 2013, pp. 109–38.10.1002/9781118402832.ch5 ↗
31. M. D. Olson, A. T. DeWald, M. R. Hill, and M. B. Prime, Exp. Mech., (2014), Vol. 55, No. 3, pp. 577–585.10.1007/s11340-014-9971-2 ↗
32. L.Dong, Q.Peng, E.H.Han, W.Ke, L.Wang, Corrosion Science, (2016), Vol. 107, pp.172-18110.1016/j.corsci.2016.02.030 ↗
33. K. Arioka, T. Yamada, T. Terachi, G. Chiba, Corrosion, (2007), 63, 1114-1123.10.5006/1.3278329 ↗
34. K. Fujimoto, T. Iwamura, S. Suzuki and T. Kobayashi, Y. Kikuchi: Proc. Work Shop on Cold Work Iron- Nickel-Base Alloys Exposed High Temp Water Environ, June 4–8, 2007 Tronto, Canada, CD-Rom.
35. X.Zhong, S.C.Bali, T.Shoji, Corrosion Science, (2017), Vol. 118, pp.143-157.10.1016/j.corsci.2017.02.003 ↗
36. L.Chang, M.G.Burke, F.Scenini, Corrosion Science, (2018), Vol. 138, pp.54-65.10.1016/j.corsci.2018.04.003 ↗
37. R.P.Matthews, R.D.Knusten, J.E.Westraadt, T.Couvant, Corrosion Science, (2017), Vol. 125, pp.175-183.10.1016/j.corsci.2017.06.023 ↗
38. S.Wang, Y.Hu, K.Fang, W.Zhang, X.Wang, Corrosion Science, (2017), Vol. 126, pp.104-120.10.1016/j.corsci.2017.06.019 ↗
39. T.Massoud, V.Maurice, L.H.Klein, A.Seyeux, P.Marcus, Corrosion Science, (2014), Vol. 84, pp.198-203.10.1016/j.corsci.2014.03.030 ↗
40. X.Xie, D.Ning, B.Chen, S.Lu, J.Sun, Corrosion Science, (2016), Vol. 112, pp. 576-584.10.1016/j.corsci.2016.08.014 ↗