Analysis of Fracture Toughness in the Transition Temperature Region of API X70 Pipeline Steels Rolled in Two-Phase Region
Source abstract
Abstract
In this study, fracture toughness in the transition temperature region of three API X70 line pipe steels rolled in the two-phase (α + γ) region was analyzed in accordance with the ASTM E1921-05 standard test method. Elastic-plastic cleavage fracture toughness (K Jc ) was determined by three-point bend tests, using precracked Charpy V-notch specimens, and then the measured K Jc values were interpreted by the three-parameter Weibull distribution. The fracture toughness test results indicated that the master curve and the 98 pct confidence curves explained the variation in the measured fracture toughness values well. Reference temperatures obtained from the fracture toughness tests as well as index temperatures obtained from the Charpy impact tests were lowest in the steel cooled at 500 °C, which did not contain brittle martensite and had a small effective grain size. In this steel, the absence of martensite led to the higher resistance to cleavage crack initiation, and the smaller effective grain size led to the higher possibility of crack arrest, thereby resulting in the best overall fracture properties.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Fatigue and fracture mechanics · Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. R. Denys: Pipeline Technology, Elsevier, Amsterdam, 2000, vol. I–II, pp. 1–116
2. D.P. Fairchild, M.L. Macia, S.D. Papka, C.W. Petersen, J.H. Stevens, S.T. Barbas, N.V. Bangaru, J.Y. Koo, M.J. Luton: Proc. Int. Pipe Dreamer’s Conf., M. Toyoda and R. Denys, eds., Yokohama, Japan, 2002, pp. 307–21.
3. K.T. Corbett, R.R. Bowen, C.W. Petersen: Int. J. Offshore Polar Eng., 2004, vol. 14, pp. 75–80
4. API Recommended Practice 5L3, American Petroleum Institute, API Publishing Service, 1220 L Street, N.W., Washington, D.C. 20005, USA, 1996, pp. 1–8
5. G. Mannucci and D. Harris: “Fracture Properties of API X100 Gas Pipeline Steels,” Final Report, European Commission, Brussels, Belgium, 2002, pp. 1–128
6. D.J. Horsley: Eng. Fract. Mech., 2003, vol. 70, pp. 547–5210.1016/S0013-7944(02)00136-4 ↗
7. S.-T. Oh, H.-J. Chang, K.H. Oh, H.N. Han: Met. Mater. Int., 2006, vol. 12, pp. 121–2910.1007/BF03027467 ↗
8. Standard Test Method for Determination of Reference Temperature for Ferritic Steels in the Transition Range, ASTM Standard E1921-05, ASTM, West Conshohocken, PA, 2005, pp. 1–29
9. I. Tamura, H. Sekine, T. Tanaka, C. Ouchi: Thermomechanical Processing of High-Strength Low-Alloy Steels, Butterworth & Co., Ltd., London, 1988, pp. 80–10010.1016/B978-0-408-11034-1.50007-6 ↗
10. J.W. Kim, J.W. Choi, D.B. Bae: Met. Mater. Int., 2005, vol. 11, pp. 131–3410.1007/BF03027456 ↗
11. I.D. Choi, D.M. Kim, S.J. Kim, D.M. Bruce, D.K. Matlock, J.G. Speer: Met. Mater. Int., 2006, vol. 12, pp. 13–1910.1007/BF03027517 ↗
12. M. Diaz-Fuentes, A. Iza-Mendia, I. Gutierrez: Metall. Mater. Trans. A, 2003, vol. 34A, pp. 2505–1610.1007/s11661-003-0010-7 ↗
13. Standard Test Method for Notched Bar Impact Testing of Metallic Materials, ASTM Standard E23-02, ASTM, West Conshohocken, PA, 2002, pp. 1–27
14. W. Oldfield: Curve Fitting Impact Test Data - a Statistical Procedure, ASTM Standard. News, 1975, pp. 24–29
15. J.Y. Koo, M.J. Luton, N.V. Bangaru, R.A. Petkovic, D.P. Fairchild, C.W. Petersen, H. Asahi, T. Hara, Y. Terada, M. Sugiyama, H. Tamehiro, Y. Komizo, S. Okaguchi, M. Hamada, A. Yamamoto, and I. Takeuchi: Proc. 13th Int. Offshore and Polar Engineering Conf., Honolulu, HI, 2003, pp. 10–18
16. N.J. Kim: J. Met., 1983, vol. 35, pp. 21–27
17. B. Hwang, Y.M. Kim, S. Lee, N.J. Kim, S.S. Ahn: Metall. Mater. Trans. A, 2005, vol. 36A, pp. 725–3910.1007/s11661-005-0188-y ↗
18. Y. Shiota, Y. Tomota, A. Moriai, T. Kamiyama: Met. Mater. Int., 2005, vol. 11, pp. 371–7610.1007/BF03027507 ↗
19. K. Wallin: Eng. Frac. Mech., 1984, vol. 19, pp. 1085–9310.1016/0013-7944(84)90153-X ↗
20. T.L. Anderson, D. Stienstra: J. Test. Eval., 1989, vol. 17, pp. 46–5310.1520/JTE11532J ↗
21. J.H. Chen, G.Z. Wang, C. Yan, H. Ma, L. Zhu: Int. J. Frac., 1997, vol. 83, pp. 105–2010.1023/A:1007306932437 ↗
22. G.T. Hahn: Metall. Trans. A, 1984, vol. 15A, pp. 947–5910.1007/BF02644685 ↗
23. C.A.N. Lanzillotto, F.B. Pickering: Met. Sci., 1982, vol. 16, pp. 371–8210.1016/0036-9748(82)90153-3 ↗
24. K. Wallin, T. Saario, K. Törrönen: Int. J. Frac., 1987, vol. 32, pp. 201–1010.1007/BF00018353 ↗
25. B.L. Bramfitt, J.G. Speer: Metall. Trans. A, 1990, vol. 21A, pp. 817–2910.1007/BF02656565 ↗
26. G. Krauss, S.W. Thompson: ISIJ, 1995, vol. 35, pp. 937–4510.2355/isijinternational.35.937 ↗
27. Y.E. Smith, A.P. Coldren, R.L. Cryderman: Toward Improved Ductility and Toughness, Climax Molybdenum Co., Ann Arbor, MI, 1971, pp. 119–42
28. K. Wallin, K. Törrönen, R. Ahlstrand, B. Timofeev, V. Rybin, V. Nikolaev, A. Morozov: Nucl. Eng. Des., 1992, vol. 135, pp. 239–4610.1016/0029-5493(92)90225-K ↗
29. S. Kim, B. Hwang, S. Lee: Metall. Mater. Trans. A, 2003, vol. 34A, pp. 1275–8110.1007/s11661-003-0238-2 ↗