Abstract
Three Mg alloys Mg-1 pctMn (M1), Mg-1 pctMn-1.3 pctSr, and Mg-1 pctMn-2.1 pctSr were subjected to two different extrusion temperatures and two different extrusion speeds in lab-scale extrusion. The extrusion temperatures of 573 K and 673 K (300 °C and 400 °C) and two ram speeds of 4 and 8 mm/s were used at constant extrusion ratio of 7. M1 exhibited strong basal texture after extrusion at 673 K (400 °C) at higher speed. At 573 K (300 °C), recrystallization in all alloys takes place completely or partially by continuous dynamic recrystallization mechanism, while particle stimulated nucleation (PSN) occurs in all M1-Sr alloys at both extrusion temperatures and speeds. At 673 K (400 °C), grain boundary bulging is the only recrystallization mechanism in alloy M1, while it occurs in combination with PSN in M1-Sr alloys. The effect of texture weakening by PSN is more significant in M1-Sr alloys extruded at 573 K (400 °C). The plant extrusion trials were carried out on Mg-1 pctMn, Mg-1 pctMn-0.3 pctSr, and Mg-1 pctMn-2.1 pctSr at 623 K (350 °C) with different speeds than in lab-scale extrusion. M1 alloy exhibited strong basal texture at both speeds, while Sr additions of 0.3 and 2.1 pct promoted similar amount of texture weakening.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Magnesium Alloys: Properties and Applications · Hydrogen Storage and Materials · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. A. Becerra, M. Pekguleryuz, Journal of Materials Research 24 (5) (2009) 1722.10.1557/jmr.2009.0205 ↗
2. S. Kleiner, P.J. Uggowitzer, Materials Science and Engineering A 379 (1-2) (2004) 258-263.10.1016/j.msea.2004.02.020 ↗
3. S.R. Agnew, J.W. Senn, and J.A. Horton: JOM, 2006, vol. 58, pp. 62–69.10.1007/s11837-006-0026-8 ↗
4. J.W. Christian, S. Mahajan, Prog. Mater. Sci. 39 (1995) 1-157.10.1016/0079-6425(94)00007-7 ↗
5. O. Muransky, M.R. Barnett, V. Luzin, S. Vogel, Mat. Sci. Eng. A 527 (2010) 1383-1394.10.1016/j.msea.2009.10.018 ↗
6. Y. Chino, M. Kado, M. Mabuchi, Mater. Sci. Eng. A 494 (2008) 343.10.1016/j.msea.2008.04.059 ↗
7. J. Bohlen, M.R. Nurnberg, J.W. Senn, D. Letzig, S.R. Agnew, Acta Materialia 55 (2007) 2101.10.1016/j.actamat.2006.11.013 ↗
8. E.A. Ball, P.B. Prangnell, Scripta Metall. Mater. 31 (1994) 111-116.10.1016/0956-716X(94)90159-7 ↗
9. L.W.F. Mackenzie, B. Davis, F.J. Humphreys, G.W. Lorimer, Mater. Sci. Technol.23 (2007) 173-1180.10.1179/174328407X226509 ↗
10. R. Cottam, J. Robson, G. Lorimer, B. Davis, Mat. Sci. Eng. A 485 (2008) 375-382.10.1016/j.msea.2007.08.016 ↗
11. H.Borkar, M.Hoseini, M. Pekguleryuz., Mater. Sci. Eng. A 537 (2012) 49-57.10.1016/j.msea.2012.01.029 ↗
12. H.Borkar, M.Hoseini, M. Pekguleryuz., Mater. Sci. Eng. A 549 (2012) 168-175.10.1016/j.msea.2012.04.029 ↗
13. J.E. Gruzleski and C.A. Aliravci: U.S. Patent No 5,143,564,1992.
14. M. Yang, F. Pan, R. Cheng, A. Tang, Mater. Sci. Eng. A 491 (2008) 440-445.10.1016/j.msea.2008.02.017 ↗
15. H.Borkar, R.Gauvin, M. Pekguleryuz, Journal of Alloys and Compounds 555 (2013) 219-224.10.1016/j.jallcom.2012.12.078 ↗
16. M. Chandrasekaran, Y.M.S. John, Mater. Sci. Eng. A 381 (2004) 308-319.10.1016/j.msea.2004.04.057 ↗
17. Govind, K. S. Nair, M. C. Mittal, R. Sikand and A. K. Gupta, Mater. Sci. Technol.24 (2008) 399.10.1179/174328408X276224 ↗
18. M. Huppmanna, S. Galla, S. Müllerb, and W. Reimersa: Mater. Sci. Eng. A, 2010 vol. 528, pp. 342–54.
19. J. Bohlen, S. Yi, D. Letzig, and K.U. Kainer: Mater. Sci. Eng. A, 2010 vol. 527, pp. 7092–98.10.1016/j.msea.2010.07.081 ↗
20. N. Stanford: Mater. Sci. Eng. A 2010 vol. 528, pp. 314–22.10.1016/j.msea.2010.08.097 ↗
21. M. Shahzad, L.Wagner, Mat. Sci. Eng. A 506 (2009) 141-147.10.1016/j.msea.2008.11.038 ↗