Formation of Hot Tear Under Controlled Solidification Conditions
Source abstract
Abstract
Aluminum alloy 7050 is known for its superior mechanical properties, and thus finds its application in aerospace industry. Vertical direct-chill (DC) casting process is typically employed for producing such an alloy. Despite its advantages, AA7050 is considered as a “hard-to-cast” alloy because of its propensity to cold cracking. This type of cracks occurs catastrophically and is difficult to predict. Previous research suggested that such a crack could be initiated by undeveloped hot tears (microscopic hot tear) formed during the DC casting process if they reach a certain critical size. However, validation of such a hypothesis has not been done yet. Therefore, a method to produce a hot tear with a controlled size is needed as part of the verification studies. In the current study, we demonstrate a method that has a potential to control the size of the created hot tear in a small-scale solidification process. We found that by changing two variables, cooling rate and displacement compensation rate, the size of the hot tear during solidification can be modified in a controlled way. An X-ray microtomography characterization technique is utilized to quantify the created hot tear. We suggest that feeding and strain rate during DC casting are more important compared with the exerted force on the sample for the formation of a hot tear. In addition, we show that there are four different domains of hot-tear development in the explored experimental window—compression, microscopic hot tear, macroscopic hot tear, and failure. The samples produced in the current study will be used for subsequent experiments that simulate cold-cracking conditions to confirm the earlier proposed model.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. J. C. Williams and E. A. Starke Jr: Acta Mater., 2003, vol. 51, pp. 5775-99.10.1016/j.actamat.2003.08.023 ↗
2. M. Lalpoor, D. G. Eskin and L. Katgerman: Mater. Sci. Eng. A, 2008, vol. 497, pp. 186-94.10.1016/j.msea.2008.06.047 ↗
3. M. Lalpoor, D. G. Eskin, D. Ruvalcaba, H. G. Fjær, A. Ten Cate, N. Ontijt and L. Katgerman: Mater. Sci. Eng. A, 2011, vol. 528, pp. 2831-42.10.1016/j.msea.2010.12.040 ↗
4. Q. Han, S. Viswanathan, D. L. Spainhower and S. K. Das: Metall. Mater. Trans. A, 2001, vol. 32A, pp. 2908-10.10.1007/s11661-001-1043-4 ↗
5. J. M. Drezet, O. Ludwig, C. Jacquerod and E. Waz: Int. J. Cast Met. Res., 2007, vol. 20, pp. 163-70.10.1179/136404607X239753 ↗
6. D. G. Eskin, M. Lalpoor and L. Katgerman: Light Metals, TMS, San Diego, CA, 2011, pp 669-74.
7. T. Subroto, A. Miroux, D. Mortensen, M. M’Hamdi, D.G. Eskin, and L. Katgerman: Modeling of Casting Welding and Advanced Solidification Process XIII (MCWASP XIII), IOP Conference Series: Materials Science and Engineering: Schladming, 2012, p. 012068.10.1088/1757-899X/33/1/012068 ↗
8. S. Terzi, L. Salvo, M. Suéry, N. Limodin, J. Adrien, E. Maire, Y. Pannier, M. Bornert, D. Bernard, M. Felberbaum, M. Rappaz, and E. Boller: Scripta Mater., 2009, vol. 61, pp. 449-52.10.1016/j.scriptamat.2009.04.041 ↗
9. A. B. Phillion, R. W. Hamilton, D. Fuloria, A. C. L. Leung, P. Rockett, T. Connolley and P. D. Lee: Acta Mater., 2011, vol. 59, pp. 1436-44.10.1016/j.actamat.2010.11.005 ↗
10. C. Puncreobutr, P.D. Lee, R.W. Hamilton, B. Cai, and T. Connolley: Metall. Mater. Trans. A, 2013, vol. 44A, pp. 5389–95.10.1007/s11661-012-1563-0 ↗
11. M. Lalpoor, D. G. Eskin and L. Katgerman: Metall. Mater. Trans. A, 2010, vol. 41A, pp. 2425-34.10.1007/s11661-010-0256-9 ↗
12. J. Schindelin, I. Arganda-Carreras, E. Frise, V. Kaynig, M. Longair, T. Pietzsch, S. Preibisch, C. Rueden, S. Saalfeld, B. Schmid, J.Y. Tinevez, D. J. White, V. Hartenstein, K. Eliceiri, P. Tomancak and A. Cardona: Nat. Methods, 2012, vol. 9, pp. 676-82.10.1038/nmeth.2019 ↗
13. E. Giraud, M. Suery and M. Coret: Metall. Mater. Trans. A, 2010, vol. 41A, pp. 2257-68.10.1007/s11661-010-0268-5 ↗
14. T. Subroto, A. Miroux, D.G. Eskin, K. Ellingsen, A. Marson, M. M’Hamdi, and L. Katgerman: 13 th International Conference on Fracture, Beijing, 2013.
15. D. Fabrègue, A. Deschamps, M. Suéry and W. J. Poole: Metall. Mater. Trans. A, 2006, vol. 37A, pp. 1459-67.10.1007/s11661-006-0090-2 ↗
16. D.G. Eskin, Suyitno and L. Katgerman: Prog. Mater. Sci., 2004, vol. 49, pp. 629-711.10.1016/S0079-6425(03)00037-9 ↗
17. J. D. Robson: Mater. Sci. Eng. A, 2004, vol. 382, pp. 112-21.10.1016/j.msea.2004.05.006 ↗
18. L. F. Mondolfo: Aluminum alloys: Structure and properties. Butterworths & Co Ltd, London, 1976.
19. Suyitno, D. G. Eskin and L. Katgerman: Mater. Sci. Eng. A, 2006, vol. 420, pp. 1-7.10.1016/j.msea.2005.12.037 ↗
20. D. G. Eskin: Physical Metallurgy of Direct Chill Casting of Aluminum Alloys (Advances in Metallic Alloys). CRC Press, Taylor & Francis group, LLC, 2008.10.1201/9781420062823 ↗
21. W. M. Van Haaften, W. H. Kool and L. Katgerman: J. Mater. Eng. Perform., 2002, vol. 11, pp. 537-43.10.1361/105994902770343791 ↗
22. Suyitno, W. H. Kool and L. Katgerman: Metall. Mater. Trans. A, 2005, vol. 36A, pp. 1537-46.10.1007/s11661-005-0245-6 ↗
23. D. G. Eskin and L. Katgerman: Metall. Mater. Trans. A, 2007, vol. 38A, pp. 1511-19.10.1007/s11661-007-9169-7 ↗
24. M. Lalpoor, Eskin, D. G., and Katgerman, L.: Metall. Mater. Trans. A, 2009, vol. 40A, pp. 3304-13.10.1007/s11661-009-0031-y ↗